rikkarth commited on
Commit
01d03f8
·
verified ·
1 Parent(s): e22d366

Add welding defect dataset: YOLO labels + COCO conversions (part 8)

Browse files
This view is limited to 50 files because it contains too many changes.   See raw diff
Files changed (50) hide show
  1. train/labels/Screenshot-2022-12-05-230149_jpeg_jpg.rf.20da164cede00ca344ab331935f99492.txt +1 -0
  2. train/labels/Screenshot-2022-12-05-230257_jpeg.rf.09a9334fa953f106f78fbc6a6ff9a129.txt +3 -0
  3. train/labels/Screenshot-2022-12-05-230257_jpeg.rf.2f590488353280b486b92075acb96616.txt +3 -0
  4. train/labels/Screenshot-2022-12-05-230317_jpeg.rf.53af4c9750612fc731be2be01a802f63.txt +2 -0
  5. train/labels/Screenshot-2022-12-05-230317_jpeg.rf.578786b94781002fb4df9ea1f33cf0a1.txt +2 -0
  6. train/labels/Screenshot-2022-12-05-230317_jpeg.rf.e44d37eb7d9a3a0ab6bf01f285cf4e14.txt +2 -0
  7. train/labels/Screenshot-2022-12-05-230348_jpeg.rf.339ce1d2b3ab821d7d59e44cc3c4c6e2.txt +3 -0
  8. train/labels/Screenshot-2022-12-05-230348_jpeg.rf.b3d1ca0aaaa9e7dee899495a84923508.txt +3 -0
  9. train/labels/Screenshot-2022-12-05-230348_jpeg.rf.d8da6c3418ea7d638b0dd65514e6284c.txt +3 -0
  10. train/labels/Screenshot-2022-12-05-230348_jpeg_jpg.rf.174ad1c90ed61ecc437ce17f484a5164.txt +3 -0
  11. train/labels/Screenshot-2022-12-05-230410_jpeg.rf.815b686e183a641b2e8f2e8dee940fb9.txt +1 -0
  12. train/labels/Screenshot-2022-12-05-230410_jpeg.rf.b82084e1a5bf2ffa658c36be61f38a3b.txt +1 -0
  13. train/labels/Screenshot-2022-12-05-230410_jpeg.rf.fe3150ca000b6a98cba3ed0dc7b6b511.txt +1 -0
  14. train/labels/Screenshot-2022-12-05-230425_jpeg_jpg.rf.55361a88f305c7c705fd011961c1f7b4.txt +1 -0
  15. train/labels/Screenshot-2022-12-05-231028_jpeg.rf.3639fbd75bd02774b67d12b1e93ef600.txt +2 -0
  16. train/labels/Screenshot-2022-12-05-231028_jpeg.rf.85e08bcc3f4f06a026c273d74c29d210.txt +2 -0
  17. train/labels/Screenshot-2022-12-05-231028_jpeg.rf.ce2c8520fbf331c2093e5ee4572876ba.txt +2 -0
  18. train/labels/Screenshot-2022-12-05-231028_jpeg_jpg.rf.610e20dcc404d2a554185a90cd78542c.txt +2 -0
  19. train/labels/Screenshot-2022-12-05-231053_jpeg.rf.202f98463560450766954ca9d12c6853.txt +2 -0
  20. train/labels/Screenshot-2022-12-05-231053_jpeg.rf.c8254ead89ba005d9a42d60369d16335.txt +2 -0
  21. train/labels/Screenshot-2022-12-05-231053_jpeg_jpg.rf.0f07386dcea961fab1974281793ea053.txt +2 -0
  22. train/labels/Screenshot-2022-12-05-231119_jpeg.rf.7f59439a81424896fa26e68c8ff5f12e.txt +2 -0
  23. train/labels/Screenshot-2022-12-05-231119_jpeg.rf.81510a342a40ef0158ae6d846289bc78.txt +2 -0
  24. train/labels/Screenshot-2022-12-05-231137_jpeg.rf.22e9d90ea1a9c731e31859648883822d.txt +1 -0
  25. train/labels/Screenshot-2022-12-05-231137_jpeg.rf.9554fb25e0ffaff0bf02f2ac8139860d.txt +1 -0
  26. train/labels/Screenshot-2022-12-05-231137_jpeg.rf.96f38dc39d8372ab068367c48190a7fd.txt +1 -0
  27. train/labels/Screenshot-2022-12-05-231221_jpeg.rf.1fee486d8aeaaabaf16cbd616ca00e0b.txt +1 -0
  28. train/labels/Screenshot-2022-12-05-231221_jpeg.rf.207be20039c4f6402df7623d03151ad8.txt +1 -0
  29. train/labels/Screenshot-2022-12-05-231221_jpeg_jpg.rf.136e93bc852c49adcd1202ef1fb24d28.txt +1 -0
  30. train/labels/Screenshot-2022-12-05-231238_jpeg.rf.7bb7d514c0306d0250bebe9cbe38ec45.txt +1 -0
  31. train/labels/Screenshot-2022-12-05-231351_jpeg.rf.26d77592ab5d10d5e3e173ec037a2588.txt +1 -0
  32. train/labels/Screenshot-2022-12-05-231351_jpeg.rf.e5278631367d0f3bec8bb340be6ae739.txt +1 -0
  33. train/labels/Screenshot-2022-12-05-231351_jpeg_jpg.rf.02dbb40248757e1b54357a33a56647c7.txt +1 -0
  34. train/labels/Screenshot-2022-12-05-231406_jpeg.rf.1221ef2cf0f3d224110a7f4402b689b6.txt +1 -0
  35. train/labels/Screenshot-2022-12-05-231406_jpeg.rf.7e65f43141bb57d86bc738aa252a507c.txt +1 -0
  36. train/labels/Screenshot-2022-12-05-231406_jpeg.rf.99e7e30871a85185ed19181342359a39.txt +1 -0
  37. train/labels/Screenshot-2022-12-05-231423_jpeg.rf.2fbdccc559f831bffc4f7c5d34b99b38.txt +1 -0
  38. train/labels/Screenshot-2022-12-05-231423_jpeg.rf.904b10f79b9439acc2161ff3fd2c7048.txt +1 -0
  39. train/labels/Screenshot-2022-12-05-231846_jpeg.rf.f88c005602467df46ae00fe22d1e5e05.txt +1 -0
  40. train/labels/Screenshot-2022-12-05-231846_jpeg.rf.f8c85a7e27724e4b195c7fe14a18698d.txt +1 -0
  41. train/labels/Screenshot-2022-12-05-231846_jpeg_jpg.rf.c3717973227fa1dc2597549de1753d3d.txt +1 -0
  42. train/labels/Screenshot-2022-12-05-231906_jpeg.rf.1731d16c9a3a98fa1337f0fb708e3875.txt +1 -0
  43. train/labels/Screenshot-2022-12-05-231906_jpeg.rf.769bca0618e034a6574073d966ed2cab.txt +1 -0
  44. train/labels/Screenshot-2022-12-05-231906_jpeg_jpg.rf.d35c29d9bb14d7705c6277f1888a15dc.txt +1 -0
  45. train/labels/Slag-inclusion-welding-images_10_jpeg_jpg.rf.fabe6926703c8e26c2bd865286c3beb3.txt +2 -0
  46. train/labels/Slag-inclusion-welding-images_12_jpeg.rf.6007f249b5cb670ec83f162064f69032.txt +1 -0
  47. train/labels/Slag-inclusion-welding-images_12_jpeg.rf.999c524c342abfe266419a43d3eb98e5.txt +1 -0
  48. train/labels/Slag-inclusion-welding-images_12_jpeg_jpg.rf.153e77ce59ed896c9d8ae7a96690d6b4.txt +1 -0
  49. train/labels/Slag-inclusion-welding-images_13_jpeg.rf.43818993c33b4b08fbeb718e5292612a.txt +1 -0
  50. train/labels/Slag-inclusion-welding-images_13_jpeg.rf.d43fc1b241523ed5aa8ed92050941e93.txt +1 -0
train/labels/Screenshot-2022-12-05-230149_jpeg_jpg.rf.20da164cede00ca344ab331935f99492.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 1 0.7484375 0.49765625 0.240625 0.9953125
train/labels/Screenshot-2022-12-05-230257_jpeg.rf.09a9334fa953f106f78fbc6a6ff9a129.txt ADDED
@@ -0,0 +1,3 @@
 
 
 
 
1
+ 0 0.36953125 0.4875 0.328125 0.96875
2
+ 2 0.37890625 0.20859375 0.0546875 0.03125
3
+ 2 0.38203125 0.140625 0.0375 0.028125
train/labels/Screenshot-2022-12-05-230257_jpeg.rf.2f590488353280b486b92075acb96616.txt ADDED
@@ -0,0 +1,3 @@
 
 
 
 
1
+ 0 0.5125 0.36953125 0.96875 0.328125
2
+ 2 0.79140625 0.37890625 0.03125 0.0546875
3
+ 2 0.859375 0.38203125 0.028125 0.0375
train/labels/Screenshot-2022-12-05-230317_jpeg.rf.53af4c9750612fc731be2be01a802f63.txt ADDED
@@ -0,0 +1,2 @@
 
 
 
1
+ 0 0.4 0.39765625 0.775 0.34375
2
+ 0 0.76796875 0.64765625 0.190625 0.4
train/labels/Screenshot-2022-12-05-230317_jpeg.rf.578786b94781002fb4df9ea1f33cf0a1.txt ADDED
@@ -0,0 +1,2 @@
 
 
 
1
+ 0 0.6 0.60234375 0.775 0.34375
2
+ 0 0.23203125 0.35234375 0.190625 0.4
train/labels/Screenshot-2022-12-05-230317_jpeg.rf.e44d37eb7d9a3a0ab6bf01f285cf4e14.txt ADDED
@@ -0,0 +1,2 @@
 
 
 
1
+ 0 0.60234375 0.4 0.34375 0.775
2
+ 0 0.35234375 0.76796875 0.4 0.190625
train/labels/Screenshot-2022-12-05-230348_jpeg.rf.339ce1d2b3ab821d7d59e44cc3c4c6e2.txt ADDED
@@ -0,0 +1,3 @@
 
 
 
 
1
+ 0 0.55546875 0.50625 0.3875 0.98125
2
+ 2 0.56953125 0.5234375 0.115625 0.0375
3
+ 2 0.66328125 0.78671875 0.134375 0.04375
train/labels/Screenshot-2022-12-05-230348_jpeg.rf.b3d1ca0aaaa9e7dee899495a84923508.txt ADDED
@@ -0,0 +1,3 @@
 
 
 
 
1
+ 0 0.50625 0.44453125 0.98125 0.3890625
2
+ 2 0.5234375 0.43046875 0.0375 0.115625
3
+ 2 0.78671875 0.33671875 0.04375 0.134375
train/labels/Screenshot-2022-12-05-230348_jpeg.rf.d8da6c3418ea7d638b0dd65514e6284c.txt ADDED
@@ -0,0 +1,3 @@
 
 
 
 
1
+ 0 0.49375 0.55546875 0.98125 0.3890625
2
+ 2 0.4765625 0.56953125 0.0375 0.115625
3
+ 2 0.21328125 0.66328125 0.04375 0.134375
train/labels/Screenshot-2022-12-05-230348_jpeg_jpg.rf.174ad1c90ed61ecc437ce17f484a5164.txt ADDED
@@ -0,0 +1,3 @@
 
 
 
 
1
+ 0 0.55546875 0.50625 0.3875 0.98125
2
+ 2 0.56953125 0.5234375 0.115625 0.0375
3
+ 2 0.66328125 0.78671875 0.134375 0.04375
train/labels/Screenshot-2022-12-05-230410_jpeg.rf.815b686e183a641b2e8f2e8dee940fb9.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.5 0.55859375 0.99375 0.353125
train/labels/Screenshot-2022-12-05-230410_jpeg.rf.b82084e1a5bf2ffa658c36be61f38a3b.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.5 0.44140625 0.99375 0.353125
train/labels/Screenshot-2022-12-05-230410_jpeg.rf.fe3150ca000b6a98cba3ed0dc7b6b511.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.55859375 0.5 0.353125 0.99375
train/labels/Screenshot-2022-12-05-230425_jpeg_jpg.rf.55361a88f305c7c705fd011961c1f7b4.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.6515625 0.40546875 0.5484375 0.2265625
train/labels/Screenshot-2022-12-05-231028_jpeg.rf.3639fbd75bd02774b67d12b1e93ef600.txt ADDED
@@ -0,0 +1,2 @@
 
 
 
1
+ 0 0.38984375 0.37578125 0.753125 0.26875
2
+ 0 0.7578125 0.60859375 0.20625 0.396875
train/labels/Screenshot-2022-12-05-231028_jpeg.rf.85e08bcc3f4f06a026c273d74c29d210.txt ADDED
@@ -0,0 +1,2 @@
 
 
 
1
+ 0 0.62421875 0.38984375 0.26875 0.753125
2
+ 0 0.39140625 0.7578125 0.396875 0.20625
train/labels/Screenshot-2022-12-05-231028_jpeg.rf.ce2c8520fbf331c2093e5ee4572876ba.txt ADDED
@@ -0,0 +1,2 @@
 
 
 
1
+ 0 0.38984375 0.37578125 0.753125 0.26875
2
+ 0 0.7578125 0.60859375 0.20625 0.396875
train/labels/Screenshot-2022-12-05-231028_jpeg_jpg.rf.610e20dcc404d2a554185a90cd78542c.txt ADDED
@@ -0,0 +1,2 @@
 
 
 
1
+ 0 0.62421875 0.38984375 0.26875 0.753125
2
+ 0 0.39140625 0.7578125 0.3984375 0.20625
train/labels/Screenshot-2022-12-05-231053_jpeg.rf.202f98463560450766954ca9d12c6853.txt ADDED
@@ -0,0 +1,2 @@
 
 
 
1
+ 0 0.49765625 0.3859375 0.9953125 0.35625
2
+ 2 0.51328125 0.35546875 0.065625 0.1140625
train/labels/Screenshot-2022-12-05-231053_jpeg.rf.c8254ead89ba005d9a42d60369d16335.txt ADDED
@@ -0,0 +1,2 @@
 
 
 
1
+ 0 0.50234375 0.6140625 0.9953125 0.35625
2
+ 2 0.48671875 0.64453125 0.065625 0.1140625
train/labels/Screenshot-2022-12-05-231053_jpeg_jpg.rf.0f07386dcea961fab1974281793ea053.txt ADDED
@@ -0,0 +1,2 @@
 
 
 
1
+ 0 0.6140625 0.49765625 0.35625 0.9953125
2
+ 2 0.64453125 0.51328125 0.1140625 0.0671875
train/labels/Screenshot-2022-12-05-231119_jpeg.rf.7f59439a81424896fa26e68c8ff5f12e.txt ADDED
@@ -0,0 +1,2 @@
 
 
 
1
+ 2 0.53515625 0.46484375 0.13125 0.078125
2
+ 0 0.521875 0.50390625 0.7375 0.8125
train/labels/Screenshot-2022-12-05-231119_jpeg.rf.81510a342a40ef0158ae6d846289bc78.txt ADDED
@@ -0,0 +1,2 @@
 
 
 
1
+ 2 0.46484375 0.46484375 0.078125 0.13125
2
+ 0 0.50390625 0.478125 0.8125 0.7375
train/labels/Screenshot-2022-12-05-231137_jpeg.rf.22e9d90ea1a9c731e31859648883822d.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 2 0.51171875 0.58984375 0.2875 0.1859375
train/labels/Screenshot-2022-12-05-231137_jpeg.rf.9554fb25e0ffaff0bf02f2ac8139860d.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 2 0.48828125 0.41015625 0.2875 0.1859375
train/labels/Screenshot-2022-12-05-231137_jpeg.rf.96f38dc39d8372ab068367c48190a7fd.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 2 0.51171875 0.58984375 0.2875 0.1859375
train/labels/Screenshot-2022-12-05-231221_jpeg.rf.1fee486d8aeaaabaf16cbd616ca00e0b.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.4421875 0.50625 0.55 0.446875
train/labels/Screenshot-2022-12-05-231221_jpeg.rf.207be20039c4f6402df7623d03151ad8.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.49375 0.4421875 0.446875 0.55
train/labels/Screenshot-2022-12-05-231221_jpeg_jpg.rf.136e93bc852c49adcd1202ef1fb24d28.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.4421875 0.50625 0.55 0.446875
train/labels/Screenshot-2022-12-05-231238_jpeg.rf.7bb7d514c0306d0250bebe9cbe38ec45.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.540625 0.50390625 0.19375 0.9796875
train/labels/Screenshot-2022-12-05-231351_jpeg.rf.26d77592ab5d10d5e3e173ec037a2588.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.39765625 0.49375 0.428125 0.984375
train/labels/Screenshot-2022-12-05-231351_jpeg.rf.e5278631367d0f3bec8bb340be6ae739.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.49375 0.60234375 0.984375 0.428125
train/labels/Screenshot-2022-12-05-231351_jpeg_jpg.rf.02dbb40248757e1b54357a33a56647c7.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.49375 0.60234375 0.984375 0.4296875
train/labels/Screenshot-2022-12-05-231406_jpeg.rf.1221ef2cf0f3d224110a7f4402b689b6.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.278125 0.58125 0.546875 0.828125
train/labels/Screenshot-2022-12-05-231406_jpeg.rf.7e65f43141bb57d86bc738aa252a507c.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.41875 0.278125 0.828125 0.546875
train/labels/Screenshot-2022-12-05-231406_jpeg.rf.99e7e30871a85185ed19181342359a39.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.721875 0.41875 0.546875 0.828125
train/labels/Screenshot-2022-12-05-231423_jpeg.rf.2fbdccc559f831bffc4f7c5d34b99b38.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 1 0.475 0.384375 0.95 0.25
train/labels/Screenshot-2022-12-05-231423_jpeg.rf.904b10f79b9439acc2161ff3fd2c7048.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 1 0.525 0.615625 0.95 0.25
train/labels/Screenshot-2022-12-05-231846_jpeg.rf.f88c005602467df46ae00fe22d1e5e05.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.50234375 0.61015625 0.9921875 0.7125
train/labels/Screenshot-2022-12-05-231846_jpeg.rf.f8c85a7e27724e4b195c7fe14a18698d.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.61015625 0.49765625 0.7125 0.9921875
train/labels/Screenshot-2022-12-05-231846_jpeg_jpg.rf.c3717973227fa1dc2597549de1753d3d.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.50234375 0.61015625 0.9921875 0.7125
train/labels/Screenshot-2022-12-05-231906_jpeg.rf.1731d16c9a3a98fa1337f0fb708e3875.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.4328125 0.615625 0.2546875 0.278125
train/labels/Screenshot-2022-12-05-231906_jpeg.rf.769bca0618e034a6574073d966ed2cab.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.615625 0.5671875 0.278125 0.2546875
train/labels/Screenshot-2022-12-05-231906_jpeg_jpg.rf.d35c29d9bb14d7705c6277f1888a15dc.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.4328125 0.615625 0.2546875 0.2796875
train/labels/Slag-inclusion-welding-images_10_jpeg_jpg.rf.fabe6926703c8e26c2bd865286c3beb3.txt ADDED
@@ -0,0 +1,2 @@
 
 
 
1
+ 0 0.43828125 0.62109375 0.740625 0.196875
2
+ 1 0.43828125 0.3375 0.7859375 0.1796875
train/labels/Slag-inclusion-welding-images_12_jpeg.rf.6007f249b5cb670ec83f162064f69032.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.50078125 0.496875 0.9984375 0.13125
train/labels/Slag-inclusion-welding-images_12_jpeg.rf.999c524c342abfe266419a43d3eb98e5.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.496875 0.49921875 0.13125 0.9984375
train/labels/Slag-inclusion-welding-images_12_jpeg_jpg.rf.153e77ce59ed896c9d8ae7a96690d6b4.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.496875 0.49921875 0.13125 0.9984375
train/labels/Slag-inclusion-welding-images_13_jpeg.rf.43818993c33b4b08fbeb718e5292612a.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.509375 0.525 0.7515625 0.94375
train/labels/Slag-inclusion-welding-images_13_jpeg.rf.d43fc1b241523ed5aa8ed92050941e93.txt ADDED
@@ -0,0 +1 @@
 
 
1
+ 0 0.475 0.509375 0.94375 0.7515625