diff --git a/valid/images/imagkvyfes_jpeg.rf.9a3675037a196097f81fbf8d3ee10c72.jpg b/valid/images/imagkvyfes_jpeg.rf.9a3675037a196097f81fbf8d3ee10c72.jpg new file mode 100644 index 0000000000000000000000000000000000000000..a6688d949617668bb80441fc855518f2a22db3c4 --- /dev/null +++ b/valid/images/imagkvyfes_jpeg.rf.9a3675037a196097f81fbf8d3ee10c72.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:04d3025260009eda2a157a9cc5804563844991d908b8d77e9a8565967f2e2195 +size 46397 diff --git a/valid/images/imagkvyfes_jpeg_jpg.rf.662acf5b9d03af6a8d54231561e9b285.jpg b/valid/images/imagkvyfes_jpeg_jpg.rf.662acf5b9d03af6a8d54231561e9b285.jpg new file mode 100644 index 0000000000000000000000000000000000000000..7eeeedb1a63adc6f764665c755c79ee71a702a2e --- /dev/null +++ b/valid/images/imagkvyfes_jpeg_jpg.rf.662acf5b9d03af6a8d54231561e9b285.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:b33e930c306fbb1188d66501109dabb200e9af84ede325cb73919ea4bc1e63f5 +size 46419 diff --git a/valid/images/istockphoto-1006281428-612x612_jpeg_jpg.rf.097a9032fb3decdd9fec0d929cb29754.jpg b/valid/images/istockphoto-1006281428-612x612_jpeg_jpg.rf.097a9032fb3decdd9fec0d929cb29754.jpg new file mode 100644 index 0000000000000000000000000000000000000000..3f0caa887c54899b35e45269c98a0850714bb6f5 --- /dev/null +++ b/valid/images/istockphoto-1006281428-612x612_jpeg_jpg.rf.097a9032fb3decdd9fec0d929cb29754.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:0ccea46053f3e8458ddc1eb8700a0a7b3544514af4108697472ccbcbaa000273 +size 39984 diff --git a/valid/images/istockphoto-1006281470-612x612_jpeg.rf.c340a57a2fa3f33cf21bd28b6e96e28a.jpg b/valid/images/istockphoto-1006281470-612x612_jpeg.rf.c340a57a2fa3f33cf21bd28b6e96e28a.jpg new file mode 100644 index 0000000000000000000000000000000000000000..11ded1ddd4b32ad2942772d4d8a74cf8c1850e5f --- /dev/null +++ b/valid/images/istockphoto-1006281470-612x612_jpeg.rf.c340a57a2fa3f33cf21bd28b6e96e28a.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:8612f534e5920cb13dce411b31929dca7af77d55d5fed2bf3ec4688efb6d95f1 +size 40199 diff --git a/valid/images/istockphoto-1006281470-612x612_jpeg_jpg.rf.c7d8b3cfa109ff2f895494227f0f3355.jpg b/valid/images/istockphoto-1006281470-612x612_jpeg_jpg.rf.c7d8b3cfa109ff2f895494227f0f3355.jpg new file mode 100644 index 0000000000000000000000000000000000000000..4c3803169f0bf7839b9e57d5910dfbdb71e86bdf --- /dev/null +++ b/valid/images/istockphoto-1006281470-612x612_jpeg_jpg.rf.c7d8b3cfa109ff2f895494227f0f3355.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:fcef51eba3737c9c470052903cf96dcacbbbaf4a73dc0007ef9e90092ba3cfb0 +size 40200 diff --git a/valid/images/istockphoto-1006281518-612x612_jpeg.rf.1de08bb6edf46aa7cf6b31e420d73ce6.jpg b/valid/images/istockphoto-1006281518-612x612_jpeg.rf.1de08bb6edf46aa7cf6b31e420d73ce6.jpg new file mode 100644 index 0000000000000000000000000000000000000000..4aae3fe258b6b9250a881a9b84a04fedd287be0e --- /dev/null +++ b/valid/images/istockphoto-1006281518-612x612_jpeg.rf.1de08bb6edf46aa7cf6b31e420d73ce6.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:ed815675d1705dfbea8fa30d3ee6500cb4a57e52f4198d4fb41f4cec91e6e8ac +size 88281 diff --git a/valid/images/istockphoto-1008822794-612x612_jpeg.rf.1ba2cbaa48f5a7824fa2f7d098a4e274.jpg b/valid/images/istockphoto-1008822794-612x612_jpeg.rf.1ba2cbaa48f5a7824fa2f7d098a4e274.jpg new file mode 100644 index 0000000000000000000000000000000000000000..0903dccd780d5e76b0f9abeef896bb29de8650e0 --- /dev/null +++ b/valid/images/istockphoto-1008822794-612x612_jpeg.rf.1ba2cbaa48f5a7824fa2f7d098a4e274.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:c367c510047cf4a5c235d235a9cd5b2abe8e0e131f6e566a66f119cecbb5b038 +size 70010 diff --git a/valid/images/istockphoto-1008822794-612x612_jpeg_jpg.rf.e367824ca13919c36524749a3eaf2890.jpg b/valid/images/istockphoto-1008822794-612x612_jpeg_jpg.rf.e367824ca13919c36524749a3eaf2890.jpg new file mode 100644 index 0000000000000000000000000000000000000000..ccbe79ba12221f52b77281d2a50a86fcd04d50a1 --- /dev/null +++ b/valid/images/istockphoto-1008822794-612x612_jpeg_jpg.rf.e367824ca13919c36524749a3eaf2890.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:ef86109cb4824f8ccba91367b397ed81fe4c35a3da1887a9cf0ca144d76354cd +size 70000 diff --git a/valid/images/istockphoto-1329411389-612x612_jpeg.rf.d8805916b1db1bf82de3c0b248ac0840.jpg b/valid/images/istockphoto-1329411389-612x612_jpeg.rf.d8805916b1db1bf82de3c0b248ac0840.jpg new file mode 100644 index 0000000000000000000000000000000000000000..1ab6fe4ca5090a5d8b268b2e95a9b2c66a36b869 --- /dev/null +++ b/valid/images/istockphoto-1329411389-612x612_jpeg.rf.d8805916b1db1bf82de3c0b248ac0840.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:8129c65ea6a89f02388ba542e72da54448855eae3366264493b69407e00e1799 +size 32753 diff --git a/valid/images/istockphoto-1341142829-612x612_jpeg.rf.8662723e5b33d0168fcac1f214c2bf5f.jpg b/valid/images/istockphoto-1341142829-612x612_jpeg.rf.8662723e5b33d0168fcac1f214c2bf5f.jpg new file mode 100644 index 0000000000000000000000000000000000000000..85fc0d982526cc0433078fea41e392f0063ecec4 --- /dev/null +++ b/valid/images/istockphoto-1341142829-612x612_jpeg.rf.8662723e5b33d0168fcac1f214c2bf5f.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:f93628835d516117876d81b79c0ee603f915093cdee759ed4162d6c62e577fc5 +size 66504 diff --git a/valid/images/istockphoto-1341142829-612x612_jpeg_jpg.rf.35fd75d819410e802938795158ed5bf6.jpg b/valid/images/istockphoto-1341142829-612x612_jpeg_jpg.rf.35fd75d819410e802938795158ed5bf6.jpg new file mode 100644 index 0000000000000000000000000000000000000000..58a597e05b93dcd234278b21aa83b3eda0f9cc2c --- /dev/null +++ b/valid/images/istockphoto-1341142829-612x612_jpeg_jpg.rf.35fd75d819410e802938795158ed5bf6.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:40bb148a2767f6333731f7920c9b91d8b54bc51d0f08cd30578a7912e2cbf7ac +size 66482 diff --git a/valid/images/mig-good-welds_10_jpeg_jpg.rf.b35c10d98c3d3b194b87a6a11e8d5204.jpg b/valid/images/mig-good-welds_10_jpeg_jpg.rf.b35c10d98c3d3b194b87a6a11e8d5204.jpg new file mode 100644 index 0000000000000000000000000000000000000000..eae1dfcf9b9b1d9f60fccbaf00c9c669c6ac7a5c --- /dev/null +++ b/valid/images/mig-good-welds_10_jpeg_jpg.rf.b35c10d98c3d3b194b87a6a11e8d5204.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:eebd8b44548d6973ddcbad5da14f5ab19dac3b4293f29ea89005d96265752754 +size 52557 diff --git a/valid/images/mig-good-welds_11_jpeg.rf.f7d53cdf1deeee8d1ebb918d2788f3ee.jpg b/valid/images/mig-good-welds_11_jpeg.rf.f7d53cdf1deeee8d1ebb918d2788f3ee.jpg new file mode 100644 index 0000000000000000000000000000000000000000..cd26596ed79e5eda6025694d7e6c03d5925c617f --- /dev/null +++ b/valid/images/mig-good-welds_11_jpeg.rf.f7d53cdf1deeee8d1ebb918d2788f3ee.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:cb8a329f15d3ef6ab4350aa1f49add17e975a3c46fd85b0ae207401a403cc7d6 +size 67538 diff --git a/valid/images/mig-good-welds_18_jpeg.rf.a6229f75ebdfb3e8f60f32c424023b57.jpg b/valid/images/mig-good-welds_18_jpeg.rf.a6229f75ebdfb3e8f60f32c424023b57.jpg new file mode 100644 index 0000000000000000000000000000000000000000..d3ff474817899e77f7de304a0452b21104172451 --- /dev/null +++ b/valid/images/mig-good-welds_18_jpeg.rf.a6229f75ebdfb3e8f60f32c424023b57.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:29e73031d70a5c9a471115c46e2ad6202c4b4d2a00b0d2a7a741ba1afc8fd3d9 +size 61096 diff --git a/valid/images/mig-good-welds_25_jpeg_jpg.rf.67ba7b27a9740a2cee33de0b2aa07b38.jpg b/valid/images/mig-good-welds_25_jpeg_jpg.rf.67ba7b27a9740a2cee33de0b2aa07b38.jpg new file mode 100644 index 0000000000000000000000000000000000000000..b7a8aa7d6ce2b98cd89cef77f04e214ec2e5a71b --- /dev/null +++ b/valid/images/mig-good-welds_25_jpeg_jpg.rf.67ba7b27a9740a2cee33de0b2aa07b38.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:71aaec225e46f55069ba8a02e09b02927acf7a6ebad84b8e43032b6c7917c8cb +size 50183 diff --git a/valid/images/mig-good-welds_26_jpeg_jpg.rf.d2df980ab9ff653d757151b3f09c7b60.jpg b/valid/images/mig-good-welds_26_jpeg_jpg.rf.d2df980ab9ff653d757151b3f09c7b60.jpg new file mode 100644 index 0000000000000000000000000000000000000000..1c9ca0f210418967145d7c9bcfca89cd44f03f4b --- /dev/null +++ b/valid/images/mig-good-welds_26_jpeg_jpg.rf.d2df980ab9ff653d757151b3f09c7b60.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:fc6fbfc1976c1ea0cecfa2213e20dd691b553662e2dd0772dffdd15285833b41 +size 37341 diff --git a/valid/images/mig-good-welds_27_jpeg_jpg.rf.a62ab80b5453ebdff52f4318f95a2128.jpg b/valid/images/mig-good-welds_27_jpeg_jpg.rf.a62ab80b5453ebdff52f4318f95a2128.jpg new file mode 100644 index 0000000000000000000000000000000000000000..85dd22190ea74d12f1a49aae617c19cfef45911d --- /dev/null +++ b/valid/images/mig-good-welds_27_jpeg_jpg.rf.a62ab80b5453ebdff52f4318f95a2128.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:5c815c235acf8058d1137c3bfd66b3632229e087004ccb4dc361361e42c69619 +size 38311 diff --git a/valid/images/mig-good-welds_31_jpeg_jpg.rf.15788d80fb006bac20b18c5e25a8ab38.jpg b/valid/images/mig-good-welds_31_jpeg_jpg.rf.15788d80fb006bac20b18c5e25a8ab38.jpg new file mode 100644 index 0000000000000000000000000000000000000000..518e37027aabcd97ec6533bdd95b1bd4a8d18808 --- /dev/null +++ b/valid/images/mig-good-welds_31_jpeg_jpg.rf.15788d80fb006bac20b18c5e25a8ab38.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:4e45ae29e47df9e10bb5c6e9221542be2a3e9ba909ce9ff0885a20bc357f549f +size 31228 diff --git a/valid/images/mig-good-welds_35_jpeg_jpg.rf.cd003ef912040fb387bc238928885861.jpg b/valid/images/mig-good-welds_35_jpeg_jpg.rf.cd003ef912040fb387bc238928885861.jpg new file mode 100644 index 0000000000000000000000000000000000000000..1cc9778f15712da37209fb3862dba6a61a8c308f --- /dev/null +++ b/valid/images/mig-good-welds_35_jpeg_jpg.rf.cd003ef912040fb387bc238928885861.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:586609718f63a463cf035297518a296683e5601d8a4bf11db6d81fc5ba986762 +size 35588 diff --git a/valid/images/overlap-welding-images_26_jpeg.rf.2ab860d40487f0e21dbd74cd2571a64b.jpg b/valid/images/overlap-welding-images_26_jpeg.rf.2ab860d40487f0e21dbd74cd2571a64b.jpg new file mode 100644 index 0000000000000000000000000000000000000000..e4f6acf4b3a5538900cea79beff7acd81a3be24b --- /dev/null +++ b/valid/images/overlap-welding-images_26_jpeg.rf.2ab860d40487f0e21dbd74cd2571a64b.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:868abb919808309e52d07739928db886e7216f5333123637d76e5ddf2625960e +size 62877 diff --git a/valid/images/overlap-welding-images_26_jpeg_jpg.rf.52dce3834bd8eae983c31c2141a20d3c.jpg b/valid/images/overlap-welding-images_26_jpeg_jpg.rf.52dce3834bd8eae983c31c2141a20d3c.jpg new file mode 100644 index 0000000000000000000000000000000000000000..a5d34baf31834fe04751140b7d6b8714cc596d17 --- /dev/null +++ b/valid/images/overlap-welding-images_26_jpeg_jpg.rf.52dce3834bd8eae983c31c2141a20d3c.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:9fddc7014b31155c4d112ca184583ca02c3829f454db1547906b0a37136d1601 +size 62860 diff --git a/valid/images/overlap-welding-images_8_jpeg.rf.496a0365bbdbeb1062d1127867afa159.jpg b/valid/images/overlap-welding-images_8_jpeg.rf.496a0365bbdbeb1062d1127867afa159.jpg new file mode 100644 index 0000000000000000000000000000000000000000..b484873d4c7fa036f23eb730fd48f67a671acd1b --- /dev/null +++ b/valid/images/overlap-welding-images_8_jpeg.rf.496a0365bbdbeb1062d1127867afa159.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:28e3005566447f4211b05272cd02181dce81353a8aa51b02a4926db13221fe5f +size 59283 diff --git a/valid/images/poor-Welding-Images_10_jpeg.rf.76882ad1939df69e3059e065f8e8c377.jpg b/valid/images/poor-Welding-Images_10_jpeg.rf.76882ad1939df69e3059e065f8e8c377.jpg new file mode 100644 index 0000000000000000000000000000000000000000..f93086de2393b437c381f674805170ebce5504ac --- /dev/null +++ b/valid/images/poor-Welding-Images_10_jpeg.rf.76882ad1939df69e3059e065f8e8c377.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:261752a538be01248978ee09231f17904354dff58be686e36e5dcde54e06bf48 +size 72201 diff --git a/valid/images/poor-Welding-Images_20_jpeg_jpg.rf.9de9f53203c40abe734f99f1daf735d3.jpg b/valid/images/poor-Welding-Images_20_jpeg_jpg.rf.9de9f53203c40abe734f99f1daf735d3.jpg new file mode 100644 index 0000000000000000000000000000000000000000..d14e570b343b70f0253d8e581610844c04f4e219 --- /dev/null +++ b/valid/images/poor-Welding-Images_20_jpeg_jpg.rf.9de9f53203c40abe734f99f1daf735d3.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:84b915fccef79e3b42eb8702ff313928443b16ae7f175fec07bd69d0bb6ac098 +size 70490 diff --git a/valid/images/poor-Welding-Images_30_jpeg.rf.182688e8dbcf6740de764394e86eaf7b.jpg b/valid/images/poor-Welding-Images_30_jpeg.rf.182688e8dbcf6740de764394e86eaf7b.jpg new file mode 100644 index 0000000000000000000000000000000000000000..e22cfda4840b06004b0c654559ec0b948b9e4340 --- /dev/null +++ b/valid/images/poor-Welding-Images_30_jpeg.rf.182688e8dbcf6740de764394e86eaf7b.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:949e6b15d14bb04e6532c7511f9578f572db81a02d5d2cd1ed5c667b261f4b8f +size 53590 diff --git a/valid/images/poor-Welding-Images_30_jpeg_jpg.rf.9c41acc876f697dfbe12a27cd68536c9.jpg b/valid/images/poor-Welding-Images_30_jpeg_jpg.rf.9c41acc876f697dfbe12a27cd68536c9.jpg new file mode 100644 index 0000000000000000000000000000000000000000..1c7a3a89af186c82a1a5d007f6db491cf047d430 --- /dev/null +++ b/valid/images/poor-Welding-Images_30_jpeg_jpg.rf.9c41acc876f697dfbe12a27cd68536c9.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:040164bfbda41787d67de83d1a8baba97e81edffe7a15133944e7a87bd16151f +size 53590 diff --git a/valid/images/poor-Welding-Images_43_jpeg.rf.30d7319782a1a3adb6083bf57a22c151.jpg b/valid/images/poor-Welding-Images_43_jpeg.rf.30d7319782a1a3adb6083bf57a22c151.jpg new file mode 100644 index 0000000000000000000000000000000000000000..dd835a9a207136baf1aa39322e2a5f4d334d0082 --- /dev/null +++ b/valid/images/poor-Welding-Images_43_jpeg.rf.30d7319782a1a3adb6083bf57a22c151.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:80bda61ca780f3e45315166aab3717f9ea84bfae3e5350caf2605dd1b86587cf +size 59552 diff --git a/valid/images/poor-Welding-Images_52_jpeg_jpg.rf.a2c054b968740496a6930c40a9f8c947.jpg b/valid/images/poor-Welding-Images_52_jpeg_jpg.rf.a2c054b968740496a6930c40a9f8c947.jpg new file mode 100644 index 0000000000000000000000000000000000000000..c6434a792e916a44ef27ac8012603ffeeed67e06 --- /dev/null +++ b/valid/images/poor-Welding-Images_52_jpeg_jpg.rf.a2c054b968740496a6930c40a9f8c947.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:182a814dc141b841ad0b72ec98541fb0d9397bfa8f44c05a98c99c07b1e29440 +size 126985 diff --git a/valid/images/poor-Welding-Images_9_jpeg_jpg.rf.f950f91df976733e2291ff30bea45aa0.jpg b/valid/images/poor-Welding-Images_9_jpeg_jpg.rf.f950f91df976733e2291ff30bea45aa0.jpg new file mode 100644 index 0000000000000000000000000000000000000000..1538bea4defad6acd0933c9e060815d2ea0050a3 --- /dev/null +++ b/valid/images/poor-Welding-Images_9_jpeg_jpg.rf.f950f91df976733e2291ff30bea45aa0.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:c4510c2038740dfeb00b8f1f0fc78fddaa731d8ddf5b9210adfaf67aa12b2cc5 +size 70692 diff --git a/valid/images/weld-defect-work-was-carried-out-using-semi-automatic-arc-welding-mig-welding-weld-defect-work-was-carried-out-using-semi-242006161_jpeg.rf.abf277a0e2de19ced505d1f57f0e6011.jpg b/valid/images/weld-defect-work-was-carried-out-using-semi-automatic-arc-welding-mig-welding-weld-defect-work-was-carried-out-using-semi-242006161_jpeg.rf.abf277a0e2de19ced505d1f57f0e6011.jpg new file mode 100644 index 0000000000000000000000000000000000000000..0334a81188dc70aff3606a76b82f19c08c5c4085 --- /dev/null +++ b/valid/images/weld-defect-work-was-carried-out-using-semi-automatic-arc-welding-mig-welding-weld-defect-work-was-carried-out-using-semi-242006161_jpeg.rf.abf277a0e2de19ced505d1f57f0e6011.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:27395ddaf0ad25a8077949fa6bfcd339160d9552ffcfab4cac8e542c74852316 +size 68718 diff --git a/valid/images/weld-defect-work-was-carried-out-using-semi-automatic-arc-welding-mig-welding-weld-defect-work-was-carried-out-using-semi-242007435_jpeg.rf.68bf8b6a1c26ca1a0cd2d06ee11d8eff.jpg b/valid/images/weld-defect-work-was-carried-out-using-semi-automatic-arc-welding-mig-welding-weld-defect-work-was-carried-out-using-semi-242007435_jpeg.rf.68bf8b6a1c26ca1a0cd2d06ee11d8eff.jpg new file mode 100644 index 0000000000000000000000000000000000000000..188c8a0ec75689b795412d50fc45c867be76ca22 --- /dev/null +++ b/valid/images/weld-defect-work-was-carried-out-using-semi-automatic-arc-welding-mig-welding-weld-defect-work-was-carried-out-using-semi-242007435_jpeg.rf.68bf8b6a1c26ca1a0cd2d06ee11d8eff.jpg @@ -0,0 +1,3 @@ +version https://git-lfs.github.com/spec/v1 +oid sha256:ebac0711737cff4263fd5b162df59969e388e0dfe630d2dcfbcf078d363df712 +size 60749 diff --git a/valid/labels/886d6ca3-1b242175-download_1_jpeg_jpg.rf.386935bff2eb78c24af0001e8b15401f.txt b/valid/labels/886d6ca3-1b242175-download_1_jpeg_jpg.rf.386935bff2eb78c24af0001e8b15401f.txt new file mode 100644 index 0000000000000000000000000000000000000000..4e42d612e9e841e750cf8c2e1a91f746ee5df5f1 --- /dev/null +++ b/valid/labels/886d6ca3-1b242175-download_1_jpeg_jpg.rf.386935bff2eb78c24af0001e8b15401f.txt @@ -0,0 +1 @@ +2 0.484375 0.72265625 0.96875 0.07421875 diff --git a/valid/labels/Good-Welding-images_17_jpeg.rf.0920fc1f7bf9f790087214be28aafbb6.txt b/valid/labels/Good-Welding-images_17_jpeg.rf.0920fc1f7bf9f790087214be28aafbb6.txt new file mode 100644 index 0000000000000000000000000000000000000000..b14ddad4a93ab750cc5f5fc59c9115ff4a73e5a7 --- /dev/null +++ b/valid/labels/Good-Welding-images_17_jpeg.rf.0920fc1f7bf9f790087214be28aafbb6.txt @@ -0,0 +1,2 @@ +0 0.24765625 0.5171875 0.36328125 0.5609375 +1 0.76484375 0.52578125 0.328125 0.4703125 diff --git a/valid/labels/Good-Welding-images_20_jpeg.rf.05786e2171fa8723312372d80c4d6762.txt b/valid/labels/Good-Welding-images_20_jpeg.rf.05786e2171fa8723312372d80c4d6762.txt new file mode 100644 index 0000000000000000000000000000000000000000..24771a661d9826dbb4e5f7ae033708e0d29cf55b --- /dev/null +++ b/valid/labels/Good-Welding-images_20_jpeg.rf.05786e2171fa8723312372d80c4d6762.txt @@ -0,0 +1 @@ +1 0.49765625 0.48359375 0.99453125 0.2390625 diff --git a/valid/labels/Good-Welding-images_22_jpeg_jpg.rf.318c9d57367dca722350fe8d63b44591.txt b/valid/labels/Good-Welding-images_22_jpeg_jpg.rf.318c9d57367dca722350fe8d63b44591.txt new file mode 100644 index 0000000000000000000000000000000000000000..64fd1dad7ab21ddd0bbda12f3df049eb62f088e1 --- /dev/null +++ b/valid/labels/Good-Welding-images_22_jpeg_jpg.rf.318c9d57367dca722350fe8d63b44591.txt @@ -0,0 +1 @@ +1 0.6234375 0.5375 0.1921875 0.1046875 diff --git a/valid/labels/Good-Welding-images_47_jpeg.rf.ac708f7ce59708ffaacf92787a0454c4.txt b/valid/labels/Good-Welding-images_47_jpeg.rf.ac708f7ce59708ffaacf92787a0454c4.txt new file mode 100644 index 0000000000000000000000000000000000000000..f7d423c3446426b31886e494121c90a27623cba9 --- /dev/null +++ b/valid/labels/Good-Welding-images_47_jpeg.rf.ac708f7ce59708ffaacf92787a0454c4.txt @@ -0,0 +1 @@ +1 0.50390625 0.5171875 0.25234375 0.96171875 diff --git a/valid/labels/Good-Welding-images_4_jpeg.rf.986518c5eb56613a41d71ac3dbd308bb.txt b/valid/labels/Good-Welding-images_4_jpeg.rf.986518c5eb56613a41d71ac3dbd308bb.txt new file mode 100644 index 0000000000000000000000000000000000000000..1c6182536b21bb927166d6e1520789b56c8d0db8 --- /dev/null +++ b/valid/labels/Good-Welding-images_4_jpeg.rf.986518c5eb56613a41d71ac3dbd308bb.txt @@ -0,0 +1 @@ +1 0.56171875 0.5265625 0.12421875 0.9421875 diff --git a/valid/labels/Not-perfect-welding-images_10_jpeg_jpg.rf.938705132c676bde86605b449fbfd55e.txt b/valid/labels/Not-perfect-welding-images_10_jpeg_jpg.rf.938705132c676bde86605b449fbfd55e.txt new file mode 100644 index 0000000000000000000000000000000000000000..ff62331ce0f6a441e1b48687fc50c6161a992736 --- /dev/null +++ b/valid/labels/Not-perfect-welding-images_10_jpeg_jpg.rf.938705132c676bde86605b449fbfd55e.txt @@ -0,0 +1,3 @@ +1 0.478125 0.221875 0.9390625 0.2765625 +0 0.47890625 0.7515625 0.953125 0.3296875 +2 0.4765625 0.73671875 0.946875 0.071875 diff --git a/valid/labels/Not-perfect-welding-images_13_jpeg.rf.dc026de714d7a3d31fbdfb4a24acaf1c.txt b/valid/labels/Not-perfect-welding-images_13_jpeg.rf.dc026de714d7a3d31fbdfb4a24acaf1c.txt new file mode 100644 index 0000000000000000000000000000000000000000..b315918e668ac8479888ea30da9d4bd9f6662ed6 --- /dev/null +++ b/valid/labels/Not-perfect-welding-images_13_jpeg.rf.dc026de714d7a3d31fbdfb4a24acaf1c.txt @@ -0,0 +1 @@ +0 0.359375 0.44453125 0.50625 0.80859375 diff --git a/valid/labels/Not-perfect-welding-images_17_jpeg_jpg.rf.64e46e84fb95dfb5e6eecc845629350c.txt b/valid/labels/Not-perfect-welding-images_17_jpeg_jpg.rf.64e46e84fb95dfb5e6eecc845629350c.txt new file mode 100644 index 0000000000000000000000000000000000000000..ca13ec376d800b89bb18f07950a49357aa76207f --- /dev/null +++ b/valid/labels/Not-perfect-welding-images_17_jpeg_jpg.rf.64e46e84fb95dfb5e6eecc845629350c.txt @@ -0,0 +1,3 @@ +0 0.48046875 0.625 0.5453125 0.2234375 +2 0.37265625 0.59140625 0.0828125 0.0640625 +2 0.66796875 0.61640625 0.0890625 0.0796875 diff --git a/valid/labels/SampleV1_1_mp4-14_jpg.rf.a63c344a8a0ff6183f314d4a5b231a71.txt b/valid/labels/SampleV1_1_mp4-14_jpg.rf.a63c344a8a0ff6183f314d4a5b231a71.txt new file mode 100644 index 0000000000000000000000000000000000000000..c53a9591bf73cf6a5a27757c2a938ac6b0ad0803 --- /dev/null +++ b/valid/labels/SampleV1_1_mp4-14_jpg.rf.a63c344a8a0ff6183f314d4a5b231a71.txt @@ -0,0 +1,4 @@ +2 0.52265625 0.63828125 0.246875 0.09140625 +2 0.4453125 0.3953125 0.14765625 0.05859375 +1 0.34296875 0.0984375 0.09296875 0.196875 +0 0.440625 0.66640625 0.1015625 0.59375 diff --git a/valid/labels/SampleV1_1_mp4-17_jpg.rf.a9d2faf4d350854fbc0d2fc2ec7a63f4.txt b/valid/labels/SampleV1_1_mp4-17_jpg.rf.a9d2faf4d350854fbc0d2fc2ec7a63f4.txt new file mode 100644 index 0000000000000000000000000000000000000000..7e1879f2dfdcc11ec06680f4128770bd488b58a5 --- /dev/null +++ b/valid/labels/SampleV1_1_mp4-17_jpg.rf.a9d2faf4d350854fbc0d2fc2ec7a63f4.txt @@ -0,0 +1 @@ +1 0.5015625 0.63125 0.09453125 0.62109375 diff --git a/valid/labels/SampleV1_1_mp4-18_jpg.rf.cddd27bcf2b930148b836f4554980319.txt b/valid/labels/SampleV1_1_mp4-18_jpg.rf.cddd27bcf2b930148b836f4554980319.txt new file mode 100644 index 0000000000000000000000000000000000000000..4c1b4bf4f53c03d5cc4f9b59bbbf79a582f635b0 --- /dev/null +++ b/valid/labels/SampleV1_1_mp4-18_jpg.rf.cddd27bcf2b930148b836f4554980319.txt @@ -0,0 +1,3 @@ +2 0.5609375 0.184375 0.14765625 0.36875 +0 0.56171875 0.25546875 0.10859375 0.51015625 +1 0.54140625 0.8578125 0.09453125 0.28359375 diff --git a/valid/labels/SampleV1_1_mp4-19_jpg.rf.094d362d62a7104ad597f1c8d56b7784.txt b/valid/labels/SampleV1_1_mp4-19_jpg.rf.094d362d62a7104ad597f1c8d56b7784.txt new file mode 100644 index 0000000000000000000000000000000000000000..c6153f993b143c1084b5e0652251687ea909ea18 --- /dev/null +++ b/valid/labels/SampleV1_1_mp4-19_jpg.rf.094d362d62a7104ad597f1c8d56b7784.txt @@ -0,0 +1,2 @@ +2 0.51953125 0.228125 0.22265625 0.17421875 +0 0.503125 0.46875 0.14375 0.63515625 diff --git a/valid/labels/SampleV1_1_mp4-24_jpg.rf.8487d87bb4c1d1ab9059da84ac881495.txt b/valid/labels/SampleV1_1_mp4-24_jpg.rf.8487d87bb4c1d1ab9059da84ac881495.txt new file mode 100644 index 0000000000000000000000000000000000000000..ea1da113273c823e7d8648ca9053211118a17610 --- /dev/null +++ b/valid/labels/SampleV1_1_mp4-24_jpg.rf.8487d87bb4c1d1ab9059da84ac881495.txt @@ -0,0 +1 @@ +1 0.52734375 0.678125 0.140625 0.64296875 diff --git a/valid/labels/SampleV1_1_mp4-37_jpg.rf.95083a00053d9a169b4b5f0147468a7d.txt b/valid/labels/SampleV1_1_mp4-37_jpg.rf.95083a00053d9a169b4b5f0147468a7d.txt new file mode 100644 index 0000000000000000000000000000000000000000..f19faa626745a7743b4ed531e00e6abc55518c67 --- /dev/null +++ b/valid/labels/SampleV1_1_mp4-37_jpg.rf.95083a00053d9a169b4b5f0147468a7d.txt @@ -0,0 +1,3 @@ +2 0.08125 0.32578125 0.16171875 0.08984375 +0 0.49375 0.40078125 0.98671875 0.22890625 +1 0.384375 0.8703125 0.76875 0.178125 diff --git a/valid/labels/SampleV1_1_mp4-4_jpg.rf.90a4aca54a06a2e5d7213f75c5d5fba5.txt b/valid/labels/SampleV1_1_mp4-4_jpg.rf.90a4aca54a06a2e5d7213f75c5d5fba5.txt new file mode 100644 index 0000000000000000000000000000000000000000..a344d45c7acfda81d7a8b05e3470699654a8b571 --- /dev/null +++ b/valid/labels/SampleV1_1_mp4-4_jpg.rf.90a4aca54a06a2e5d7213f75c5d5fba5.txt @@ -0,0 +1,4 @@ +2 0.5 0.1796875 0.1734375 0.08984375 +2 0.49296875 0.5453125 0.16015625 0.11328125 +0 0.48671875 0.39609375 0.11171875 0.509375 +1 0.409375 0.90234375 0.0796875 0.1953125 diff --git a/valid/labels/SampleV1_1_mp4-51_jpg.rf.3d073c6b2f2d417e5492f68793ce0033.txt b/valid/labels/SampleV1_1_mp4-51_jpg.rf.3d073c6b2f2d417e5492f68793ce0033.txt new file mode 100644 index 0000000000000000000000000000000000000000..f2c378127d2e52542d73378a8fefe14a46406239 --- /dev/null +++ b/valid/labels/SampleV1_1_mp4-51_jpg.rf.3d073c6b2f2d417e5492f68793ce0033.txt @@ -0,0 +1,8 @@ +2 0.86796875 0.01640625 0.2640625 0.0328125 +2 0.73203125 0.64375 0.10234375 0.06875 +2 0.96328125 0.6109375 0.0734375 0.04296875 +2 0.32734375 0.3109375 0.08828125 0.03671875 +0 0.234375 0.2875 0.46875 0.05859375 +1 0.8234375 0.271875 0.353125 0.05234375 +0 0.84375 0.6375 0.3125 0.059375 +1 0.2484375 0.6953125 0.49609375 0.06015625 diff --git a/valid/labels/SampleV1_1_mp4-54_jpg.rf.1c796a2e06811dea4be419e80956f270.txt b/valid/labels/SampleV1_1_mp4-54_jpg.rf.1c796a2e06811dea4be419e80956f270.txt new file mode 100644 index 0000000000000000000000000000000000000000..14fc493aa747f58102da334490715a059e881dfb --- /dev/null +++ b/valid/labels/SampleV1_1_mp4-54_jpg.rf.1c796a2e06811dea4be419e80956f270.txt @@ -0,0 +1,4 @@ +2 0.91328125 0.27890625 0.17265625 0.06015625 +1 0.2953125 0.296875 0.590625 0.053125 +1 0.2875 0.6859375 0.56484375 0.0453125 +1 0.9125 0.68125 0.1703125 0.04140625 diff --git a/valid/labels/SampleV1_1_mp4-60_jpg.rf.f380bd888e3092f2864a3798d26b394a.txt b/valid/labels/SampleV1_1_mp4-60_jpg.rf.f380bd888e3092f2864a3798d26b394a.txt new file mode 100644 index 0000000000000000000000000000000000000000..1d513333807a294b0726d7e4fe9e88014e857792 --- /dev/null +++ b/valid/labels/SampleV1_1_mp4-60_jpg.rf.f380bd888e3092f2864a3798d26b394a.txt @@ -0,0 +1,2 @@ +1 0.5984375 0.3234375 0.80234375 0.0453125 +1 0.58828125 0.753125 0.8234375 0.07421875 diff --git a/valid/labels/SampleV1_1_mp4-61_jpg.rf.ed4cd01f17bdb2df5fa9b3dd9c91c833.txt b/valid/labels/SampleV1_1_mp4-61_jpg.rf.ed4cd01f17bdb2df5fa9b3dd9c91c833.txt new file mode 100644 index 0000000000000000000000000000000000000000..d616e6b1d47b269b27a65fb00a2120d5528ce89e --- /dev/null +++ b/valid/labels/SampleV1_1_mp4-61_jpg.rf.ed4cd01f17bdb2df5fa9b3dd9c91c833.txt @@ -0,0 +1,4 @@ +1 0.90625 0.31875 0.1875 0.053125 +1 0.31484375 0.35234375 0.6296875 0.0453125 +1 0.30703125 0.7875 0.6140625 0.0640625 +1 0.9203125 0.75703125 0.15859375 0.0453125 diff --git a/valid/labels/SampleV1_2_mp4-12_jpg.rf.aa96da1d076e08ad75cace39788fbbe2.txt b/valid/labels/SampleV1_2_mp4-12_jpg.rf.aa96da1d076e08ad75cace39788fbbe2.txt new file mode 100644 index 0000000000000000000000000000000000000000..bead58caed9cd86015daeb900272723545b93e91 --- /dev/null +++ b/valid/labels/SampleV1_2_mp4-12_jpg.rf.aa96da1d076e08ad75cace39788fbbe2.txt @@ -0,0 +1,4 @@ +2 0.80234375 0.06171875 0.19609375 0.0765625 +2 0.715625 0.18828125 0.10625 0.0765625 +2 0.9453125 0.60078125 0.0609375 0.040625 +0 0.8140625 0.3875 0.1453125 0.725 diff --git a/valid/labels/SampleV1_2_mp4-17_jpg.rf.a16416c9c0bec8ef151d26fc509db43d.txt b/valid/labels/SampleV1_2_mp4-17_jpg.rf.a16416c9c0bec8ef151d26fc509db43d.txt new file mode 100644 index 0000000000000000000000000000000000000000..96b8721913e65ee6d6e2da98b78a67ef5b1016c5 --- /dev/null +++ b/valid/labels/SampleV1_2_mp4-17_jpg.rf.a16416c9c0bec8ef151d26fc509db43d.txt @@ -0,0 +1 @@ +1 0.671875 0.55390625 0.16171875 0.7203125 diff --git a/valid/labels/SampleV1_2_mp4-27_jpg.rf.65ce6fb08af5a11743d0e0e67f8e6633.txt b/valid/labels/SampleV1_2_mp4-27_jpg.rf.65ce6fb08af5a11743d0e0e67f8e6633.txt new file mode 100644 index 0000000000000000000000000000000000000000..65c0c9a033b1aab808e740ec903e86069fc51053 --- /dev/null +++ b/valid/labels/SampleV1_2_mp4-27_jpg.rf.65ce6fb08af5a11743d0e0e67f8e6633.txt @@ -0,0 +1,7 @@ +2 0.8109375 0.328125 0.12421875 0.08828125 +2 0.6421875 0.2703125 0.078125 0.040625 +2 0.628125 0.340625 0.0734375 0.053125 +2 0.6984375 0.77109375 0.07578125 0.07265625 +2 0.90078125 0.73359375 0.1109375 0.05625 +0 0.55546875 0.28984375 0.8890625 0.1921875 +0 0.5015625 0.70703125 0.996875 0.1796875 diff --git a/valid/labels/SampleV1_2_mp4-2_jpg.rf.d050f469c873b976c77829aa93cde991.txt b/valid/labels/SampleV1_2_mp4-2_jpg.rf.d050f469c873b976c77829aa93cde991.txt new file mode 100644 index 0000000000000000000000000000000000000000..a875613faee7e8ed6dae55c41e965926025272c2 --- /dev/null +++ b/valid/labels/SampleV1_2_mp4-2_jpg.rf.d050f469c873b976c77829aa93cde991.txt @@ -0,0 +1,7 @@ +1 0.09765625 0.18203125 0.0578125 0.28828125 +1 0.5875 0.190625 0.05546875 0.2796875 +1 0.98203125 0.2015625 0.0359375 0.26875 +1 0.14609375 0.52421875 0.06953125 0.26875 +1 0.6046875 0.51875 0.04921875 0.253125 +1 0.9609375 0.52890625 0.053125 0.25625 +1 0.14609375 0.875 0.0390625 0.24921875 diff --git a/valid/labels/SampleV1_2_mp4-35_jpg.rf.112706bdf7b84566f9b8fa03084da685.txt b/valid/labels/SampleV1_2_mp4-35_jpg.rf.112706bdf7b84566f9b8fa03084da685.txt new file mode 100644 index 0000000000000000000000000000000000000000..a14086a9e80dd4489946eac5ac791df32b2735c5 --- /dev/null +++ b/valid/labels/SampleV1_2_mp4-35_jpg.rf.112706bdf7b84566f9b8fa03084da685.txt @@ -0,0 +1,5 @@ +2 0.80234375 0.8703125 0.1265625 0.0640625 +2 0.79375 0.134375 0.17734375 0.04296875 +0 0.51015625 0.13671875 0.73984375 0.04140625 +1 0.4875 0.47265625 0.73359375 0.046875 +0 0.49453125 0.8734375 0.72421875 0.0453125 diff --git a/valid/labels/SampleV1_2_mp4-36_jpg.rf.243306d36dee214682f24787ba17c637.txt b/valid/labels/SampleV1_2_mp4-36_jpg.rf.243306d36dee214682f24787ba17c637.txt new file mode 100644 index 0000000000000000000000000000000000000000..b5f83ca1d0601943995a697f8fb9d31ebadadb67 --- /dev/null +++ b/valid/labels/SampleV1_2_mp4-36_jpg.rf.243306d36dee214682f24787ba17c637.txt @@ -0,0 +1,6 @@ +1 0.703125 0.125 0.59375 0.04140625 +1 0.11484375 0.1078125 0.2296875 0.04453125 +1 0.1046875 0.4796875 0.209375 0.0375 +1 0.6875 0.45390625 0.625 0.0359375 +1 0.09765625 0.87890625 0.1953125 0.0390625 +1 0.68671875 0.85 0.6265625 0.04140625 diff --git a/valid/labels/SampleV1_2_mp4-41_jpg.rf.20229b120f1103fdb06ecbde078fe63f.txt b/valid/labels/SampleV1_2_mp4-41_jpg.rf.20229b120f1103fdb06ecbde078fe63f.txt new file mode 100644 index 0000000000000000000000000000000000000000..b87eed64a8191c3680824ae7ef29acdcab3ec853 --- /dev/null +++ b/valid/labels/SampleV1_2_mp4-41_jpg.rf.20229b120f1103fdb06ecbde078fe63f.txt @@ -0,0 +1,8 @@ +2 0.0921875 0.27734375 0.08984375 0.0390625 +1 0.91953125 0.2515625 0.11484375 0.2484375 +1 0.53203125 0.2734375 0.07109375 0.25234375 +0 0.09296875 0.3015625 0.1015625 0.24609375 +1 0.19609375 0.60546875 0.11328125 0.24765625 +1 0.62109375 0.5734375 0.0921875 0.240625 +1 0.9640625 0.55546875 0.071875 0.2453125 +1 0.27734375 0.90546875 0.06640625 0.1890625 diff --git a/valid/labels/SampleV1_2_mp4-42_jpg.rf.9210f4e128753895cb12a47cde84068d.txt b/valid/labels/SampleV1_2_mp4-42_jpg.rf.9210f4e128753895cb12a47cde84068d.txt new file mode 100644 index 0000000000000000000000000000000000000000..2fe94607599f185fa43a86666093f08b496439a8 --- /dev/null +++ b/valid/labels/SampleV1_2_mp4-42_jpg.rf.9210f4e128753895cb12a47cde84068d.txt @@ -0,0 +1,7 @@ +1 0.1328125 0.28046875 0.03984375 0.2125 +1 0.51015625 0.28046875 0.03359375 0.215625 +1 0.8375 0.2859375 0.053125 0.2109375 +1 0.171875 0.5453125 0.0453125 0.21015625 +1 0.53828125 0.5421875 0.04375 0.2046875 +1 0.83515625 0.54765625 0.04140625 0.2046875 +1 0.18125 0.83125 0.03046875 0.21484375 diff --git a/valid/labels/SampleV1_2_mp4-5_jpg.rf.16bb7a236edddcaeb6d32772e9383599.txt b/valid/labels/SampleV1_2_mp4-5_jpg.rf.16bb7a236edddcaeb6d32772e9383599.txt new file mode 100644 index 0000000000000000000000000000000000000000..c93a32ebfc9dba3ec3c5990bd61e08d72151f754 --- /dev/null +++ b/valid/labels/SampleV1_2_mp4-5_jpg.rf.16bb7a236edddcaeb6d32772e9383599.txt @@ -0,0 +1,5 @@ +2 0.4921875 0.11328125 0.21015625 0.0859375 +2 0.49375 0.3296875 0.25390625 0.11171875 +2 0.5640625 0.459375 0.08984375 0.05078125 +2 0.575 0.959375 0.0875 0.0765625 +0 0.49375 0.41796875 0.13828125 0.6796875 diff --git a/valid/labels/SampleV2_1_mp4-19_jpg.rf.60b093f1d55ac66be3bfe89287952b36.txt b/valid/labels/SampleV2_1_mp4-19_jpg.rf.60b093f1d55ac66be3bfe89287952b36.txt new file mode 100644 index 0000000000000000000000000000000000000000..e182386dfdc0acfe5f376575ddad13665ff743f1 --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-19_jpg.rf.60b093f1d55ac66be3bfe89287952b36.txt @@ -0,0 +1,6 @@ +2 0.7140625 0.38984375 0.0921875 0.20234375 +2 0.19453125 0.37890625 0.0453125 0.15625 +0 0.71953125 0.390625 0.3953125 0.1484375 +0 0.1046875 0.45625 0.209375 0.15078125 +1 0.63828125 0.02734375 0.29609375 0.05078125 +1 0.16015625 0.096875 0.3203125 0.08046875 diff --git a/valid/labels/SampleV2_1_mp4-26_jpg.rf.a8431cb1acce1c55d32861c982c2a16a.txt b/valid/labels/SampleV2_1_mp4-26_jpg.rf.a8431cb1acce1c55d32861c982c2a16a.txt new file mode 100644 index 0000000000000000000000000000000000000000..158af2efdbfb97b2eec538ee1f16e7c27a276542 --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-26_jpg.rf.a8431cb1acce1c55d32861c982c2a16a.txt @@ -0,0 +1,4 @@ +2 0.5796875 0.690625 0.075 0.15859375 +2 0.840625 0.5890625 0.06328125 0.19296875 +1 0.58671875 0.22890625 0.46953125 0.09375 +0 0.64375 0.65390625 0.4546875 0.2296875 diff --git a/valid/labels/SampleV2_1_mp4-28_jpg.rf.1135f8b80048837cc4940c2efbb856b9.txt b/valid/labels/SampleV2_1_mp4-28_jpg.rf.1135f8b80048837cc4940c2efbb856b9.txt new file mode 100644 index 0000000000000000000000000000000000000000..5d4eb78de461ec0f1ab2831ca371dd6f2bfbfe5d --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-28_jpg.rf.1135f8b80048837cc4940c2efbb856b9.txt @@ -0,0 +1,5 @@ +2 0.62890625 0.36640625 0.0828125 0.109375 +2 0.83359375 0.2828125 0.06484375 0.16484375 +1 0.1265625 0.23828125 0.240625 0.07578125 +0 0.68359375 0.3171875 0.36484375 0.18671875 +1 0.6296875 0.046875 0.39453125 0.08515625 diff --git a/valid/labels/SampleV2_1_mp4-36_jpg.rf.85bf707647bfe9fb87b897f7c840cf7e.txt b/valid/labels/SampleV2_1_mp4-36_jpg.rf.85bf707647bfe9fb87b897f7c840cf7e.txt new file mode 100644 index 0000000000000000000000000000000000000000..f043a82170cafed17c5b706a2dab65f2110f3cac --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-36_jpg.rf.85bf707647bfe9fb87b897f7c840cf7e.txt @@ -0,0 +1 @@ +1 0.68359375 0.46484375 0.53828125 0.16328125 diff --git a/valid/labels/SampleV2_1_mp4-45_jpg.rf.c87e632bdc4ec4a94271b4eaa6b1a9e0.txt b/valid/labels/SampleV2_1_mp4-45_jpg.rf.c87e632bdc4ec4a94271b4eaa6b1a9e0.txt new file mode 100644 index 0000000000000000000000000000000000000000..2e22d847dee826668b0415716ab6d483aa34659b --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-45_jpg.rf.c87e632bdc4ec4a94271b4eaa6b1a9e0.txt @@ -0,0 +1,3 @@ +2 0.796875 0.12265625 0.05625 0.096875 +0 0.63203125 0.13359375 0.4109375 0.125 +1 0.67734375 0.8140625 0.50234375 0.17734375 diff --git a/valid/labels/SampleV2_1_mp4-46_jpg.rf.ad9473ef8b282d478346a1d1d0abe215.txt b/valid/labels/SampleV2_1_mp4-46_jpg.rf.ad9473ef8b282d478346a1d1d0abe215.txt new file mode 100644 index 0000000000000000000000000000000000000000..f73f4812727179ceb1d8f848b763c130d30b5c09 --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-46_jpg.rf.ad9473ef8b282d478346a1d1d0abe215.txt @@ -0,0 +1,2 @@ +2 0.82109375 0.2625 0.08828125 0.1046875 +0 0.61796875 0.29453125 0.48359375 0.1328125 diff --git a/valid/labels/SampleV2_1_mp4-48_jpg.rf.b34ab60a5e4bee8aec8425096027e52b.txt b/valid/labels/SampleV2_1_mp4-48_jpg.rf.b34ab60a5e4bee8aec8425096027e52b.txt new file mode 100644 index 0000000000000000000000000000000000000000..032838da3716113e571582863eb0ca61bd69b12f --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-48_jpg.rf.b34ab60a5e4bee8aec8425096027e52b.txt @@ -0,0 +1,4 @@ +2 0.89609375 0.7609375 0.1046875 0.17578125 +2 0.6796875 0.1421875 0.13125 0.17265625 +0 0.58125 0.125 0.40703125 0.1140625 +0 0.6171875 0.790625 0.68359375 0.20859375 diff --git a/valid/labels/SampleV2_1_mp4-49_jpg.rf.d72484b42eee037b9e0daa0f11a39098.txt b/valid/labels/SampleV2_1_mp4-49_jpg.rf.d72484b42eee037b9e0daa0f11a39098.txt new file mode 100644 index 0000000000000000000000000000000000000000..222738ed74d24438ae18e96d209340b62b2bd99b --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-49_jpg.rf.d72484b42eee037b9e0daa0f11a39098.txt @@ -0,0 +1,3 @@ +2 0.6765625 0.34609375 0.16328125 0.2578125 +2 0.475 0.29140625 0.053125 0.06171875 +0 0.55546875 0.31484375 0.46796875 0.1171875 diff --git a/valid/labels/SampleV2_1_mp4-54_jpg.rf.4b82e163c6f559e7e83067ae4b6f2858.txt b/valid/labels/SampleV2_1_mp4-54_jpg.rf.4b82e163c6f559e7e83067ae4b6f2858.txt new file mode 100644 index 0000000000000000000000000000000000000000..960f81efb9a77a797ae3ee46a818e846fe33713e --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-54_jpg.rf.4b82e163c6f559e7e83067ae4b6f2858.txt @@ -0,0 +1 @@ +1 0.41640625 0.5953125 0.2109375 0.778125 diff --git a/valid/labels/SampleV2_1_mp4-55_jpg.rf.9e9f1f7134211f2dfeca93c5a5c57d99.txt b/valid/labels/SampleV2_1_mp4-55_jpg.rf.9e9f1f7134211f2dfeca93c5a5c57d99.txt new file mode 100644 index 0000000000000000000000000000000000000000..82f48408ff025cc5208d5c87c4876204d162db04 --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-55_jpg.rf.9e9f1f7134211f2dfeca93c5a5c57d99.txt @@ -0,0 +1 @@ +1 0.40859375 0.4921875 0.078125 0.78984375 diff --git a/valid/labels/SampleV2_1_mp4-58_jpg.rf.e5d60d6bc9052a6da409610cd36d4bd2.txt b/valid/labels/SampleV2_1_mp4-58_jpg.rf.e5d60d6bc9052a6da409610cd36d4bd2.txt new file mode 100644 index 0000000000000000000000000000000000000000..ad47425df0e3e7d1731b881e57de55a79aa28450 --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-58_jpg.rf.e5d60d6bc9052a6da409610cd36d4bd2.txt @@ -0,0 +1,4 @@ +2 0.5796875 0.25546875 0.11875 0.2453125 +2 0.9484375 0.49765625 0.0359375 0.9859375 +1 0.20703125 0.44453125 0.0421875 0.54609375 +0 0.5546875 0.46328125 0.040625 0.78984375 diff --git a/valid/labels/SampleV2_1_mp4-5_jpg.rf.badd9da3a7988f268c5c9560c556f768.txt b/valid/labels/SampleV2_1_mp4-5_jpg.rf.badd9da3a7988f268c5c9560c556f768.txt new file mode 100644 index 0000000000000000000000000000000000000000..c8f941702f4d5da556b97cd152c138bd90019da3 --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-5_jpg.rf.badd9da3a7988f268c5c9560c556f768.txt @@ -0,0 +1,6 @@ +2 0.76328125 0.109375 0.253125 0.06484375 +2 0.95390625 0.5796875 0.0921875 0.20390625 +2 0.3546875 0.60703125 0.08046875 0.096875 +2 0.19375 0.64140625 0.23125 0.08515625 +1 0.328125 0.175 0.2171875 0.08828125 +1 0.7484375 0.58125 0.22578125 0.103125 diff --git a/valid/labels/SampleV2_1_mp4-71_jpg.rf.98f5b29a48e31e04ab640fde74618d72.txt b/valid/labels/SampleV2_1_mp4-71_jpg.rf.98f5b29a48e31e04ab640fde74618d72.txt new file mode 100644 index 0000000000000000000000000000000000000000..537832fd65c5b6e80ae611d96db467bd55d64f43 --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-71_jpg.rf.98f5b29a48e31e04ab640fde74618d72.txt @@ -0,0 +1,4 @@ +1 0.92265625 0.571875 0.0828125 0.85625 +1 0.434375 0.4796875 0.03515625 0.54609375 +1 0.21796875 0.4578125 0.03125 0.46796875 +1 0.10078125 0.4515625 0.02890625 0.375 diff --git a/valid/labels/SampleV2_1_mp4-82_jpg.rf.717570be58e76f0610d63e980ae5a4dd.txt b/valid/labels/SampleV2_1_mp4-82_jpg.rf.717570be58e76f0610d63e980ae5a4dd.txt new file mode 100644 index 0000000000000000000000000000000000000000..e89d29c8818067745659245901f804ebe2e0f1ce --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-82_jpg.rf.717570be58e76f0610d63e980ae5a4dd.txt @@ -0,0 +1,6 @@ +2 0.78125 0.40078125 0.08828125 0.13125 +2 0.78203125 0.71171875 0.0890625 0.1328125 +2 0.31875 0.5546875 0.034375 0.09375 +2 0.321875 0.69921875 0.03515625 0.1234375 +0 0.7734375 0.36640625 0.09609375 0.73203125 +1 0.4078125 0.45390625 0.040625 0.9078125 diff --git a/valid/labels/SampleV2_1_mp4-87_jpg.rf.12980a35d2ca22a764c03f513986835f.txt b/valid/labels/SampleV2_1_mp4-87_jpg.rf.12980a35d2ca22a764c03f513986835f.txt new file mode 100644 index 0000000000000000000000000000000000000000..1861b79ab2e19fe927cf48a1b82ccc48f703139b --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-87_jpg.rf.12980a35d2ca22a764c03f513986835f.txt @@ -0,0 +1,5 @@ +2 0.8953125 0.3140625 0.0953125 0.146875 +2 0.44140625 0.6515625 0.0703125 0.19140625 +2 0.453125 0.2828125 0.05546875 0.09140625 +0 0.9140625 0.45390625 0.09921875 0.8546875 +0 0.4515625 0.47734375 0.0484375 0.69921875 diff --git a/valid/labels/SampleV2_1_mp4-88_jpg.rf.fd634b2771f83a934a475220631b30a1.txt b/valid/labels/SampleV2_1_mp4-88_jpg.rf.fd634b2771f83a934a475220631b30a1.txt new file mode 100644 index 0000000000000000000000000000000000000000..4c075569e831a2a50a818e3d739b08e945e03fab --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-88_jpg.rf.fd634b2771f83a934a475220631b30a1.txt @@ -0,0 +1,5 @@ +2 0.26796875 0.64921875 0.065625 0.16484375 +2 0.26875 0.2703125 0.06953125 0.16640625 +2 0.5859375 0.41796875 0.09375 0.26875 +0 0.58671875 0.434375 0.0609375 0.81328125 +0 0.26875 0.478125 0.05234375 0.5984375 diff --git a/valid/labels/SampleV2_1_mp4-91_jpg.rf.4f34106919c3af160d47423bc01eae9e.txt b/valid/labels/SampleV2_1_mp4-91_jpg.rf.4f34106919c3af160d47423bc01eae9e.txt new file mode 100644 index 0000000000000000000000000000000000000000..1d3a967d692efb2f8c8ba12bf4a75092d8f6068e --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-91_jpg.rf.4f34106919c3af160d47423bc01eae9e.txt @@ -0,0 +1,5 @@ +2 0.2390625 0.3796875 0.0859375 0.18203125 +2 0.05234375 0.53828125 0.05 0.1296875 +0 0.24375 0.3609375 0.04765625 0.6421875 +1 0.5796875 0.5046875 0.04921875 0.91640625 +0 0.05859375 0.39453125 0.05546875 0.4765625 diff --git a/valid/labels/SampleV2_1_mp4-93_jpg.rf.49924234dcc2581222ac782ef2b21389.txt b/valid/labels/SampleV2_1_mp4-93_jpg.rf.49924234dcc2581222ac782ef2b21389.txt new file mode 100644 index 0000000000000000000000000000000000000000..dd2c10ef59778f0cc678cd75b11cdd5989c88249 --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-93_jpg.rf.49924234dcc2581222ac782ef2b21389.txt @@ -0,0 +1,4 @@ +2 0.1078125 0.2859375 0.09296875 0.15625 +1 0.75859375 0.478125 0.1359375 0.95625 +1 0.33515625 0.37734375 0.0390625 0.68671875 +0 0.11171875 0.26484375 0.05859375 0.4890625 diff --git a/valid/labels/SampleV2_1_mp4-95_jpg.rf.d76ce536a429e52ddb09741449a211dc.txt b/valid/labels/SampleV2_1_mp4-95_jpg.rf.d76ce536a429e52ddb09741449a211dc.txt new file mode 100644 index 0000000000000000000000000000000000000000..bd1600fc1712de3a4b1a23ae8ddbbf28604c2784 --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-95_jpg.rf.d76ce536a429e52ddb09741449a211dc.txt @@ -0,0 +1,6 @@ +2 0.45390625 0.4796875 0.0640625 0.8640625 +2 0.1859375 0.4140625 0.03984375 0.57578125 +2 0.02734375 0.31875 0.040625 0.44296875 +0 0.465625 0.471875 0.08046875 0.8515625 +0 0.18984375 0.40859375 0.03671875 0.58671875 +0 0.02421875 0.31171875 0.0328125 0.44765625 diff --git a/valid/labels/SampleV2_1_mp4-98_jpg.rf.5665e70a4b1e0bf9b2ac6290814a6a5a.txt b/valid/labels/SampleV2_1_mp4-98_jpg.rf.5665e70a4b1e0bf9b2ac6290814a6a5a.txt new file mode 100644 index 0000000000000000000000000000000000000000..49a1ab57bcafefb23219a376c057a161adc2bcc8 --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-98_jpg.rf.5665e70a4b1e0bf9b2ac6290814a6a5a.txt @@ -0,0 +1,4 @@ +2 0.403125 0.36796875 0.07890625 0.653125 +2 0.159375 0.3421875 0.0390625 0.60625 +0 0.4078125 0.3421875 0.09765625 0.66796875 +0 0.15546875 0.3171875 0.06796875 0.61875 diff --git a/valid/labels/SampleV2_1_mp4-9_jpg.rf.521adae90867d781ba8bab0b885692d7.txt b/valid/labels/SampleV2_1_mp4-9_jpg.rf.521adae90867d781ba8bab0b885692d7.txt new file mode 100644 index 0000000000000000000000000000000000000000..e1c9801bedd6d14320fde42cfbdcc4bba8221c0e --- /dev/null +++ b/valid/labels/SampleV2_1_mp4-9_jpg.rf.521adae90867d781ba8bab0b885692d7.txt @@ -0,0 +1,5 @@ +2 0.7765625 0.47890625 0.16328125 0.11875 +2 0.5578125 0.4734375 0.1421875 0.09296875 +1 0.62734375 0.07578125 0.309375 0.09296875 +1 0.08828125 0.52734375 0.1734375 0.07890625 +1 0.14609375 0.1046875 0.265625 0.06171875 diff --git a/valid/labels/SampleV2_2_mp4-0_jpg.rf.275b3da454b64e55ad0487ac2e0f7e48.txt b/valid/labels/SampleV2_2_mp4-0_jpg.rf.275b3da454b64e55ad0487ac2e0f7e48.txt new file mode 100644 index 0000000000000000000000000000000000000000..9a55092376fb3479ce9b179e33e88bd2642e3c16 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-0_jpg.rf.275b3da454b64e55ad0487ac2e0f7e48.txt @@ -0,0 +1,17 @@ +2 0.13515625 0.63984375 0.2125 0.0640625 +2 0.8984375 0.153125 0.053125 0.0671875 +2 0.8296875 0.378125 0.0578125 0.08359375 +2 0.94375 0.378125 0.04765625 0.07734375 +2 0.3328125 0.1578125 0.034375 0.04375 +1 0.5125 0.71171875 0.253125 0.075 +1 0.92265625 0.71171875 0.1546875 0.046875 +0 0.1171875 0.640625 0.23359375 0.084375 +1 0.21171875 0.33984375 0.18046875 0.0515625 +0 0.2734375 0.15703125 0.15234375 0.03125 +1 0.5296875 0.365625 0.171875 0.059375 +1 0.56015625 0.1703125 0.16015625 0.04296875 +0 0.89765625 0.37890625 0.2015625 0.0546875 +0 0.85390625 0.15625 0.18671875 0.05 +1 0.55859375 0.02890625 0.13984375 0.04765625 +1 0.31640625 0.0265625 0.128125 0.0296875 +1 0.821875 0.01484375 0.14375 0.0296875 diff --git a/valid/labels/SampleV2_2_mp4-101_jpg.rf.b5fd5a9e856ef2919a7c22033dd1cc16.txt b/valid/labels/SampleV2_2_mp4-101_jpg.rf.b5fd5a9e856ef2919a7c22033dd1cc16.txt new file mode 100644 index 0000000000000000000000000000000000000000..32ffcd412a77f8b9cb0c44c14ff5b7691191e783 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-101_jpg.rf.b5fd5a9e856ef2919a7c22033dd1cc16.txt @@ -0,0 +1,5 @@ +2 0.97265625 0.4609375 0.053125 0.921875 +2 0.265625 0.49765625 0.03828125 0.4890625 +0 0.9703125 0.46953125 0.059375 0.9390625 +1 0.534375 0.465625 0.06484375 0.68046875 +0 0.26796875 0.48671875 0.04140625 0.5140625 diff --git a/valid/labels/SampleV2_2_mp4-104_jpg.rf.5ede669ef4e216cd3fac3a9064dba352.txt b/valid/labels/SampleV2_2_mp4-104_jpg.rf.5ede669ef4e216cd3fac3a9064dba352.txt new file mode 100644 index 0000000000000000000000000000000000000000..e9cf2d8074770d0308f69b9fb3fa7983a1a86f91 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-104_jpg.rf.5ede669ef4e216cd3fac3a9064dba352.txt @@ -0,0 +1,6 @@ +2 0.38203125 0.190625 0.02734375 0.38046875 +2 0.92734375 0.14140625 0.0390625 0.2796875 +0 0.3828125 0.1921875 0.02734375 0.384375 +1 0.60703125 0.1671875 0.03671875 0.334375 +0 0.92890625 0.14609375 0.03671875 0.29140625 +1 0.5234375 0.87265625 0.0375 0.2546875 diff --git a/valid/labels/SampleV2_2_mp4-105_jpg.rf.411567f9f03bbc9edd2e7593e547130a.txt b/valid/labels/SampleV2_2_mp4-105_jpg.rf.411567f9f03bbc9edd2e7593e547130a.txt new file mode 100644 index 0000000000000000000000000000000000000000..17b56c3e93ae396251e3137ac307eaca23c367c5 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-105_jpg.rf.411567f9f03bbc9edd2e7593e547130a.txt @@ -0,0 +1,7 @@ +2 0.3171875 0.1171875 0.0265625 0.23125 +2 0.67890625 0.08125 0.03125 0.15625 +0 0.31796875 0.11796875 0.02578125 0.2359375 +1 0.47578125 0.0984375 0.0296875 0.196875 +0 0.678125 0.07890625 0.028125 0.1578125 +1 0.41640625 0.70546875 0.03515625 0.3765625 +1 0.65859375 0.784375 0.03515625 0.43046875 diff --git a/valid/labels/SampleV2_2_mp4-106_jpg.rf.377879e04f1e7209a3aa340ccfe1084b.txt b/valid/labels/SampleV2_2_mp4-106_jpg.rf.377879e04f1e7209a3aa340ccfe1084b.txt new file mode 100644 index 0000000000000000000000000000000000000000..fefc7a8409c1305c76581f78640041c3f66a1096 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-106_jpg.rf.377879e04f1e7209a3aa340ccfe1084b.txt @@ -0,0 +1,9 @@ +2 0.23828125 0.0921875 0.0265625 0.18359375 +2 0.50859375 0.06875 0.025 0.1375 +2 0.7421875 0.71875 0.05625 0.45546875 +0 0.74296875 0.71875 0.0515625 0.4734375 +1 0.49296875 0.66484375 0.03125 0.3921875 +1 0.31171875 0.584375 0.025 0.31640625 +0 0.23984375 0.090625 0.02890625 0.18125 +1 0.365625 0.07890625 0.02890625 0.15703125 +0 0.50859375 0.071875 0.025 0.14375 diff --git a/valid/labels/SampleV2_2_mp4-107_jpg.rf.6246eabc13b91626965a27f1f15e66da.txt b/valid/labels/SampleV2_2_mp4-107_jpg.rf.6246eabc13b91626965a27f1f15e66da.txt new file mode 100644 index 0000000000000000000000000000000000000000..e8f2e4d7b7b3ba8bb17e75f2f1d88ae55b5da023 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-107_jpg.rf.6246eabc13b91626965a27f1f15e66da.txt @@ -0,0 +1,10 @@ +2 0.190625 0.0828125 0.0234375 0.16484375 +2 0.4234375 0.06953125 0.025 0.1390625 +0 0.19140625 0.08359375 0.0234375 0.16640625 +1 0.303125 0.0734375 0.02578125 0.146875 +0 0.42109375 0.071875 0.0296875 0.14375 +1 0.61640625 0.06015625 0.03046875 0.1203125 +1 0.25625 0.5328125 0.0265625 0.28828125 +1 0.40546875 0.61171875 0.028125 0.35 +1 0.6 0.6515625 0.0453125 0.41328125 +1 0.88125 0.775 0.04453125 0.44765625 diff --git a/valid/labels/SampleV2_2_mp4-15_jpg.rf.c9369ba7c201f092d921fc2c194acced.txt b/valid/labels/SampleV2_2_mp4-15_jpg.rf.c9369ba7c201f092d921fc2c194acced.txt new file mode 100644 index 0000000000000000000000000000000000000000..ddbbfd96cdd4872feb781f9f275c9ac7694d31fc --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-15_jpg.rf.c9369ba7c201f092d921fc2c194acced.txt @@ -0,0 +1,3 @@ +2 0.51171875 0.42109375 0.2671875 0.1109375 +2 0.63046875 0.97265625 0.359375 0.05390625 +0 0.546875 0.421875 0.33828125 0.09140625 diff --git a/valid/labels/SampleV2_2_mp4-16_jpg.rf.f4bbcada5f40bce4df39a976db8dc142.txt b/valid/labels/SampleV2_2_mp4-16_jpg.rf.f4bbcada5f40bce4df39a976db8dc142.txt new file mode 100644 index 0000000000000000000000000000000000000000..0c8f45dca2fd835d5583de1909faab2f75102f90 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-16_jpg.rf.f4bbcada5f40bce4df39a976db8dc142.txt @@ -0,0 +1,4 @@ +2 0.521875 0.3046875 0.21953125 0.09140625 +2 0.0515625 0.6125 0.10234375 0.0859375 +0 0.5515625 0.30390625 0.29921875 0.07421875 +1 0.5796875 0.7796875 0.40859375 0.1359375 diff --git a/valid/labels/SampleV2_2_mp4-1_jpg.rf.73ea0781472fb5d74992d45f7ca0c1fc.txt b/valid/labels/SampleV2_2_mp4-1_jpg.rf.73ea0781472fb5d74992d45f7ca0c1fc.txt new file mode 100644 index 0000000000000000000000000000000000000000..10f19e390cdef1fe6445394de779219f7e34a9d5 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-1_jpg.rf.73ea0781472fb5d74992d45f7ca0c1fc.txt @@ -0,0 +1,16 @@ +2 0.159375 0.68828125 0.07578125 0.08046875 +2 0.9078125 0.18828125 0.04921875 0.06796875 +2 0.84140625 0.41953125 0.06484375 0.08671875 +2 0.97578125 0.78125 0.04296875 0.06796875 +0 0.1109375 0.69296875 0.2109375 0.1015625 +1 0.51171875 0.771875 0.2609375 0.08359375 +0 0.92578125 0.77734375 0.1484375 0.06640625 +0 0.90390625 0.415625 0.1921875 0.06640625 +1 0.53125 0.40234375 0.1828125 0.06640625 +1 0.2015625 0.38125 0.19375 0.06171875 +1 0.265625 0.18828125 0.15859375 0.04296875 +1 0.559375 0.196875 0.16484375 0.04765625 +0 0.8625 0.1859375 0.19453125 0.06015625 +1 0.30859375 0.04375 0.13359375 0.03203125 +1 0.5578125 0.04765625 0.1453125 0.04609375 +1 0.828125 0.03125 0.15625 0.03671875 diff --git a/valid/labels/SampleV2_2_mp4-20_jpg.rf.adbaddd455765d21603b4a34045f79ba.txt b/valid/labels/SampleV2_2_mp4-20_jpg.rf.adbaddd455765d21603b4a34045f79ba.txt new file mode 100644 index 0000000000000000000000000000000000000000..5c60510f6f84f9160653ec5902b888a268f3cbda --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-20_jpg.rf.adbaddd455765d21603b4a34045f79ba.txt @@ -0,0 +1,9 @@ +2 0.0953125 0.20859375 0.178125 0.08359375 +2 0.4765625 0.0203125 0.13359375 0.03984375 +2 0.409375 0.60546875 0.12265625 0.09375 +2 0.68828125 0.57421875 0.07734375 0.1015625 +0 0.53671875 0.58984375 0.371875 0.1046875 +1 0.52421875 0.24921875 0.2734375 0.09140625 +0 0.09375 0.20625 0.1875 0.07890625 +0 0.5078125 0.01796875 0.2 0.03515625 +1 0.03203125 0.6234375 0.06328125 0.06953125 diff --git a/valid/labels/SampleV2_2_mp4-27_jpg.rf.a7ae2be75ede72849af7cdaa224b1e8c.txt b/valid/labels/SampleV2_2_mp4-27_jpg.rf.a7ae2be75ede72849af7cdaa224b1e8c.txt new file mode 100644 index 0000000000000000000000000000000000000000..60a43d714fd6df4be7b43574e1f4c26fb6196807 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-27_jpg.rf.a7ae2be75ede72849af7cdaa224b1e8c.txt @@ -0,0 +1,6 @@ +2 0.5875 0.0796875 0.071875 0.09140625 +2 0.409375 0.496875 0.14765625 0.1140625 +2 0.08046875 0.11484375 0.15859375 0.06015625 +0 0.53046875 0.08359375 0.296875 0.07109375 +0 0.5390625 0.49609375 0.4 0.1125 +0 0.084375 0.1125 0.16875 0.06484375 diff --git a/valid/labels/SampleV2_2_mp4-28_jpg.rf.f6b19083b855e5fc84d22389a10fce73.txt b/valid/labels/SampleV2_2_mp4-28_jpg.rf.f6b19083b855e5fc84d22389a10fce73.txt new file mode 100644 index 0000000000000000000000000000000000000000..a9f6d980200ca05184d9f12c29e665ab24d75734 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-28_jpg.rf.f6b19083b855e5fc84d22389a10fce73.txt @@ -0,0 +1,8 @@ +2 0.59453125 0.0640625 0.0671875 0.08203125 +2 0.46953125 0.06953125 0.16875 0.08046875 +2 0.090625 0.08359375 0.18125 0.0734375 +2 0.4328125 0.4125 0.1375 0.08203125 +2 0.62421875 0.41015625 0.19453125 0.0953125 +0 0.09296875 0.08671875 0.1859375 0.05390625 +0 0.5265625 0.06328125 0.2828125 0.07109375 +0 0.54921875 0.409375 0.3671875 0.08828125 diff --git a/valid/labels/SampleV2_2_mp4-3_jpg.rf.777e550ce73ebc75d9a55fcbd5be63ad.txt b/valid/labels/SampleV2_2_mp4-3_jpg.rf.777e550ce73ebc75d9a55fcbd5be63ad.txt new file mode 100644 index 0000000000000000000000000000000000000000..7b5e53f156e8797c11f27d1ac613067dc90ea552 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-3_jpg.rf.777e550ce73ebc75d9a55fcbd5be63ad.txt @@ -0,0 +1,16 @@ +2 0.94765625 0.26640625 0.04921875 0.07265625 +2 0.0890625 0.85078125 0.17734375 0.06953125 +2 0.8828125 0.540625 0.07734375 0.06953125 +2 0.10078125 0.4703125 0.06796875 0.06171875 +0 0.090625 0.8484375 0.18125 0.075 +0 0.1703125 0.47265625 0.2078125 0.06015625 +1 0.24453125 0.24921875 0.171875 0.03515625 +1 0.2953125 0.090625 0.1453125 0.03828125 +1 0.5609375 0.103125 0.153125 0.05546875 +1 0.5640625 0.27265625 0.178125 0.05078125 +1 0.53203125 0.5078125 0.19921875 0.06484375 +1 0.50625 0.9578125 0.29375 0.084375 +1 0.85546875 0.0921875 0.16796875 0.04140625 +0 0.890625 0.259375 0.20390625 0.06484375 +0 0.92265625 0.54375 0.1546875 0.06015625 +1 0.9515625 0.97578125 0.096875 0.0453125 diff --git a/valid/labels/SampleV2_2_mp4-43_jpg.rf.fd1bb2c4d44428af450b9edfaed846e1.txt b/valid/labels/SampleV2_2_mp4-43_jpg.rf.fd1bb2c4d44428af450b9edfaed846e1.txt new file mode 100644 index 0000000000000000000000000000000000000000..dd3af6cf65630e0c1f6af4153c7080f3495927c3 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-43_jpg.rf.fd1bb2c4d44428af450b9edfaed846e1.txt @@ -0,0 +1,8 @@ +2 0.35703125 0.6953125 0.21171875 0.07890625 +2 0.059375 0.24453125 0.11796875 0.05703125 +2 0.89453125 0.0328125 0.209375 0.065625 +0 0.05625 0.2390625 0.1125 0.053125 +1 0.4859375 0.215625 0.2765625 0.09375 +0 0.46171875 0.665625 0.43046875 0.15859375 +0 0.89375 0.03359375 0.2125 0.0671875 +1 0.94296875 0.24921875 0.1140625 0.0765625 diff --git a/valid/labels/SampleV2_2_mp4-49_jpg.rf.cf91f96af558247185905d18a0c96df1.txt b/valid/labels/SampleV2_2_mp4-49_jpg.rf.cf91f96af558247185905d18a0c96df1.txt new file mode 100644 index 0000000000000000000000000000000000000000..c5d558ed3efd817c2a0c4d702f35faffe2280d97 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-49_jpg.rf.cf91f96af558247185905d18a0c96df1.txt @@ -0,0 +1 @@ +1 0.50390625 0.4171875 0.44609375 0.109375 diff --git a/valid/labels/SampleV2_2_mp4-52_jpg.rf.a90ead5d9dacc59cddd183bf89be0433.txt b/valid/labels/SampleV2_2_mp4-52_jpg.rf.a90ead5d9dacc59cddd183bf89be0433.txt new file mode 100644 index 0000000000000000000000000000000000000000..66dc2566edb981d1c9350854e21b24681328c807 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-52_jpg.rf.a90ead5d9dacc59cddd183bf89be0433.txt @@ -0,0 +1,2 @@ +2 0.5046875 0.33984375 0.28125 0.1234375 +0 0.57421875 0.33515625 0.44765625 0.09296875 diff --git a/valid/labels/SampleV2_2_mp4-56_jpg.rf.78b4cbd8ba2c948c2e519ebe3998efe5.txt b/valid/labels/SampleV2_2_mp4-56_jpg.rf.78b4cbd8ba2c948c2e519ebe3998efe5.txt new file mode 100644 index 0000000000000000000000000000000000000000..0835418e3ef9fd9b4795c06ca61b8a0d5330b2ba --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-56_jpg.rf.78b4cbd8ba2c948c2e519ebe3998efe5.txt @@ -0,0 +1,2 @@ +1 0.68828125 0.0859375 0.38515625 0.05390625 +1 0.7015625 0.55 0.596875 0.128125 diff --git a/valid/labels/SampleV2_2_mp4-64_jpg.rf.a6717af4b97678b3c8c51b61b9c31ae6.txt b/valid/labels/SampleV2_2_mp4-64_jpg.rf.a6717af4b97678b3c8c51b61b9c31ae6.txt new file mode 100644 index 0000000000000000000000000000000000000000..3444f3991aac693d2529625ce5d6825aeba3120d --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-64_jpg.rf.a6717af4b97678b3c8c51b61b9c31ae6.txt @@ -0,0 +1,5 @@ +2 0.815625 0.47734375 0.07734375 0.2703125 +2 0.80625 0.93828125 0.08125 0.1234375 +0 0.81640625 0.54921875 0.07265625 0.8703125 +1 0.4296875 0.40546875 0.0546875 0.609375 +1 0.2515625 0.32890625 0.03515625 0.45703125 diff --git a/valid/labels/SampleV2_2_mp4-70_jpg.rf.b9880314f27f844543ecf94cbe119936.txt b/valid/labels/SampleV2_2_mp4-70_jpg.rf.b9880314f27f844543ecf94cbe119936.txt new file mode 100644 index 0000000000000000000000000000000000000000..1c7ff2fc6bc65ec8475e37e763960dd7f5995f98 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-70_jpg.rf.b9880314f27f844543ecf94cbe119936.txt @@ -0,0 +1,5 @@ +2 0.48671875 0.7171875 0.0515625 0.33203125 +2 0.92578125 0.22734375 0.08515625 0.21484375 +0 0.92734375 0.559375 0.06640625 0.878125 +0 0.4953125 0.56875 0.0671875 0.653125 +1 0.2421875 0.46875 0.0375 0.4890625 diff --git a/valid/labels/SampleV2_2_mp4-72_jpg.rf.bf98b4a834e88a1cf6ca44d2c1bd8433.txt b/valid/labels/SampleV2_2_mp4-72_jpg.rf.bf98b4a834e88a1cf6ca44d2c1bd8433.txt new file mode 100644 index 0000000000000000000000000000000000000000..03dd10d1932af44394bcb2f236a1717e7aaa1df9 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-72_jpg.rf.bf98b4a834e88a1cf6ca44d2c1bd8433.txt @@ -0,0 +1,2 @@ +1 0.8125 0.62734375 0.06796875 0.7421875 +1 0.37578125 0.58046875 0.04921875 0.6328125 diff --git a/valid/labels/SampleV2_2_mp4-79_jpg.rf.46674fcdba85463e3a72275eb64e9a60.txt b/valid/labels/SampleV2_2_mp4-79_jpg.rf.46674fcdba85463e3a72275eb64e9a60.txt new file mode 100644 index 0000000000000000000000000000000000000000..8be364fccb3a9b3decae43ed951c865b59003abb --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-79_jpg.rf.46674fcdba85463e3a72275eb64e9a60.txt @@ -0,0 +1,2 @@ +1 0.3265625 0.48515625 0.04609375 0.5171875 +1 0.65 0.559375 0.0609375 0.7484375 diff --git a/valid/labels/SampleV2_2_mp4-81_jpg.rf.77d49a43c4179a3aa7f9030f87dabbd7.txt b/valid/labels/SampleV2_2_mp4-81_jpg.rf.77d49a43c4179a3aa7f9030f87dabbd7.txt new file mode 100644 index 0000000000000000000000000000000000000000..1a219a2cecbce6796a222b14d6bf7b6775a43047 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-81_jpg.rf.77d49a43c4179a3aa7f9030f87dabbd7.txt @@ -0,0 +1,4 @@ +2 0.78671875 0.23828125 0.0640625 0.353125 +1 0.1984375 0.40859375 0.04296875 0.43515625 +1 0.4078125 0.48046875 0.0375 0.57890625 +0 0.7671875 0.4796875 0.090625 0.83046875 diff --git a/valid/labels/SampleV2_2_mp4-85_jpg.rf.c362dd8c973cea60f136c5996b0fd398.txt b/valid/labels/SampleV2_2_mp4-85_jpg.rf.c362dd8c973cea60f136c5996b0fd398.txt new file mode 100644 index 0000000000000000000000000000000000000000..e112a40426ecd41301da317940ec089fc43bcf51 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-85_jpg.rf.c362dd8c973cea60f136c5996b0fd398.txt @@ -0,0 +1,4 @@ +1 0.5265625 0.4078125 0.05625 0.66796875 +1 0.28046875 0.32265625 0.0453125 0.509375 +1 0.1265625 0.3484375 0.04453125 0.43515625 +1 0.92578125 0.4953125 0.04296875 0.990625 diff --git a/valid/labels/SampleV2_2_mp4-86_jpg.rf.19aea41c47d1e1780f1929e3fbdd2885.txt b/valid/labels/SampleV2_2_mp4-86_jpg.rf.19aea41c47d1e1780f1929e3fbdd2885.txt new file mode 100644 index 0000000000000000000000000000000000000000..6f5b5be296f329608ffb37ac63b05007cf63ea23 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-86_jpg.rf.19aea41c47d1e1780f1929e3fbdd2885.txt @@ -0,0 +1,4 @@ +1 0.07265625 0.31953125 0.03828125 0.4015625 +1 0.1984375 0.29609375 0.04609375 0.475 +1 0.4 0.36875 0.053125 0.59296875 +1 0.91796875 0.4765625 0.0546875 0.94453125 diff --git a/valid/labels/SampleV2_2_mp4-92_jpg.rf.15cfce2d493dc6a68332c975e9a7963f.txt b/valid/labels/SampleV2_2_mp4-92_jpg.rf.15cfce2d493dc6a68332c975e9a7963f.txt new file mode 100644 index 0000000000000000000000000000000000000000..4164f4f649441c3a1d1548613fa9e3cf4cd738d5 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-92_jpg.rf.15cfce2d493dc6a68332c975e9a7963f.txt @@ -0,0 +1,7 @@ +2 0.33203125 0.49609375 0.04921875 0.45859375 +2 0.13203125 0.29921875 0.05 0.1140625 +2 0.121875 0.55703125 0.046875 0.18515625 +1 0.71015625 0.5046875 0.071875 0.8484375 +0 0.3328125 0.453125 0.04453125 0.55390625 +0 0.125 0.40703125 0.04296875 0.46875 +1 0.01015625 0.3828125 0.0203125 0.3640625 diff --git a/valid/labels/SampleV2_2_mp4-95_jpg.rf.86acaf1d7f3a8beaa664fbb3f99c6350.txt b/valid/labels/SampleV2_2_mp4-95_jpg.rf.86acaf1d7f3a8beaa664fbb3f99c6350.txt new file mode 100644 index 0000000000000000000000000000000000000000..e9e46d0984f7ee22a4859f9a5adfc0eaf424d7a5 --- /dev/null +++ b/valid/labels/SampleV2_2_mp4-95_jpg.rf.86acaf1d7f3a8beaa664fbb3f99c6350.txt @@ -0,0 +1,7 @@ +2 0.74765625 0.76484375 0.09609375 0.2640625 +2 0.34453125 0.3078125 0.06640625 0.1375 +2 0.3375 0.49921875 0.0546875 0.16171875 +0 0.7484375 0.48671875 0.0671875 0.84375 +0 0.34453125 0.44140625 0.06640625 0.6296875 +1 0.1484375 0.39375 0.04296875 0.471875 +1 0.04609375 0.384375 0.040625 0.3828125 diff --git a/valid/labels/SampleV3_1_mp4-0_jpg.rf.1d6bb718f5b356b490d3e25bf179a479.txt b/valid/labels/SampleV3_1_mp4-0_jpg.rf.1d6bb718f5b356b490d3e25bf179a479.txt new file mode 100644 index 0000000000000000000000000000000000000000..5686c2558b66d7b384960dc1f5abeb56dcc3d4f8 --- /dev/null +++ b/valid/labels/SampleV3_1_mp4-0_jpg.rf.1d6bb718f5b356b490d3e25bf179a479.txt @@ -0,0 +1,11 @@ +1 0.11171875 0.2 0.0390625 0.165625 +1 0.36484375 0.209375 0.0359375 0.16328125 +1 0.6015625 0.2109375 0.02421875 0.16328125 +1 0.853125 0.2109375 0.034375 0.1609375 +1 0.11953125 0.428125 0.0296875 0.1546875 +1 0.3640625 0.4328125 0.028125 0.1515625 +1 0.5984375 0.43359375 0.0265625 0.159375 +1 0.8546875 0.4296875 0.03984375 0.12265625 +1 0.1328125 0.63984375 0.0328125 0.16171875 +1 0.37265625 0.64140625 0.0328125 0.15 +1 0.6109375 0.65234375 0.0328125 0.15546875 diff --git a/valid/labels/SampleV3_1_mp4-13_jpg.rf.9c722bb64ecb60b5e2e3fa62e36ce412.txt b/valid/labels/SampleV3_1_mp4-13_jpg.rf.9c722bb64ecb60b5e2e3fa62e36ce412.txt new file mode 100644 index 0000000000000000000000000000000000000000..a412b393ce49daa362564fb20af76bb33a737dce --- /dev/null +++ b/valid/labels/SampleV3_1_mp4-13_jpg.rf.9c722bb64ecb60b5e2e3fa62e36ce412.txt @@ -0,0 +1,2 @@ +2 0.496875 0.57578125 0.140625 0.06796875 +0 0.48984375 0.4984375 0.10390625 0.49453125 diff --git a/valid/labels/SampleV3_1_mp4-19_jpg.rf.a000296df89ca8e3f1b1baca1a561389.txt b/valid/labels/SampleV3_1_mp4-19_jpg.rf.a000296df89ca8e3f1b1baca1a561389.txt new file mode 100644 index 0000000000000000000000000000000000000000..00bb1030f2b1805366c09c80e8e109d716e29580 --- /dev/null +++ b/valid/labels/SampleV3_1_mp4-19_jpg.rf.a000296df89ca8e3f1b1baca1a561389.txt @@ -0,0 +1,2 @@ +1 0.50625 0.50625 0.121875 0.4453125 +1 0.4578125 0.95546875 0.06171875 0.08828125 diff --git a/valid/labels/SampleV3_1_mp4-21_jpg.rf.94ea729bd33cfe09509abe9746d1f593.txt b/valid/labels/SampleV3_1_mp4-21_jpg.rf.94ea729bd33cfe09509abe9746d1f593.txt new file mode 100644 index 0000000000000000000000000000000000000000..e01c6fad3c97f721d50989b1d59fe090e83d7f60 --- /dev/null +++ b/valid/labels/SampleV3_1_mp4-21_jpg.rf.94ea729bd33cfe09509abe9746d1f593.txt @@ -0,0 +1,2 @@ +1 0.421875 0.5 0.096875 0.45078125 +1 0.4125 0.95703125 0.078125 0.0859375 diff --git a/valid/labels/SampleV3_1_mp4-26_jpg.rf.406222f5b42747032789348c97722061.txt b/valid/labels/SampleV3_1_mp4-26_jpg.rf.406222f5b42747032789348c97722061.txt new file mode 100644 index 0000000000000000000000000000000000000000..1dd4f8cc8938d56232cf26fc6242edfdb51ea259 --- /dev/null +++ b/valid/labels/SampleV3_1_mp4-26_jpg.rf.406222f5b42747032789348c97722061.txt @@ -0,0 +1,3 @@ +1 0.46484375 0.12734375 0.1109375 0.2546875 +1 0.54609375 0.70078125 0.1265625 0.4921875 +1 0.471875 0.20234375 0.11796875 0.12109375 diff --git a/valid/labels/SampleV3_1_mp4-48_jpg.rf.130e02397dda7755ed0b3cf1a78e3a79.txt b/valid/labels/SampleV3_1_mp4-48_jpg.rf.130e02397dda7755ed0b3cf1a78e3a79.txt new file mode 100644 index 0000000000000000000000000000000000000000..76a2be462995fbfcf83e8060e7eb9f49ae0fb464 --- /dev/null +++ b/valid/labels/SampleV3_1_mp4-48_jpg.rf.130e02397dda7755ed0b3cf1a78e3a79.txt @@ -0,0 +1,6 @@ +1 0.8265625 0.20078125 0.34609375 0.04453125 +1 0.1890625 0.2328125 0.378125 0.040625 +1 0.81015625 0.55 0.3796875 0.05625 +1 0.18359375 0.571875 0.36640625 0.046875 +1 0.81640625 0.89765625 0.3671875 0.04296875 +1 0.19375 0.934375 0.3875 0.053125 diff --git a/valid/labels/SampleV3_1_mp4-4_jpg.rf.281e1118cc81d1440d23ec5deeb87e6a.txt b/valid/labels/SampleV3_1_mp4-4_jpg.rf.281e1118cc81d1440d23ec5deeb87e6a.txt new file mode 100644 index 0000000000000000000000000000000000000000..42ccb29e13075c97556cda03f7abf93a429fc9d5 --- /dev/null +++ b/valid/labels/SampleV3_1_mp4-4_jpg.rf.281e1118cc81d1440d23ec5deeb87e6a.txt @@ -0,0 +1,4 @@ +2 0.50859375 0.40546875 0.07578125 0.0921875 +2 0.515625 0.59140625 0.08046875 0.12734375 +0 0.48359375 0.44921875 0.08984375 0.5 +1 0.4546875 0.9546875 0.0640625 0.08984375 diff --git a/valid/labels/SampleV3_1_mp4-5_jpg.rf.006630ee6ce3158adea0bb6954471619.txt b/valid/labels/SampleV3_1_mp4-5_jpg.rf.006630ee6ce3158adea0bb6954471619.txt new file mode 100644 index 0000000000000000000000000000000000000000..6d11c760c841690259c45903b185458bcf9971a0 --- /dev/null +++ b/valid/labels/SampleV3_1_mp4-5_jpg.rf.006630ee6ce3158adea0bb6954471619.txt @@ -0,0 +1,4 @@ +2 0.56328125 0.41796875 0.078125 0.10703125 +2 0.55390625 0.2625 0.078125 0.165625 +0 0.52734375 0.278125 0.10390625 0.525 +1 0.4890625 0.87578125 0.078125 0.2484375 diff --git a/valid/labels/SampleV3_1_mp4-6_jpg.rf.d1126d0aa7e39b053d8e12d06119c038.txt b/valid/labels/SampleV3_1_mp4-6_jpg.rf.d1126d0aa7e39b053d8e12d06119c038.txt new file mode 100644 index 0000000000000000000000000000000000000000..d1f187c79135e2943e73726da2750740ef64bec7 --- /dev/null +++ b/valid/labels/SampleV3_1_mp4-6_jpg.rf.d1126d0aa7e39b053d8e12d06119c038.txt @@ -0,0 +1,3 @@ +2 0.52421875 0.18359375 0.07578125 0.13828125 +0 0.49140625 0.14921875 0.096875 0.2984375 +1 0.46953125 0.76015625 0.08984375 0.47890625 diff --git a/valid/labels/SampleV3_1_mp4-7_jpg.rf.049ce027b075777fecf385949a61911e.txt b/valid/labels/SampleV3_1_mp4-7_jpg.rf.049ce027b075777fecf385949a61911e.txt new file mode 100644 index 0000000000000000000000000000000000000000..6badefc9cd51dfb0669d9852123a6c1593fecaa0 --- /dev/null +++ b/valid/labels/SampleV3_1_mp4-7_jpg.rf.049ce027b075777fecf385949a61911e.txt @@ -0,0 +1,2 @@ +2 0.4859375 0.025 0.14375 0.05 +1 0.465625 0.52890625 0.0734375 0.48984375 diff --git a/valid/labels/SampleV3_1_mp4-9_jpg.rf.5526521eeb01350cd3d7a92666a1fa39.txt b/valid/labels/SampleV3_1_mp4-9_jpg.rf.5526521eeb01350cd3d7a92666a1fa39.txt new file mode 100644 index 0000000000000000000000000000000000000000..079944b8dde65bfb164edbb834f2205bf491518e --- /dev/null +++ b/valid/labels/SampleV3_1_mp4-9_jpg.rf.5526521eeb01350cd3d7a92666a1fa39.txt @@ -0,0 +1,2 @@ +1 0.49609375 0.1703125 0.0734375 0.33984375 +1 0.51953125 0.75859375 0.12109375 0.4828125 diff --git a/valid/labels/SampleV3_2_mp4-16_jpg.rf.195b0f17e1a0d1c707c0d6bca8a14e33.txt b/valid/labels/SampleV3_2_mp4-16_jpg.rf.195b0f17e1a0d1c707c0d6bca8a14e33.txt new file mode 100644 index 0000000000000000000000000000000000000000..997fd1c1ad63c7e1686c1c2ae784f8d94684456e --- /dev/null +++ b/valid/labels/SampleV3_2_mp4-16_jpg.rf.195b0f17e1a0d1c707c0d6bca8a14e33.txt @@ -0,0 +1,2 @@ +1 0.5296875 0.709375 0.121875 0.55078125 +1 0.55 0.046875 0.09453125 0.09375 diff --git a/valid/labels/SampleV3_2_mp4-27_jpg.rf.3ad00580f33975c5a86c0cc806e86da8.txt b/valid/labels/SampleV3_2_mp4-27_jpg.rf.3ad00580f33975c5a86c0cc806e86da8.txt new file mode 100644 index 0000000000000000000000000000000000000000..f04eba389a166fd8acab9f2f81bb049ae7349f29 --- /dev/null +++ b/valid/labels/SampleV3_2_mp4-27_jpg.rf.3ad00580f33975c5a86c0cc806e86da8.txt @@ -0,0 +1,4 @@ +2 0.50859375 0.8640625 0.20546875 0.0875 +2 0.1546875 0.86640625 0.30859375 0.0796875 +1 0.28359375 0.409375 0.5671875 0.059375 +0 0.33828125 0.8640625 0.6765625 0.0640625 diff --git a/valid/labels/SampleV3_2_mp4-5_jpg.rf.b4a8485335e9a43300033ecf1fd13d58.txt b/valid/labels/SampleV3_2_mp4-5_jpg.rf.b4a8485335e9a43300033ecf1fd13d58.txt new file mode 100644 index 0000000000000000000000000000000000000000..e761dfe796bd4aa448013a9cd6bbb34ab776e562 --- /dev/null +++ b/valid/labels/SampleV3_2_mp4-5_jpg.rf.b4a8485335e9a43300033ecf1fd13d58.txt @@ -0,0 +1,4 @@ +2 0.4890625 0.3765625 0.14296875 0.09765625 +2 0.46640625 0.88359375 0.1140625 0.2328125 +0 0.49921875 0.26875 0.11796875 0.5375 +0 0.46328125 0.88203125 0.1203125 0.2359375 diff --git a/valid/labels/Screenshot-2022-12-05-223504_jpeg_jpg.rf.5b9d1fe2f7702f51c2d7add5fb05dbc8.txt b/valid/labels/Screenshot-2022-12-05-223504_jpeg_jpg.rf.5b9d1fe2f7702f51c2d7add5fb05dbc8.txt new file mode 100644 index 0000000000000000000000000000000000000000..436d626fa2858f0400b532935bb0f98f27872c23 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-223504_jpeg_jpg.rf.5b9d1fe2f7702f51c2d7add5fb05dbc8.txt @@ -0,0 +1 @@ +0 0.30703125 0.459375 0.434375 0.8734375 diff --git a/valid/labels/Screenshot-2022-12-05-223526_jpeg.rf.62ffe12406717a1e99af51812c60e2f0.txt b/valid/labels/Screenshot-2022-12-05-223526_jpeg.rf.62ffe12406717a1e99af51812c60e2f0.txt new file mode 100644 index 0000000000000000000000000000000000000000..e00baf785b71ffb259c7f658fa3ceeb4128e57a2 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-223526_jpeg.rf.62ffe12406717a1e99af51812c60e2f0.txt @@ -0,0 +1 @@ +1 0.4984375 0.5 0.996875 0.46484375 diff --git a/valid/labels/Screenshot-2022-12-05-223639_jpeg.rf.86f504360592eab360a0ad9923d695ab.txt b/valid/labels/Screenshot-2022-12-05-223639_jpeg.rf.86f504360592eab360a0ad9923d695ab.txt new file mode 100644 index 0000000000000000000000000000000000000000..2073840c5d30a38d65ed4029ad1576fda4e3bf80 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-223639_jpeg.rf.86f504360592eab360a0ad9923d695ab.txt @@ -0,0 +1 @@ +0 0.51875 0.40625 0.728125 0.8125 diff --git a/valid/labels/Screenshot-2022-12-05-223752_jpeg.rf.7348bf4ffa9f42e3b5f9cecae54904f7.txt b/valid/labels/Screenshot-2022-12-05-223752_jpeg.rf.7348bf4ffa9f42e3b5f9cecae54904f7.txt new file mode 100644 index 0000000000000000000000000000000000000000..1eede7b4524dfdd4d343cd89991fba18526a889a --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-223752_jpeg.rf.7348bf4ffa9f42e3b5f9cecae54904f7.txt @@ -0,0 +1,2 @@ +0 0.49765625 0.49375 0.9953125 0.54140625 +2 0.528125 0.66875 0.89921875 0.1015625 diff --git a/valid/labels/Screenshot-2022-12-05-223809_jpeg.rf.75c76284bef743a4a6af4b483099b1d6.txt b/valid/labels/Screenshot-2022-12-05-223809_jpeg.rf.75c76284bef743a4a6af4b483099b1d6.txt new file mode 100644 index 0000000000000000000000000000000000000000..86150c0e989d69701d0e0e67468734a9bd7d52a1 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-223809_jpeg.rf.75c76284bef743a4a6af4b483099b1d6.txt @@ -0,0 +1,3 @@ +0 0.49765625 0.47734375 0.9953125 0.1046875 +2 0.24609375 0.48671875 0.03359375 0.071875 +2 0.39609375 0.49375 0.07421875 0.05859375 diff --git a/valid/labels/Screenshot-2022-12-05-223853_jpeg.rf.45266c6071617a79519234bc2fe623fe.txt b/valid/labels/Screenshot-2022-12-05-223853_jpeg.rf.45266c6071617a79519234bc2fe623fe.txt new file mode 100644 index 0000000000000000000000000000000000000000..14223dcf13fd1231ebb056f656ffb487fe0be224 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-223853_jpeg.rf.45266c6071617a79519234bc2fe623fe.txt @@ -0,0 +1 @@ +0 0.49765625 0.52265625 0.990625 0.88046875 diff --git a/valid/labels/Screenshot-2022-12-05-223914_jpeg.rf.e035e2c927f94af7de47b7ab08dfcc31.txt b/valid/labels/Screenshot-2022-12-05-223914_jpeg.rf.e035e2c927f94af7de47b7ab08dfcc31.txt new file mode 100644 index 0000000000000000000000000000000000000000..a2c914c7e317afe769515b7842c5c771ef1bd1fc --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-223914_jpeg.rf.e035e2c927f94af7de47b7ab08dfcc31.txt @@ -0,0 +1 @@ +1 0.49609375 0.42578125 0.9703125 0.271875 diff --git a/valid/labels/Screenshot-2022-12-05-224230_jpeg_jpg.rf.ba89bb982523710628a63e72753a082c.txt b/valid/labels/Screenshot-2022-12-05-224230_jpeg_jpg.rf.ba89bb982523710628a63e72753a082c.txt new file mode 100644 index 0000000000000000000000000000000000000000..42673bdb943891ee3455e9ae124e6334c5b322bc --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-224230_jpeg_jpg.rf.ba89bb982523710628a63e72753a082c.txt @@ -0,0 +1,4 @@ +0 0.48359375 0.503125 0.8453125 0.2203125 +2 0.5390625 0.49296875 0.2 0.1171875 +2 0.8609375 0.49296875 0.0453125 0.090625 +2 0.753125 0.42734375 0.04375 0.0421875 diff --git a/valid/labels/Screenshot-2022-12-05-224335_jpeg.rf.c35543fed8b5ced1b9fa9c0820cc3d8e.txt b/valid/labels/Screenshot-2022-12-05-224335_jpeg.rf.c35543fed8b5ced1b9fa9c0820cc3d8e.txt new file mode 100644 index 0000000000000000000000000000000000000000..30b0e4099c833d484d75c4eeb207c1fd55b231b6 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-224335_jpeg.rf.c35543fed8b5ced1b9fa9c0820cc3d8e.txt @@ -0,0 +1,2 @@ +0 0.425 0.3765625 0.4625 0.16328125 +0 0.73828125 0.5375 0.315625 0.50234375 diff --git a/valid/labels/Screenshot-2022-12-05-224452_jpeg_jpg.rf.77fa1b8ce73ab003993911ea2f15dbb4.txt b/valid/labels/Screenshot-2022-12-05-224452_jpeg_jpg.rf.77fa1b8ce73ab003993911ea2f15dbb4.txt new file mode 100644 index 0000000000000000000000000000000000000000..3b27816e2c759a299d172f92fc018b08594cf1a1 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-224452_jpeg_jpg.rf.77fa1b8ce73ab003993911ea2f15dbb4.txt @@ -0,0 +1,2 @@ +0 0.43359375 0.4984375 0.3828125 0.996875 +2 0.4515625 0.55546875 0.0796875 0.084375 diff --git a/valid/labels/Screenshot-2022-12-05-225802_jpeg.rf.28430c83d1d9356b2d4cfe243346c67a.txt b/valid/labels/Screenshot-2022-12-05-225802_jpeg.rf.28430c83d1d9356b2d4cfe243346c67a.txt new file mode 100644 index 0000000000000000000000000000000000000000..28b794d60be70d5fdbe4bf2ad82a2e964e698ec2 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-225802_jpeg.rf.28430c83d1d9356b2d4cfe243346c67a.txt @@ -0,0 +1,2 @@ +0 0.4984375 0.4359375 0.996875 0.603125 +2 0.50234375 0.41875 0.98984375 0.13515625 diff --git a/valid/labels/Screenshot-2022-12-05-230113_jpeg.rf.6bd80d57fa3d24bb034bedede5b3753a.txt b/valid/labels/Screenshot-2022-12-05-230113_jpeg.rf.6bd80d57fa3d24bb034bedede5b3753a.txt new file mode 100644 index 0000000000000000000000000000000000000000..0a91f2e8b08803acea332b2e1c3f3f6e39d0c0c3 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-230113_jpeg.rf.6bd80d57fa3d24bb034bedede5b3753a.txt @@ -0,0 +1 @@ +1 0.49765625 0.6859375 0.9953125 0.4421875 diff --git a/valid/labels/Screenshot-2022-12-05-230206_jpeg.rf.eb59ba5f04140f3ddfadf825c5882698.txt b/valid/labels/Screenshot-2022-12-05-230206_jpeg.rf.eb59ba5f04140f3ddfadf825c5882698.txt new file mode 100644 index 0000000000000000000000000000000000000000..75f1a9fa4a973b51fa264c552f504ebb0581b7a8 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-230206_jpeg.rf.eb59ba5f04140f3ddfadf825c5882698.txt @@ -0,0 +1,5 @@ +2 0.43515625 0.37421875 0.09453125 0.046875 +2 0.6140625 0.3875 0.12109375 0.0828125 +0 0.528125 0.27734375 0.12734375 0.303125 +0 0.81640625 0.56484375 0.1421875 0.19296875 +0 0.2484375 0.56484375 0.0890625 0.20078125 diff --git a/valid/labels/Screenshot-2022-12-05-230425_jpeg.rf.408a6993093d8ddbf3b5c2113d0aca3b.txt b/valid/labels/Screenshot-2022-12-05-230425_jpeg.rf.408a6993093d8ddbf3b5c2113d0aca3b.txt new file mode 100644 index 0000000000000000000000000000000000000000..69bcd8c199c19c615287d23a9be42423b63b5664 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-230425_jpeg.rf.408a6993093d8ddbf3b5c2113d0aca3b.txt @@ -0,0 +1 @@ +0 0.6515625 0.40546875 0.5484375 0.22578125 diff --git a/valid/labels/Screenshot-2022-12-05-231119_jpeg_jpg.rf.74da8da50af4bb513ea70d85a0659462.txt b/valid/labels/Screenshot-2022-12-05-231119_jpeg_jpg.rf.74da8da50af4bb513ea70d85a0659462.txt new file mode 100644 index 0000000000000000000000000000000000000000..13fe39644e6418ef733d7545bc619f0c65dbacf3 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-231119_jpeg_jpg.rf.74da8da50af4bb513ea70d85a0659462.txt @@ -0,0 +1,2 @@ +2 0.53515625 0.46484375 0.13125 0.078125 +0 0.521875 0.50390625 0.7375 0.8125 diff --git a/valid/labels/Screenshot-2022-12-05-231137_jpeg_jpg.rf.42877dab72b743349e3403cfeffff7ca.txt b/valid/labels/Screenshot-2022-12-05-231137_jpeg_jpg.rf.42877dab72b743349e3403cfeffff7ca.txt new file mode 100644 index 0000000000000000000000000000000000000000..6d2f78120ab8fe9752231a999d83e0d766f5a80c --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-231137_jpeg_jpg.rf.42877dab72b743349e3403cfeffff7ca.txt @@ -0,0 +1 @@ +2 0.41015625 0.51171875 0.1859375 0.2875 diff --git a/valid/labels/Screenshot-2022-12-05-231238_jpeg_jpg.rf.d4ca24553c304b31c5493c0a101ae739.txt b/valid/labels/Screenshot-2022-12-05-231238_jpeg_jpg.rf.d4ca24553c304b31c5493c0a101ae739.txt new file mode 100644 index 0000000000000000000000000000000000000000..b0e31ac8f861bc3dcaa631d91057bddf5aa9e525 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-231238_jpeg_jpg.rf.d4ca24553c304b31c5493c0a101ae739.txt @@ -0,0 +1 @@ +0 0.49609375 0.540625 0.9796875 0.19375 diff --git a/valid/labels/Screenshot-2022-12-05-231406_jpeg_jpg.rf.5cff747fa56257165f3fa3ec3c53fc39.txt b/valid/labels/Screenshot-2022-12-05-231406_jpeg_jpg.rf.5cff747fa56257165f3fa3ec3c53fc39.txt new file mode 100644 index 0000000000000000000000000000000000000000..e55f3c964db9ce086a210e6ab6610056b29738a4 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-231406_jpeg_jpg.rf.5cff747fa56257165f3fa3ec3c53fc39.txt @@ -0,0 +1 @@ +0 0.41875 0.278125 0.828125 0.546875 diff --git a/valid/labels/Screenshot-2022-12-05-231929_jpeg.rf.f891e45c3d87c9c6065553364d4be811.txt b/valid/labels/Screenshot-2022-12-05-231929_jpeg.rf.f891e45c3d87c9c6065553364d4be811.txt new file mode 100644 index 0000000000000000000000000000000000000000..6a2b1bf40c0a0132d26db258b8212575019fc660 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-231929_jpeg.rf.f891e45c3d87c9c6065553364d4be811.txt @@ -0,0 +1 @@ +0 0.46015625 0.525 0.1859375 0.43828125 diff --git a/valid/labels/Screenshot-2022-12-05-231929_jpeg_jpg.rf.0f2a7b6941f6c0b4285f0385cd92f9b3.txt b/valid/labels/Screenshot-2022-12-05-231929_jpeg_jpg.rf.0f2a7b6941f6c0b4285f0385cd92f9b3.txt new file mode 100644 index 0000000000000000000000000000000000000000..8067288e07767fa84bb9f386da93fd2e75c56373 --- /dev/null +++ b/valid/labels/Screenshot-2022-12-05-231929_jpeg_jpg.rf.0f2a7b6941f6c0b4285f0385cd92f9b3.txt @@ -0,0 +1 @@ +0 0.46015625 0.525 0.1859375 0.4390625 diff --git a/valid/labels/Slag-inclusion-welding-images_10_jpeg.rf.76e154136e36d7f0ef49da95d4493734.txt b/valid/labels/Slag-inclusion-welding-images_10_jpeg.rf.76e154136e36d7f0ef49da95d4493734.txt new file mode 100644 index 0000000000000000000000000000000000000000..27fe013eccb820c643674fd4c47a6dc497a963bc --- /dev/null +++ b/valid/labels/Slag-inclusion-welding-images_10_jpeg.rf.76e154136e36d7f0ef49da95d4493734.txt @@ -0,0 +1,2 @@ +0 0.43828125 0.62109375 0.73984375 0.19609375 +1 0.43828125 0.3375 0.78515625 0.1796875 diff --git a/valid/labels/Slag-inclusion-welding-images_11_jpeg_jpg.rf.b93cbb4ed4793f16bd717a04201af241.txt b/valid/labels/Slag-inclusion-welding-images_11_jpeg_jpg.rf.b93cbb4ed4793f16bd717a04201af241.txt new file mode 100644 index 0000000000000000000000000000000000000000..2705510e8cadffb277599603f67ac7ec10c3018c --- /dev/null +++ b/valid/labels/Slag-inclusion-welding-images_11_jpeg_jpg.rf.b93cbb4ed4793f16bd717a04201af241.txt @@ -0,0 +1 @@ +0 0.46484375 0.47890625 0.3578125 0.7390625 diff --git a/valid/labels/Slag-inclusion-welding-images_14_jpeg.rf.c7117b8f95af1083b64afd7308ad2d32.txt b/valid/labels/Slag-inclusion-welding-images_14_jpeg.rf.c7117b8f95af1083b64afd7308ad2d32.txt new file mode 100644 index 0000000000000000000000000000000000000000..aa4b77d973d7ce2d04df7892adeb67c1e3ff9c10 --- /dev/null +++ b/valid/labels/Slag-inclusion-welding-images_14_jpeg.rf.c7117b8f95af1083b64afd7308ad2d32.txt @@ -0,0 +1 @@ +2 0.4328125 0.503125 0.08125 0.07265625 diff --git a/valid/labels/Slag-inclusion-welding-images_14_jpeg_jpg.rf.b20e22c3dfe4485186c2c8b4609e1fe4.txt b/valid/labels/Slag-inclusion-welding-images_14_jpeg_jpg.rf.b20e22c3dfe4485186c2c8b4609e1fe4.txt new file mode 100644 index 0000000000000000000000000000000000000000..6afd91fea6c8800a5bf5b6326ff6e794ba547d1f --- /dev/null +++ b/valid/labels/Slag-inclusion-welding-images_14_jpeg_jpg.rf.b20e22c3dfe4485186c2c8b4609e1fe4.txt @@ -0,0 +1 @@ +2 0.4328125 0.503125 0.08125 0.0734375 diff --git a/valid/labels/Spatters-welding-images_16_jpeg_jpg.rf.832f84e5806d9b8841325d7247cecea0.txt b/valid/labels/Spatters-welding-images_16_jpeg_jpg.rf.832f84e5806d9b8841325d7247cecea0.txt new file mode 100644 index 0000000000000000000000000000000000000000..32f4f67159e1310e75ec7d1e2222a2841e4d1dc4 --- /dev/null +++ b/valid/labels/Spatters-welding-images_16_jpeg_jpg.rf.832f84e5806d9b8841325d7247cecea0.txt @@ -0,0 +1,3 @@ +0 0.55546875 0.48125 0.746875 0.33125 +2 0.72890625 0.38515625 0.1421875 0.1453125 +2 0.3796875 0.60390625 0.159375 0.1796875 diff --git a/valid/labels/Spatters-welding-images_22_jpeg.rf.cec9da6e680db1da8e28a3a4baae7fbd.txt b/valid/labels/Spatters-welding-images_22_jpeg.rf.cec9da6e680db1da8e28a3a4baae7fbd.txt new file mode 100644 index 0000000000000000000000000000000000000000..bb7b38a3d39332467dff89259abe61c6401305bb --- /dev/null +++ b/valid/labels/Spatters-welding-images_22_jpeg.rf.cec9da6e680db1da8e28a3a4baae7fbd.txt @@ -0,0 +1,4 @@ +0 0.5015625 0.53046875 0.996875 0.0921875 +2 0.2390625 0.52265625 0.08828125 0.02890625 +2 0.4484375 0.51328125 0.08125 0.0296875 +2 0.32890625 0.5140625 0.0515625 0.0296875 diff --git a/valid/labels/Spatters-welding-images_22_jpeg_jpg.rf.1d748d9acb97b8a67e411d03636e15db.txt b/valid/labels/Spatters-welding-images_22_jpeg_jpg.rf.1d748d9acb97b8a67e411d03636e15db.txt new file mode 100644 index 0000000000000000000000000000000000000000..253119e846352162b09b5093d4994cad9e9e747f --- /dev/null +++ b/valid/labels/Spatters-welding-images_22_jpeg_jpg.rf.1d748d9acb97b8a67e411d03636e15db.txt @@ -0,0 +1,4 @@ +0 0.5015625 0.53046875 0.996875 0.0921875 +2 0.2390625 0.52265625 0.0875 0.028125 +2 0.4484375 0.51328125 0.08125 0.0296875 +2 0.32890625 0.5140625 0.0515625 0.0296875 diff --git a/valid/labels/Spatters-welding-images_29_jpeg.rf.d8f4368809e6e3a0bf14874474eeea2a.txt b/valid/labels/Spatters-welding-images_29_jpeg.rf.d8f4368809e6e3a0bf14874474eeea2a.txt new file mode 100644 index 0000000000000000000000000000000000000000..5632a7b1e10d4cfde45023fa794bb8d289d8c243 --- /dev/null +++ b/valid/labels/Spatters-welding-images_29_jpeg.rf.d8f4368809e6e3a0bf14874474eeea2a.txt @@ -0,0 +1,3 @@ +1 0.66328125 0.41171875 0.23203125 0.1296875 +1 0.3015625 0.50859375 0.34765625 0.1421875 +1 0.91640625 0.26171875 0.15546875 0.1703125 diff --git a/valid/labels/Spatters-welding-images_30_jpeg.rf.df84999e6ccf066d522b816ab10aef0b.txt b/valid/labels/Spatters-welding-images_30_jpeg.rf.df84999e6ccf066d522b816ab10aef0b.txt new file mode 100644 index 0000000000000000000000000000000000000000..b28b8f41100587b6a61cda222a5e687b31ccd8ad --- /dev/null +++ b/valid/labels/Spatters-welding-images_30_jpeg.rf.df84999e6ccf066d522b816ab10aef0b.txt @@ -0,0 +1,4 @@ +0 0.4984375 0.47265625 0.996875 0.28515625 +2 0.6234375 0.8078125 0.1 0.1453125 +2 0.86796875 0.7 0.103125 0.0703125 +2 0.1484375 0.8375 0.096875 0.18515625 diff --git a/valid/labels/b19076f9-53e9d096-c19_jpg.rf.8e97bd5f1a505e175dc6a6918e97434f.txt b/valid/labels/b19076f9-53e9d096-c19_jpg.rf.8e97bd5f1a505e175dc6a6918e97434f.txt new file mode 100644 index 0000000000000000000000000000000000000000..a7f428f0aec703db7974ce7577a6856b15a51dbb --- /dev/null +++ b/valid/labels/b19076f9-53e9d096-c19_jpg.rf.8e97bd5f1a505e175dc6a6918e97434f.txt @@ -0,0 +1 @@ +2 0.475 0.38359375 0.07421875 0.35546875 diff --git a/valid/labels/bad_weld_vid163_jpeg.rf.dcfd957133a5c91b884761901dbf8ef3.txt b/valid/labels/bad_weld_vid163_jpeg.rf.dcfd957133a5c91b884761901dbf8ef3.txt new file mode 100644 index 0000000000000000000000000000000000000000..7a9134ed573882cd8e4c292639b41bd459122396 --- /dev/null +++ b/valid/labels/bad_weld_vid163_jpeg.rf.dcfd957133a5c91b884761901dbf8ef3.txt @@ -0,0 +1 @@ +0 0.453125 0.42578125 0.20234375 0.115625 diff --git a/valid/labels/bad_weld_vid168_jpeg.rf.9b5c3ade6349dbbdba4a7fb658acdae6.txt b/valid/labels/bad_weld_vid168_jpeg.rf.9b5c3ade6349dbbdba4a7fb658acdae6.txt new file mode 100644 index 0000000000000000000000000000000000000000..51a8fc3d3716be40a693d1664899b800d1edfc8e --- /dev/null +++ b/valid/labels/bad_weld_vid168_jpeg.rf.9b5c3ade6349dbbdba4a7fb658acdae6.txt @@ -0,0 +1 @@ +0 0.41875 0.50625 0.30859375 0.165625 diff --git a/valid/labels/bad_weld_vid179_jpeg.rf.1978f09db22800499cbf15b91dc7e97e.txt b/valid/labels/bad_weld_vid179_jpeg.rf.1978f09db22800499cbf15b91dc7e97e.txt new file mode 100644 index 0000000000000000000000000000000000000000..605034eca1e27122ed61c1e46c993c48b6591f29 --- /dev/null +++ b/valid/labels/bad_weld_vid179_jpeg.rf.1978f09db22800499cbf15b91dc7e97e.txt @@ -0,0 +1,3 @@ +0 0.54375 0.4703125 0.19765625 0.190625 +2 0.48515625 0.525 0.0453125 0.0609375 +2 0.540625 0.478125 0.0546875 0.059375 diff --git a/valid/labels/bad_weld_vid179_jpeg_jpg.rf.7916ad0b26b08d11a4aa57a8fd099db6.txt b/valid/labels/bad_weld_vid179_jpeg_jpg.rf.7916ad0b26b08d11a4aa57a8fd099db6.txt new file mode 100644 index 0000000000000000000000000000000000000000..5b4195123de8a0521e9a69706f240e1d39f0850b --- /dev/null +++ b/valid/labels/bad_weld_vid179_jpeg_jpg.rf.7916ad0b26b08d11a4aa57a8fd099db6.txt @@ -0,0 +1,3 @@ +0 0.54375 0.4703125 0.1984375 0.190625 +2 0.48515625 0.525 0.0453125 0.0609375 +2 0.540625 0.478125 0.0546875 0.059375 diff --git a/valid/labels/bad_weld_vid180_jpeg.rf.c763ff5834a82c22cbf06e97ac57e770.txt b/valid/labels/bad_weld_vid180_jpeg.rf.c763ff5834a82c22cbf06e97ac57e770.txt new file mode 100644 index 0000000000000000000000000000000000000000..9ef03b76a4d2bb1d91b0be208813bbe801be9671 --- /dev/null +++ b/valid/labels/bad_weld_vid180_jpeg.rf.c763ff5834a82c22cbf06e97ac57e770.txt @@ -0,0 +1,3 @@ +0 0.5453125 0.478125 0.1953125 0.1859375 +2 0.4859375 0.528125 0.04921875 0.05390625 +2 0.540625 0.478125 0.05078125 0.0515625 diff --git a/valid/labels/bad_weld_vid181_jpeg_jpg.rf.7d9912c2d73df82417963a765beb335e.txt b/valid/labels/bad_weld_vid181_jpeg_jpg.rf.7d9912c2d73df82417963a765beb335e.txt new file mode 100644 index 0000000000000000000000000000000000000000..c3076b9ea4d377106f4baa5dab538aceabd468cd --- /dev/null +++ b/valid/labels/bad_weld_vid181_jpeg_jpg.rf.7d9912c2d73df82417963a765beb335e.txt @@ -0,0 +1,3 @@ +0 0.5484375 0.47890625 0.190625 0.175 +2 0.4859375 0.52890625 0.0484375 0.05625 +2 0.540625 0.48046875 0.0515625 0.053125 diff --git a/valid/labels/bad_weld_vid183_jpeg.rf.722e481e277f2197c2be4a7e8812c075.txt b/valid/labels/bad_weld_vid183_jpeg.rf.722e481e277f2197c2be4a7e8812c075.txt new file mode 100644 index 0000000000000000000000000000000000000000..7d88a803068b2f52d56a15df8fce07667def82c6 --- /dev/null +++ b/valid/labels/bad_weld_vid183_jpeg.rf.722e481e277f2197c2be4a7e8812c075.txt @@ -0,0 +1,3 @@ +0 0.54921875 0.484375 0.196875 0.1734375 +2 0.48515625 0.528125 0.0453125 0.053125 +2 0.540625 0.4796875 0.0546875 0.05390625 diff --git a/valid/labels/bad_weld_vid204_jpeg_jpg.rf.45accbfbc23769c5d81d8c0dad9afc0b.txt b/valid/labels/bad_weld_vid204_jpeg_jpg.rf.45accbfbc23769c5d81d8c0dad9afc0b.txt new file mode 100644 index 0000000000000000000000000000000000000000..6a835ba882bb05f2938a6e06f7a8c1eae86b009a --- /dev/null +++ b/valid/labels/bad_weld_vid204_jpeg_jpg.rf.45accbfbc23769c5d81d8c0dad9afc0b.txt @@ -0,0 +1 @@ +0 0.5015625 0.53046875 0.1890625 0.09375 diff --git a/valid/labels/bad_weld_vid260_jpeg.rf.4780b7d712ce3cefbc37e339f91bc46c.txt b/valid/labels/bad_weld_vid260_jpeg.rf.4780b7d712ce3cefbc37e339f91bc46c.txt new file mode 100644 index 0000000000000000000000000000000000000000..2e391ea6d68a572b9b9b30b544025d69061930f8 --- /dev/null +++ b/valid/labels/bad_weld_vid260_jpeg.rf.4780b7d712ce3cefbc37e339f91bc46c.txt @@ -0,0 +1,5 @@ +0 0.5046875 0.421875 0.12734375 0.09609375 +1 0.7015625 0.48984375 0.1515625 0.109375 +1 0.328125 0.36953125 0.11328125 0.08046875 +2 0.4921875 0.4296875 0.01171875 0.02109375 +2 0.5421875 0.44140625 0.03359375 0.025 diff --git a/valid/labels/bad_weld_vid276_jpeg.rf.7fdc86ef117bb3a29b68236ac9d9db62.txt b/valid/labels/bad_weld_vid276_jpeg.rf.7fdc86ef117bb3a29b68236ac9d9db62.txt new file mode 100644 index 0000000000000000000000000000000000000000..efbf59f46b3bb0ae8d613c6f4edaf6e33a2902b4 --- /dev/null +++ b/valid/labels/bad_weld_vid276_jpeg.rf.7fdc86ef117bb3a29b68236ac9d9db62.txt @@ -0,0 +1,3 @@ +0 0.49375 0.5828125 0.20390625 0.1515625 +2 0.425 0.62109375 0.0421875 0.046875 +2 0.4796875 0.584375 0.05078125 0.05 diff --git a/valid/labels/bad_weld_vid321_jpeg.rf.52beace05100b829ead3a5c3616d9205.txt b/valid/labels/bad_weld_vid321_jpeg.rf.52beace05100b829ead3a5c3616d9205.txt new file mode 100644 index 0000000000000000000000000000000000000000..fae37e3dae75f32feb80f9278c4043852a3a0d14 --- /dev/null +++ b/valid/labels/bad_weld_vid321_jpeg.rf.52beace05100b829ead3a5c3616d9205.txt @@ -0,0 +1 @@ +0 0.675 0.43046875 0.41328125 0.2609375 diff --git a/valid/labels/bad_weld_vid322_jpeg.rf.6aba6132033c0afe50c966a35920a198.txt b/valid/labels/bad_weld_vid322_jpeg.rf.6aba6132033c0afe50c966a35920a198.txt new file mode 100644 index 0000000000000000000000000000000000000000..f2809fe02b4b010f0e7c77ef80af49ca1ae0de37 --- /dev/null +++ b/valid/labels/bad_weld_vid322_jpeg.rf.6aba6132033c0afe50c966a35920a198.txt @@ -0,0 +1 @@ +0 0.684375 0.5421875 0.42734375 0.24609375 diff --git a/valid/labels/bad_weld_vid368_jpeg_jpg.rf.cc8c996094237a36bcee56ba35fb5cd6.txt b/valid/labels/bad_weld_vid368_jpeg_jpg.rf.cc8c996094237a36bcee56ba35fb5cd6.txt new file mode 100644 index 0000000000000000000000000000000000000000..afa060f94c1777cdb5062ef640235018e7ad2dc1 --- /dev/null +++ b/valid/labels/bad_weld_vid368_jpeg_jpg.rf.cc8c996094237a36bcee56ba35fb5cd6.txt @@ -0,0 +1,3 @@ +0 0.5546875 0.30078125 0.5625 0.565625 +2 0.48515625 0.24609375 0.028125 0.1203125 +2 0.590625 0.31875 0.0375 0.065625 diff --git a/valid/labels/bad_weld_vid373_jpeg_jpg.rf.36f2ede2ba2bd27f37b766a0c98c8d9b.txt b/valid/labels/bad_weld_vid373_jpeg_jpg.rf.36f2ede2ba2bd27f37b766a0c98c8d9b.txt new file mode 100644 index 0000000000000000000000000000000000000000..756347b52c4d0b453a42e4f9073646e41276f3bd --- /dev/null +++ b/valid/labels/bad_weld_vid373_jpeg_jpg.rf.36f2ede2ba2bd27f37b766a0c98c8d9b.txt @@ -0,0 +1,2 @@ +0 0.4234375 0.440625 0.846875 0.2375 +2 0.421875 0.44921875 0.8359375 0.11875 diff --git a/valid/labels/bad_weld_vid395_jpeg_jpg.rf.29860add816c33eef305b2fc0b70611c.txt b/valid/labels/bad_weld_vid395_jpeg_jpg.rf.29860add816c33eef305b2fc0b70611c.txt new file mode 100644 index 0000000000000000000000000000000000000000..e906a4f7b2e7dc06cfe8f41fc280bda34c51a591 --- /dev/null +++ b/valid/labels/bad_weld_vid395_jpeg_jpg.rf.29860add816c33eef305b2fc0b70611c.txt @@ -0,0 +1,2 @@ +1 0.17578125 0.2921875 0.3515625 0.184375 +0 0.65 0.33125 0.409375 0.2328125 diff --git a/valid/labels/bad_weld_vid400_jpeg.rf.839271725e205b8bfb2730ad7ea3cc53.txt b/valid/labels/bad_weld_vid400_jpeg.rf.839271725e205b8bfb2730ad7ea3cc53.txt new file mode 100644 index 0000000000000000000000000000000000000000..14fd3939ff40768348b96b4c43efc11d1aa71c97 --- /dev/null +++ b/valid/labels/bad_weld_vid400_jpeg.rf.839271725e205b8bfb2730ad7ea3cc53.txt @@ -0,0 +1,2 @@ +1 0.3265625 0.3484375 0.60078125 0.4109375 +0 0.83671875 0.11640625 0.3203125 0.2328125 diff --git a/valid/labels/bad_weld_vid401_jpeg.rf.c8a5993aee6de81c1d3a0ddf5bf5997f.txt b/valid/labels/bad_weld_vid401_jpeg.rf.c8a5993aee6de81c1d3a0ddf5bf5997f.txt new file mode 100644 index 0000000000000000000000000000000000000000..a2065a33ac418cda71985ebe819ef708b271762b --- /dev/null +++ b/valid/labels/bad_weld_vid401_jpeg.rf.c8a5993aee6de81c1d3a0ddf5bf5997f.txt @@ -0,0 +1,2 @@ +1 0.26953125 0.3921875 0.5390625 0.384375 +0 0.7546875 0.13828125 0.32890625 0.2765625 diff --git a/valid/labels/bad_weld_vid402_jpeg_jpg.rf.390693d9ec1ae40b4b54462dba48ac9f.txt b/valid/labels/bad_weld_vid402_jpeg_jpg.rf.390693d9ec1ae40b4b54462dba48ac9f.txt new file mode 100644 index 0000000000000000000000000000000000000000..64b9ae7cf0bf54699e7d22a41a817c945806e749 --- /dev/null +++ b/valid/labels/bad_weld_vid402_jpeg_jpg.rf.390693d9ec1ae40b4b54462dba48ac9f.txt @@ -0,0 +1,2 @@ +1 0.271875 0.428125 0.5328125 0.3890625 +0 0.7484375 0.1734375 0.315625 0.2703125 diff --git a/valid/labels/bad_weld_vid452_jpeg.rf.c6473066b2f3e14ade45c1e78d1d70a1.txt b/valid/labels/bad_weld_vid452_jpeg.rf.c6473066b2f3e14ade45c1e78d1d70a1.txt new file mode 100644 index 0000000000000000000000000000000000000000..5a1e9e80c30da0a5b8f55166a54cafccd734cc0a --- /dev/null +++ b/valid/labels/bad_weld_vid452_jpeg.rf.c6473066b2f3e14ade45c1e78d1d70a1.txt @@ -0,0 +1,3 @@ +0 0.5625 0.434375 0.32734375 0.26796875 +2 0.6296875 0.409375 0.15390625 0.14453125 +2 0.46875 0.5078125 0.07109375 0.0734375 diff --git a/valid/labels/bad_weld_vid452_jpeg_jpg.rf.3dd44c46e92a2845c806d788734bc8e7.txt b/valid/labels/bad_weld_vid452_jpeg_jpg.rf.3dd44c46e92a2845c806d788734bc8e7.txt new file mode 100644 index 0000000000000000000000000000000000000000..4f3b4ac74242b9c0c84211ee771549a0de08c933 --- /dev/null +++ b/valid/labels/bad_weld_vid452_jpeg_jpg.rf.3dd44c46e92a2845c806d788734bc8e7.txt @@ -0,0 +1,3 @@ +0 0.5625 0.434375 0.328125 0.26875 +2 0.6296875 0.409375 0.153125 0.1453125 +2 0.46875 0.5078125 0.071875 0.0734375 diff --git a/valid/labels/bad_weld_vid456_jpeg.rf.bc9a0a55effbb910be74ea1588bc5ace.txt b/valid/labels/bad_weld_vid456_jpeg.rf.bc9a0a55effbb910be74ea1588bc5ace.txt new file mode 100644 index 0000000000000000000000000000000000000000..5bc2243446ca5073ae7ee2d9f8b6d1d5958b6182 --- /dev/null +++ b/valid/labels/bad_weld_vid456_jpeg.rf.bc9a0a55effbb910be74ea1588bc5ace.txt @@ -0,0 +1,3 @@ +2 0.4859375 0.54375 0.26640625 0.134375 +0 0.4265625 0.5515625 0.53046875 0.25 +2 0.24609375 0.6171875 0.0765625 0.07890625 diff --git a/valid/labels/bad_weld_vid456_jpeg_jpg.rf.c01c23b35e46d61220077f0ea2d43ca2.txt b/valid/labels/bad_weld_vid456_jpeg_jpg.rf.c01c23b35e46d61220077f0ea2d43ca2.txt new file mode 100644 index 0000000000000000000000000000000000000000..4ce5053a7950ec330fef94d3ec3a14363b03fb53 --- /dev/null +++ b/valid/labels/bad_weld_vid456_jpeg_jpg.rf.c01c23b35e46d61220077f0ea2d43ca2.txt @@ -0,0 +1,3 @@ +2 0.4859375 0.54375 0.265625 0.134375 +0 0.4265625 0.5515625 0.53125 0.25 +2 0.24609375 0.6171875 0.0765625 0.0796875 diff --git a/valid/labels/bad_weld_vid458_jpeg.rf.fae9a6806b1ce765c984acd78987c515.txt b/valid/labels/bad_weld_vid458_jpeg.rf.fae9a6806b1ce765c984acd78987c515.txt new file mode 100644 index 0000000000000000000000000000000000000000..5dc2025beaf7588c76fe0673b009b6f781daef6e --- /dev/null +++ b/valid/labels/bad_weld_vid458_jpeg.rf.fae9a6806b1ce765c984acd78987c515.txt @@ -0,0 +1,2 @@ +0 0.2625 0.64453125 0.5203125 0.28046875 +2 0.228125 0.6515625 0.27734375 0.14453125 diff --git a/valid/labels/bad_weld_vid472_jpeg.rf.4d043cf88ee27b16d389630261fab392.txt b/valid/labels/bad_weld_vid472_jpeg.rf.4d043cf88ee27b16d389630261fab392.txt new file mode 100644 index 0000000000000000000000000000000000000000..729b0c0fe567f3894f490b041559a9a77fa4f530 --- /dev/null +++ b/valid/labels/bad_weld_vid472_jpeg.rf.4d043cf88ee27b16d389630261fab392.txt @@ -0,0 +1,3 @@ +0 0.44765625 0.51875 0.79609375 0.19453125 +2 0.37421875 0.559375 0.190625 0.05234375 +2 0.6453125 0.5125 0.1984375 0.0546875 diff --git a/valid/labels/bad_weld_vid472_jpeg_jpg.rf.133f525e40ef7437455bdae357bdb118.txt b/valid/labels/bad_weld_vid472_jpeg_jpg.rf.133f525e40ef7437455bdae357bdb118.txt new file mode 100644 index 0000000000000000000000000000000000000000..2119b8617141734367234309a1ba71d7d78a9d13 --- /dev/null +++ b/valid/labels/bad_weld_vid472_jpeg_jpg.rf.133f525e40ef7437455bdae357bdb118.txt @@ -0,0 +1,3 @@ +0 0.44765625 0.51875 0.796875 0.1953125 +2 0.37421875 0.559375 0.190625 0.0515625 +2 0.6453125 0.5125 0.1984375 0.0546875 diff --git a/valid/labels/bad_weld_vid474_jpeg.rf.12551d2733eff800defad2110bebacb8.txt b/valid/labels/bad_weld_vid474_jpeg.rf.12551d2733eff800defad2110bebacb8.txt new file mode 100644 index 0000000000000000000000000000000000000000..ff8e0653d7be4670576daf7f48be105764b5c1c7 --- /dev/null +++ b/valid/labels/bad_weld_vid474_jpeg.rf.12551d2733eff800defad2110bebacb8.txt @@ -0,0 +1,2 @@ +0 0.40703125 0.53203125 0.79453125 0.153125 +2 0.303125 0.5640625 0.190625 0.06484375 diff --git a/valid/labels/bad_weld_vid560_jpeg.rf.453f097391a39c10263feb0d80a4408c.txt b/valid/labels/bad_weld_vid560_jpeg.rf.453f097391a39c10263feb0d80a4408c.txt new file mode 100644 index 0000000000000000000000000000000000000000..1b77da50d86a288fb6e012ef76250665a8cc1814 --- /dev/null +++ b/valid/labels/bad_weld_vid560_jpeg.rf.453f097391a39c10263feb0d80a4408c.txt @@ -0,0 +1,2 @@ +0 0.45 0.69140625 0.22734375 0.6140625 +2 0.45703125 0.64609375 0.115625 0.3390625 diff --git a/valid/labels/bad_weld_vid566_jpeg.rf.d42464cd3debe3e894ca0d6ab1884276.txt b/valid/labels/bad_weld_vid566_jpeg.rf.d42464cd3debe3e894ca0d6ab1884276.txt new file mode 100644 index 0000000000000000000000000000000000000000..e843ad094e54b8265df073db8d73ddf466fdf421 --- /dev/null +++ b/valid/labels/bad_weld_vid566_jpeg.rf.d42464cd3debe3e894ca0d6ab1884276.txt @@ -0,0 +1,2 @@ +2 0.4953125 0.43828125 0.0328125 0.22890625 +0 0.49765625 0.4703125 0.05625 0.48203125 diff --git a/valid/labels/bad_weld_vid577_jpeg.rf.00fd7013a93c1b335a6b59a7f57318b2.txt b/valid/labels/bad_weld_vid577_jpeg.rf.00fd7013a93c1b335a6b59a7f57318b2.txt new file mode 100644 index 0000000000000000000000000000000000000000..79689eb1269801077300fc8315e1c28aae3b1fc7 --- /dev/null +++ b/valid/labels/bad_weld_vid577_jpeg.rf.00fd7013a93c1b335a6b59a7f57318b2.txt @@ -0,0 +1,2 @@ +0 0.4734375 0.51875 0.40546875 0.2515625 +2 0.47109375 0.53359375 0.1984375 0.121875 diff --git a/valid/labels/bad_weld_vid642_jpeg.rf.04ffd220cb1e589842d8b8a92dbe8ae7.txt b/valid/labels/bad_weld_vid642_jpeg.rf.04ffd220cb1e589842d8b8a92dbe8ae7.txt new file mode 100644 index 0000000000000000000000000000000000000000..29ec0beb48ab641457eac248730e5a03b93fe729 --- /dev/null +++ b/valid/labels/bad_weld_vid642_jpeg.rf.04ffd220cb1e589842d8b8a92dbe8ae7.txt @@ -0,0 +1 @@ +0 0.50625 0.43125 0.140625 0.859375 diff --git a/valid/labels/bad_weld_vid644_jpeg_jpg.rf.e6550f4e18eb3c630d35f229de5cf860.txt b/valid/labels/bad_weld_vid644_jpeg_jpg.rf.e6550f4e18eb3c630d35f229de5cf860.txt new file mode 100644 index 0000000000000000000000000000000000000000..cbe3e61221319137a2ee01443841ce2a768b9c46 --- /dev/null +++ b/valid/labels/bad_weld_vid644_jpeg_jpg.rf.e6550f4e18eb3c630d35f229de5cf860.txt @@ -0,0 +1 @@ +0 0.60390625 0.50078125 0.1546875 0.996875 diff --git a/valid/labels/bad_weld_vid688_jpeg.rf.5011fcf9b99f5670549e04ad7b882cf6.txt b/valid/labels/bad_weld_vid688_jpeg.rf.5011fcf9b99f5670549e04ad7b882cf6.txt new file mode 100644 index 0000000000000000000000000000000000000000..0d3376eb18051246d38ea6409b84fed5939d9d21 --- /dev/null +++ b/valid/labels/bad_weld_vid688_jpeg.rf.5011fcf9b99f5670549e04ad7b882cf6.txt @@ -0,0 +1,3 @@ +0 0.56875 0.490625 0.2078125 0.975 +2 0.553125 0.615625 0.1171875 0.6625 +0 0.6671875 0.409375 0.06640625 0.721875 diff --git a/valid/labels/bad_weld_vid689_jpeg.rf.f7dd125d58e36523c6c66360152f4b6a.txt b/valid/labels/bad_weld_vid689_jpeg.rf.f7dd125d58e36523c6c66360152f4b6a.txt new file mode 100644 index 0000000000000000000000000000000000000000..ab7ca38c398a80b5184cb914d545945fbcb8428e --- /dev/null +++ b/valid/labels/bad_weld_vid689_jpeg.rf.f7dd125d58e36523c6c66360152f4b6a.txt @@ -0,0 +1,3 @@ +0 0.58125 0.42578125 0.1859375 0.8515625 +2 0.5546875 0.44375 0.103125 0.70703125 +0 0.6890625 0.3515625 0.0859375 0.69140625 diff --git a/valid/labels/bad_weld_vid691_jpeg_jpg.rf.3a0a4e31cdde119a47964ebfa459f67b.txt b/valid/labels/bad_weld_vid691_jpeg_jpg.rf.3a0a4e31cdde119a47964ebfa459f67b.txt new file mode 100644 index 0000000000000000000000000000000000000000..4fd6e139bdcfd5b16ede2e9ae60fdd5b769b68d9 --- /dev/null +++ b/valid/labels/bad_weld_vid691_jpeg_jpg.rf.3a0a4e31cdde119a47964ebfa459f67b.txt @@ -0,0 +1,3 @@ +0 0.303125 0.465625 0.171875 0.93125 +2 0.346875 0.51328125 0.0921875 0.6828125 +0 0.5015625 0.4140625 0.153125 0.828125 diff --git a/valid/labels/bad_weld_vid723_jpeg.rf.ecb73ed4cae5241972d088a16840fe53.txt b/valid/labels/bad_weld_vid723_jpeg.rf.ecb73ed4cae5241972d088a16840fe53.txt new file mode 100644 index 0000000000000000000000000000000000000000..c13c7a09ebd0274a24ed69b42bf1f33b421b6927 --- /dev/null +++ b/valid/labels/bad_weld_vid723_jpeg.rf.ecb73ed4cae5241972d088a16840fe53.txt @@ -0,0 +1,3 @@ +0 0.5453125 0.34921875 0.07109375 0.6484375 +1 0.6703125 0.48515625 0.08828125 0.67109375 +0 0.809375 0.59453125 0.14921875 0.6109375 diff --git a/valid/labels/bad_weld_vid723_jpeg_jpg.rf.479c95090238a00b38312a17e6c37767.txt b/valid/labels/bad_weld_vid723_jpeg_jpg.rf.479c95090238a00b38312a17e6c37767.txt new file mode 100644 index 0000000000000000000000000000000000000000..55e7bc5642d9c5e8b0c30358dae8106b6b54eb7e --- /dev/null +++ b/valid/labels/bad_weld_vid723_jpeg_jpg.rf.479c95090238a00b38312a17e6c37767.txt @@ -0,0 +1,3 @@ +0 0.5453125 0.34921875 0.071875 0.6484375 +1 0.6703125 0.48515625 0.0890625 0.671875 +0 0.809375 0.59453125 0.15 0.6109375 diff --git a/valid/labels/bad_weld_vid85_jpeg_jpg.rf.4ec131c145176b8e4fee392e414937c3.txt b/valid/labels/bad_weld_vid85_jpeg_jpg.rf.4ec131c145176b8e4fee392e414937c3.txt new file mode 100644 index 0000000000000000000000000000000000000000..726ad0ed0f902889e988330a1df8fa6d24e1b513 --- /dev/null +++ b/valid/labels/bad_weld_vid85_jpeg_jpg.rf.4ec131c145176b8e4fee392e414937c3.txt @@ -0,0 +1 @@ +1 0.45 0.46640625 0.5484375 0.184375 diff --git a/valid/labels/bad_weld_vid89_jpeg.rf.76e231e95f0fb6af62300f478e3c0784.txt b/valid/labels/bad_weld_vid89_jpeg.rf.76e231e95f0fb6af62300f478e3c0784.txt new file mode 100644 index 0000000000000000000000000000000000000000..74b406d825dffd98e72c467ba4b4fd1bff98bf98 --- /dev/null +++ b/valid/labels/bad_weld_vid89_jpeg.rf.76e231e95f0fb6af62300f478e3c0784.txt @@ -0,0 +1 @@ +0 0.31171875 0.3640625 0.3515625 0.2390625 diff --git a/valid/labels/bad_weld_vid97_jpeg.rf.0b98c1d6ca7194b1c2cc46fd695d5491.txt b/valid/labels/bad_weld_vid97_jpeg.rf.0b98c1d6ca7194b1c2cc46fd695d5491.txt new file mode 100644 index 0000000000000000000000000000000000000000..f0e91d358dfe044ecc4ca74e1aeac11d252f84c5 --- /dev/null +++ b/valid/labels/bad_weld_vid97_jpeg.rf.0b98c1d6ca7194b1c2cc46fd695d5491.txt @@ -0,0 +1 @@ +2 0.51328125 0.36015625 0.5640625 0.1625 diff --git a/valid/labels/badly-welded-corner-rusty-old-metal-bad-weld-how-not-to-cook-132406262_jpeg.rf.afb82e608ea5d4bc90d9eabd2970a257.txt b/valid/labels/badly-welded-corner-rusty-old-metal-bad-weld-how-not-to-cook-132406262_jpeg.rf.afb82e608ea5d4bc90d9eabd2970a257.txt new file mode 100644 index 0000000000000000000000000000000000000000..cac95bdbde01879456fb7a26bb59fea261e6cadf --- /dev/null +++ b/valid/labels/badly-welded-corner-rusty-old-metal-bad-weld-how-not-to-cook-132406262_jpeg.rf.afb82e608ea5d4bc90d9eabd2970a257.txt @@ -0,0 +1,3 @@ +0 0.56015625 0.51796875 0.8578125 0.69765625 +2 0.3078125 0.69140625 0.0484375 0.06953125 +2 0.6015625 0.45234375 0.0328125 0.0375 diff --git a/valid/labels/badly-welded-corner-rusty-old-metal-bad-weld-how-not-to-cook-132406262_jpeg_jpg.rf.f9547b57e86a53683e7c2b1f9bd68759.txt b/valid/labels/badly-welded-corner-rusty-old-metal-bad-weld-how-not-to-cook-132406262_jpeg_jpg.rf.f9547b57e86a53683e7c2b1f9bd68759.txt new file mode 100644 index 0000000000000000000000000000000000000000..791469000afaffa3e0e81c52b4e25d3aa81047cf --- /dev/null +++ b/valid/labels/badly-welded-corner-rusty-old-metal-bad-weld-how-not-to-cook-132406262_jpeg_jpg.rf.f9547b57e86a53683e7c2b1f9bd68759.txt @@ -0,0 +1,3 @@ +0 0.56015625 0.51796875 0.8578125 0.6984375 +2 0.3078125 0.69140625 0.0484375 0.0703125 +2 0.6015625 0.45234375 0.0328125 0.0375 diff --git a/valid/labels/be37a81e-f0f3ef45-2008-01_2_jpg.rf.039b32374e750695157e0b494ab8de48.txt b/valid/labels/be37a81e-f0f3ef45-2008-01_2_jpg.rf.039b32374e750695157e0b494ab8de48.txt new file mode 100644 index 0000000000000000000000000000000000000000..fb7b28f0697031f4f747995f7c23e98669483167 --- /dev/null +++ b/valid/labels/be37a81e-f0f3ef45-2008-01_2_jpg.rf.039b32374e750695157e0b494ab8de48.txt @@ -0,0 +1 @@ +2 0.53828125 0.4546875 0.89453125 0.17578125 diff --git a/valid/labels/bhjv_jpeg.rf.946206be8cbc2cda721645b8e87a5ae7.txt b/valid/labels/bhjv_jpeg.rf.946206be8cbc2cda721645b8e87a5ae7.txt new file mode 100644 index 0000000000000000000000000000000000000000..71b6287eefc95d630ad5a21764b59d87a77347c7 --- /dev/null +++ b/valid/labels/bhjv_jpeg.rf.946206be8cbc2cda721645b8e87a5ae7.txt @@ -0,0 +1,3 @@ +2 0.359375 0.4484375 0.07578125 0.096875 +2 0.7984375 0.4609375 0.0953125 0.12109375 +2 0.596875 0.37578125 0.05234375 0.0609375 diff --git a/valid/labels/carbon-steel-good-welds_10_jpeg_jpg.rf.5f643e2f016682f4974fd298d70aa0e6.txt b/valid/labels/carbon-steel-good-welds_10_jpeg_jpg.rf.5f643e2f016682f4974fd298d70aa0e6.txt new file mode 100644 index 0000000000000000000000000000000000000000..1fd5e4a8b93b5d23db5664e6ea9c2c55cb5a0a2f --- /dev/null +++ b/valid/labels/carbon-steel-good-welds_10_jpeg_jpg.rf.5f643e2f016682f4974fd298d70aa0e6.txt @@ -0,0 +1 @@ +1 0.4859375 0.66015625 0.7265625 0.234375 diff --git a/valid/labels/carbon-steel-good-welds_11_jpeg_jpg.rf.2a7673deb7baff5fe012929f5a2229d8.txt b/valid/labels/carbon-steel-good-welds_11_jpeg_jpg.rf.2a7673deb7baff5fe012929f5a2229d8.txt new file mode 100644 index 0000000000000000000000000000000000000000..197569a6dc6fc7b0af0db84675332c1e032959ed --- /dev/null +++ b/valid/labels/carbon-steel-good-welds_11_jpeg_jpg.rf.2a7673deb7baff5fe012929f5a2229d8.txt @@ -0,0 +1 @@ +1 0.578125 0.5703125 0.0703125 0.5796875 diff --git a/valid/labels/carbon-steel-good-welds_48_jpeg.rf.b963e5cf9d95d70385f0d77c5757cbfa.txt b/valid/labels/carbon-steel-good-welds_48_jpeg.rf.b963e5cf9d95d70385f0d77c5757cbfa.txt new file mode 100644 index 0000000000000000000000000000000000000000..e699a9a3bdeaea4a772923e7195fe2590035bb17 --- /dev/null +++ b/valid/labels/carbon-steel-good-welds_48_jpeg.rf.b963e5cf9d95d70385f0d77c5757cbfa.txt @@ -0,0 +1 @@ +1 0.55703125 0.53828125 0.884375 0.3125 diff --git a/valid/labels/crack-welding-images_11_jpeg.rf.4564ca826447b26204e4a227966f89b5.txt b/valid/labels/crack-welding-images_11_jpeg.rf.4564ca826447b26204e4a227966f89b5.txt new file mode 100644 index 0000000000000000000000000000000000000000..a6640b7612b5c259bb4d201122ac4766648d23e8 --- /dev/null +++ b/valid/labels/crack-welding-images_11_jpeg.rf.4564ca826447b26204e4a227966f89b5.txt @@ -0,0 +1 @@ +2 0.45 0.55703125 0.89921875 0.10078125 diff --git a/valid/labels/crack-welding-images_12_jpeg.rf.5e6844a1b19b96db44dcc0d423b6d41f.txt b/valid/labels/crack-welding-images_12_jpeg.rf.5e6844a1b19b96db44dcc0d423b6d41f.txt new file mode 100644 index 0000000000000000000000000000000000000000..bb4c8c4899148ffa2193e5299ccdae63a8bf993a --- /dev/null +++ b/valid/labels/crack-welding-images_12_jpeg.rf.5e6844a1b19b96db44dcc0d423b6d41f.txt @@ -0,0 +1,3 @@ +1 0.475 0.225 0.928125 0.2765625 +2 0.48203125 0.7328125 0.95859375 0.0640625 +0 0.49296875 0.76484375 0.9859375 0.35625 diff --git a/valid/labels/crack-welding-images_12_jpeg_jpg.rf.1af4ac8caf4e2ed4ffad3c0bbf70e0c4.txt b/valid/labels/crack-welding-images_12_jpeg_jpg.rf.1af4ac8caf4e2ed4ffad3c0bbf70e0c4.txt new file mode 100644 index 0000000000000000000000000000000000000000..7772a04a6d02073044bb8966bbd89cd08fe75bc1 --- /dev/null +++ b/valid/labels/crack-welding-images_12_jpeg_jpg.rf.1af4ac8caf4e2ed4ffad3c0bbf70e0c4.txt @@ -0,0 +1,3 @@ +1 0.475 0.225 0.928125 0.2765625 +2 0.48203125 0.7328125 0.959375 0.0640625 +0 0.49296875 0.76484375 0.9859375 0.35625 diff --git a/valid/labels/crack-welding-images_21_jpeg_jpg.rf.a8fe58377f24d954a14e75c731321a8b.txt b/valid/labels/crack-welding-images_21_jpeg_jpg.rf.a8fe58377f24d954a14e75c731321a8b.txt new file mode 100644 index 0000000000000000000000000000000000000000..4b5f38e696cd8c85d0176e0e3c5a2dd06e1062c8 --- /dev/null +++ b/valid/labels/crack-welding-images_21_jpeg_jpg.rf.a8fe58377f24d954a14e75c731321a8b.txt @@ -0,0 +1 @@ +2 0.61796875 0.46484375 0.1390625 0.8890625 diff --git a/valid/labels/d18b341f-e637a315-c21_jpg.rf.12173f7ad5047c3c89e3bee036329565.txt b/valid/labels/d18b341f-e637a315-c21_jpg.rf.12173f7ad5047c3c89e3bee036329565.txt new file mode 100644 index 0000000000000000000000000000000000000000..ddd53b44ce6dae0bc6cc34fd158a9ac57b74d886 --- /dev/null +++ b/valid/labels/d18b341f-e637a315-c21_jpg.rf.12173f7ad5047c3c89e3bee036329565.txt @@ -0,0 +1 @@ +2 0.478125 0.51796875 0.771875 0.2015625 diff --git a/valid/labels/good-stick-welds_19_png.rf.2d3c403b66b7544b943c7549efe5f1bf.txt b/valid/labels/good-stick-welds_19_png.rf.2d3c403b66b7544b943c7549efe5f1bf.txt new file mode 100644 index 0000000000000000000000000000000000000000..913f3b3033a366e14e596b66fc70d78264424050 --- /dev/null +++ b/valid/labels/good-stick-welds_19_png.rf.2d3c403b66b7544b943c7549efe5f1bf.txt @@ -0,0 +1,7 @@ +1 0.49453125 0.12265625 0.9859375 0.0578125 +0 0.49921875 0.25859375 0.99609375 0.04140625 +0 0.5015625 0.38671875 0.99140625 0.05546875 +0 0.5 0.53203125 0.996875 0.05625 +0 0.4984375 0.6828125 0.996875 0.0921875 +0 0.503125 0.81328125 0.99140625 0.07109375 +0 0.496875 0.96640625 0.990625 0.0515625 diff --git a/valid/labels/good-stick-welds_30_jpeg_jpg.rf.c507d686552cb971896c907c9baea8c2.txt b/valid/labels/good-stick-welds_30_jpeg_jpg.rf.c507d686552cb971896c907c9baea8c2.txt new file mode 100644 index 0000000000000000000000000000000000000000..4fc77326373925c0750e5e2cd8bec248e5dc4a6b --- /dev/null +++ b/valid/labels/good-stick-welds_30_jpeg_jpg.rf.c507d686552cb971896c907c9baea8c2.txt @@ -0,0 +1,3 @@ +1 0.17265625 0.38828125 0.240625 0.18125 +1 0.47890625 0.53828125 0.328125 0.2234375 +1 0.81796875 0.69453125 0.30625 0.2296875 diff --git a/valid/labels/good-stick-welds_34_jpeg_jpg.rf.4dda4c452265275489fb48216b070472.txt b/valid/labels/good-stick-welds_34_jpeg_jpg.rf.4dda4c452265275489fb48216b070472.txt new file mode 100644 index 0000000000000000000000000000000000000000..6debc3463295bccbfc9fdbf1700ae20d3ecada8f --- /dev/null +++ b/valid/labels/good-stick-welds_34_jpeg_jpg.rf.4dda4c452265275489fb48216b070472.txt @@ -0,0 +1,2 @@ +1 0.15625 0.37109375 0.221875 0.140625 +1 0.4859375 0.575 0.321875 0.2484375 diff --git a/valid/labels/good-stick-welds_40_jpeg.rf.02d6464767a154c7e9eb48831dd0b5cd.txt b/valid/labels/good-stick-welds_40_jpeg.rf.02d6464767a154c7e9eb48831dd0b5cd.txt new file mode 100644 index 0000000000000000000000000000000000000000..8127e23129864a3ac58b7948da8694acb3713b8f --- /dev/null +++ b/valid/labels/good-stick-welds_40_jpeg.rf.02d6464767a154c7e9eb48831dd0b5cd.txt @@ -0,0 +1,2 @@ +1 0.48515625 0.35078125 0.8375 0.06015625 +0 0.52421875 0.56328125 0.91484375 0.35078125 diff --git a/valid/labels/good-stick-welds_40_jpeg_jpg.rf.0df4cdae3d76751da6e05881cf16abd3.txt b/valid/labels/good-stick-welds_40_jpeg_jpg.rf.0df4cdae3d76751da6e05881cf16abd3.txt new file mode 100644 index 0000000000000000000000000000000000000000..5e140e2ed0f361b571dc3b2966047d76750486bd --- /dev/null +++ b/valid/labels/good-stick-welds_40_jpeg_jpg.rf.0df4cdae3d76751da6e05881cf16abd3.txt @@ -0,0 +1,2 @@ +1 0.48515625 0.35078125 0.8375 0.0609375 +0 0.52421875 0.56328125 0.915625 0.3515625 diff --git a/valid/labels/good-stick-welds_5_jpeg.rf.5136a23b59deb0a08bc15d2231f61f03.txt b/valid/labels/good-stick-welds_5_jpeg.rf.5136a23b59deb0a08bc15d2231f61f03.txt new file mode 100644 index 0000000000000000000000000000000000000000..ff1baec07653b4428d7dd7c728bcd1e109a67c7a --- /dev/null +++ b/valid/labels/good-stick-welds_5_jpeg.rf.5136a23b59deb0a08bc15d2231f61f03.txt @@ -0,0 +1,3 @@ +0 0.23671875 0.725 0.359375 0.18046875 +1 0.6375 0.70546875 0.24296875 0.146875 +1 0.840625 0.803125 0.16015625 0.11640625 diff --git a/valid/labels/good-tig-welds_10_jpeg.rf.a597ec46a20477948091aa79f234549d.txt b/valid/labels/good-tig-welds_10_jpeg.rf.a597ec46a20477948091aa79f234549d.txt new file mode 100644 index 0000000000000000000000000000000000000000..ed0c6adc363332bb5df7379f03f059bbeb24403d --- /dev/null +++ b/valid/labels/good-tig-welds_10_jpeg.rf.a597ec46a20477948091aa79f234549d.txt @@ -0,0 +1,2 @@ +1 0.19765625 0.79375 0.3953125 0.19765625 +1 0.52109375 0.63671875 0.27734375 0.17578125 diff --git a/valid/labels/good-tig-welds_14_jpeg_jpg.rf.16154c6c23cd6940c695a23d4d9b91cd.txt b/valid/labels/good-tig-welds_14_jpeg_jpg.rf.16154c6c23cd6940c695a23d4d9b91cd.txt new file mode 100644 index 0000000000000000000000000000000000000000..7bb239e57485a239da72b8a657447564fcdbd49a --- /dev/null +++ b/valid/labels/good-tig-welds_14_jpeg_jpg.rf.16154c6c23cd6940c695a23d4d9b91cd.txt @@ -0,0 +1 @@ +1 0.46015625 0.60390625 0.396875 0.790625 diff --git a/valid/labels/good-tig-welds_15_png_jpg.rf.f1afde2a16c4e53b4a01cdfd30f8a8a8.txt b/valid/labels/good-tig-welds_15_png_jpg.rf.f1afde2a16c4e53b4a01cdfd30f8a8a8.txt new file mode 100644 index 0000000000000000000000000000000000000000..ac0d9bb1d11ff5b3860c8da853b1ca84da4526d3 --- /dev/null +++ b/valid/labels/good-tig-welds_15_png_jpg.rf.f1afde2a16c4e53b4a01cdfd30f8a8a8.txt @@ -0,0 +1 @@ +1 0.59609375 0.415625 0.8046875 0.83125 diff --git a/valid/labels/good-tig-welds_16_jpeg_jpg.rf.1a0a82cde3f2954e721d665985ab484a.txt b/valid/labels/good-tig-welds_16_jpeg_jpg.rf.1a0a82cde3f2954e721d665985ab484a.txt new file mode 100644 index 0000000000000000000000000000000000000000..0b3fcc48be201b38828468fa75074812022e215b --- /dev/null +++ b/valid/labels/good-tig-welds_16_jpeg_jpg.rf.1a0a82cde3f2954e721d665985ab484a.txt @@ -0,0 +1,2 @@ +1 0.725 0.30234375 0.1015625 0.3359375 +1 0.53046875 0.525 0.2734375 0.165625 diff --git a/valid/labels/good-tig-welds_24_jpeg_jpg.rf.ecb134263a51d2cf0640dc0ffc1adfb3.txt b/valid/labels/good-tig-welds_24_jpeg_jpg.rf.ecb134263a51d2cf0640dc0ffc1adfb3.txt new file mode 100644 index 0000000000000000000000000000000000000000..0401c4234bbda5853286eb24318b29fe0133a189 --- /dev/null +++ b/valid/labels/good-tig-welds_24_jpeg_jpg.rf.ecb134263a51d2cf0640dc0ffc1adfb3.txt @@ -0,0 +1,3 @@ +1 0.2328125 0.271875 0.2078125 0.1203125 +1 0.3765625 0.4546875 0.209375 0.1953125 +1 0.62265625 0.70859375 0.2984375 0.2671875 diff --git a/valid/labels/good-tig-welds_34_jpeg.rf.abf957630365786d0d4b244828d6ef61.txt b/valid/labels/good-tig-welds_34_jpeg.rf.abf957630365786d0d4b244828d6ef61.txt new file mode 100644 index 0000000000000000000000000000000000000000..6c80563f7f310ff169592488b4b98f8435b65e5f --- /dev/null +++ b/valid/labels/good-tig-welds_34_jpeg.rf.abf957630365786d0d4b244828d6ef61.txt @@ -0,0 +1 @@ +1 0.43828125 0.43359375 0.35703125 0.82578125 diff --git a/valid/labels/good-tig-welds_38_jpeg_jpg.rf.5dff2cd446adc29d410810665bae2aaf.txt b/valid/labels/good-tig-welds_38_jpeg_jpg.rf.5dff2cd446adc29d410810665bae2aaf.txt new file mode 100644 index 0000000000000000000000000000000000000000..a57d9ff5998dc58c35284432dcd49b6db46f0f35 --- /dev/null +++ b/valid/labels/good-tig-welds_38_jpeg_jpg.rf.5dff2cd446adc29d410810665bae2aaf.txt @@ -0,0 +1 @@ +1 0.39140625 0.57421875 0.58125 0.621875 diff --git a/valid/labels/good-tig-welds_42_jpeg.rf.ddb86cc0daba6eeb32ba03f54ba3e3f6.txt b/valid/labels/good-tig-welds_42_jpeg.rf.ddb86cc0daba6eeb32ba03f54ba3e3f6.txt new file mode 100644 index 0000000000000000000000000000000000000000..7af0ebe1aebe748a44488bba21ca9a0cfc89ce4a --- /dev/null +++ b/valid/labels/good-tig-welds_42_jpeg.rf.ddb86cc0daba6eeb32ba03f54ba3e3f6.txt @@ -0,0 +1 @@ +1 0.50859375 0.521875 0.9453125 0.15703125 diff --git a/valid/labels/good-tig-welds_46_jpeg.rf.9518c5cb28e92294488332ea0d90b63f.txt b/valid/labels/good-tig-welds_46_jpeg.rf.9518c5cb28e92294488332ea0d90b63f.txt new file mode 100644 index 0000000000000000000000000000000000000000..ed805d46fa8d16bef67ce736fbdce2722c079668 --- /dev/null +++ b/valid/labels/good-tig-welds_46_jpeg.rf.9518c5cb28e92294488332ea0d90b63f.txt @@ -0,0 +1 @@ +1 0.41328125 0.6546875 0.7953125 0.1765625 diff --git a/valid/labels/good-tig-welds_48_jpeg_jpg.rf.341822c37f412303bbce6f8ad8e9fcf6.txt b/valid/labels/good-tig-welds_48_jpeg_jpg.rf.341822c37f412303bbce6f8ad8e9fcf6.txt new file mode 100644 index 0000000000000000000000000000000000000000..43b45df7cd7566eedf52d50bb3ff0ff4461fb812 --- /dev/null +++ b/valid/labels/good-tig-welds_48_jpeg_jpg.rf.341822c37f412303bbce6f8ad8e9fcf6.txt @@ -0,0 +1 @@ +1 0.525 0.4984375 0.60625 0.3515625 diff --git a/valid/labels/good-tig-welds_4_jpeg.rf.969e447cb4eea7e399674a997b94d626.txt b/valid/labels/good-tig-welds_4_jpeg.rf.969e447cb4eea7e399674a997b94d626.txt new file mode 100644 index 0000000000000000000000000000000000000000..9e55476e39d34f2309c865003c0dd2387ac1a9ca --- /dev/null +++ b/valid/labels/good-tig-welds_4_jpeg.rf.969e447cb4eea7e399674a997b94d626.txt @@ -0,0 +1 @@ +1 0.596875 0.5578125 0.76640625 0.4578125 diff --git a/valid/labels/good_weld_vid1000_jpeg.rf.431b1ac56af2da7e93f8cb80d41df8b0.txt b/valid/labels/good_weld_vid1000_jpeg.rf.431b1ac56af2da7e93f8cb80d41df8b0.txt new file mode 100644 index 0000000000000000000000000000000000000000..f8ea544321e7bcc452d0da6deeddee56b2afc9c5 --- /dev/null +++ b/valid/labels/good_weld_vid1000_jpeg.rf.431b1ac56af2da7e93f8cb80d41df8b0.txt @@ -0,0 +1,2 @@ +1 0.1765625 0.65234375 0.23125 0.3234375 +1 0.396875 0.365625 0.1953125 0.309375 diff --git a/valid/labels/good_weld_vid1001_jpeg.rf.c05d6b9a3bff284ea1b8e812b245ecd5.txt b/valid/labels/good_weld_vid1001_jpeg.rf.c05d6b9a3bff284ea1b8e812b245ecd5.txt new file mode 100644 index 0000000000000000000000000000000000000000..a0826bf087933b85e3db3a2dc85e1809973bd070 --- /dev/null +++ b/valid/labels/good_weld_vid1001_jpeg.rf.c05d6b9a3bff284ea1b8e812b245ecd5.txt @@ -0,0 +1,7 @@ +1 0.0515625 0.140625 0.04453125 0.21953125 +1 0.1234375 0.16796875 0.06953125 0.171875 +1 0.2046875 0.1859375 0.0578125 0.1640625 +1 0.41640625 0.509375 0.2515625 0.521875 +1 0.60703125 0.68515625 0.0546875 0.5265625 +1 0.71328125 0.67734375 0.08125 0.5375 +1 0.825 0.6390625 0.1328125 0.453125 diff --git a/valid/labels/good_weld_vid1002_jpeg.rf.4e0fd9118624ab11c89f35194f5fdebd.txt b/valid/labels/good_weld_vid1002_jpeg.rf.4e0fd9118624ab11c89f35194f5fdebd.txt new file mode 100644 index 0000000000000000000000000000000000000000..b0e0c1f215dcdb62f06d4409fb1ef63edd61424f --- /dev/null +++ b/valid/labels/good_weld_vid1002_jpeg.rf.4e0fd9118624ab11c89f35194f5fdebd.txt @@ -0,0 +1,7 @@ +1 0.06875 0.16875 0.05859375 0.2234375 +1 0.146875 0.20546875 0.07421875 0.21953125 +1 0.23203125 0.2625 0.0734375 0.225 +1 0.42265625 0.51796875 0.2515625 0.521875 +1 0.61328125 0.6640625 0.075 0.54140625 +1 0.7375 0.65078125 0.08125 0.5375 +1 0.86953125 0.65234375 0.15625 0.5234375 diff --git a/valid/labels/good_weld_vid103_jpeg.rf.4599c60a073a2d6879937423d4c15ed5.txt b/valid/labels/good_weld_vid103_jpeg.rf.4599c60a073a2d6879937423d4c15ed5.txt new file mode 100644 index 0000000000000000000000000000000000000000..5bc9e8c96a8487edf0d250ff5f7b3452c6f07cc0 --- /dev/null +++ b/valid/labels/good_weld_vid103_jpeg.rf.4599c60a073a2d6879937423d4c15ed5.txt @@ -0,0 +1 @@ +1 0.6375 0.603125 0.38203125 0.31796875 diff --git a/valid/labels/good_weld_vid1075_jpeg_jpg.rf.8676bc5578bc6b3d0f637b423d737b9c.txt b/valid/labels/good_weld_vid1075_jpeg_jpg.rf.8676bc5578bc6b3d0f637b423d737b9c.txt new file mode 100644 index 0000000000000000000000000000000000000000..a372be9475eb727c21d626820c568bbb3481e000 --- /dev/null +++ b/valid/labels/good_weld_vid1075_jpeg_jpg.rf.8676bc5578bc6b3d0f637b423d737b9c.txt @@ -0,0 +1 @@ +1 0.51953125 0.64765625 0.1609375 0.240625 diff --git a/valid/labels/good_weld_vid108_jpeg.rf.25c621a0f8095deb9f117b95e20c39af.txt b/valid/labels/good_weld_vid108_jpeg.rf.25c621a0f8095deb9f117b95e20c39af.txt new file mode 100644 index 0000000000000000000000000000000000000000..ba729aa31ada35634565b180490a05922f2e5efa --- /dev/null +++ b/valid/labels/good_weld_vid108_jpeg.rf.25c621a0f8095deb9f117b95e20c39af.txt @@ -0,0 +1 @@ +1 0.76015625 0.79375 0.184375 0.15390625 diff --git a/valid/labels/good_weld_vid1217_jpeg_jpg.rf.5f9a145c6b3abe5b8ff79c84c3550072.txt b/valid/labels/good_weld_vid1217_jpeg_jpg.rf.5f9a145c6b3abe5b8ff79c84c3550072.txt new file mode 100644 index 0000000000000000000000000000000000000000..64d8097a587145dee7c1a6a8ef810ed92230a1c0 --- /dev/null +++ b/valid/labels/good_weld_vid1217_jpeg_jpg.rf.5f9a145c6b3abe5b8ff79c84c3550072.txt @@ -0,0 +1,2 @@ +1 0.61328125 0.671875 0.0296875 0.271875 +1 0.7109375 0.56953125 0.1328125 0.1609375 diff --git a/valid/labels/good_weld_vid1240_jpeg.rf.f771a2cbc1cfc676225d2b5b58fcebd9.txt b/valid/labels/good_weld_vid1240_jpeg.rf.f771a2cbc1cfc676225d2b5b58fcebd9.txt new file mode 100644 index 0000000000000000000000000000000000000000..d0e70ef2f92973c18e4215858296f87814167278 --- /dev/null +++ b/valid/labels/good_weld_vid1240_jpeg.rf.f771a2cbc1cfc676225d2b5b58fcebd9.txt @@ -0,0 +1,2 @@ +1 0.340625 0.325 0.0984375 0.278125 +1 0.4421875 0.22890625 0.1 0.096875 diff --git a/valid/labels/good_weld_vid1250_jpeg.rf.184d36ad6973fa61dc667ece24d887ad.txt b/valid/labels/good_weld_vid1250_jpeg.rf.184d36ad6973fa61dc667ece24d887ad.txt new file mode 100644 index 0000000000000000000000000000000000000000..87acb881a835b46407285cc046ff24447a30569d --- /dev/null +++ b/valid/labels/good_weld_vid1250_jpeg.rf.184d36ad6973fa61dc667ece24d887ad.txt @@ -0,0 +1,2 @@ +1 0.6609375 0.80078125 0.04140625 0.390625 +1 0.575 0.4859375 0.06640625 0.0890625 diff --git a/valid/labels/good_weld_vid1263_jpeg_jpg.rf.45aab142d792aa34c644e783f02138d1.txt b/valid/labels/good_weld_vid1263_jpeg_jpg.rf.45aab142d792aa34c644e783f02138d1.txt new file mode 100644 index 0000000000000000000000000000000000000000..54e94eaecaeffee58d8acd290594d1de69f04257 --- /dev/null +++ b/valid/labels/good_weld_vid1263_jpeg_jpg.rf.45aab142d792aa34c644e783f02138d1.txt @@ -0,0 +1,2 @@ +1 0.4890625 0.5484375 0.4484375 0.1359375 +1 0.4765625 0.41171875 0.3171875 0.121875 diff --git a/valid/labels/good_weld_vid1265_jpeg.rf.cb7970d35fd26518c02d6a73ee17231a.txt b/valid/labels/good_weld_vid1265_jpeg.rf.cb7970d35fd26518c02d6a73ee17231a.txt new file mode 100644 index 0000000000000000000000000000000000000000..2f90ba10ecb7cc60023b6efacb0c8f6ba8d1521b --- /dev/null +++ b/valid/labels/good_weld_vid1265_jpeg.rf.cb7970d35fd26518c02d6a73ee17231a.txt @@ -0,0 +1 @@ +1 0.3171875 0.69140625 0.20390625 0.203125 diff --git a/valid/labels/good_weld_vid148_jpeg.rf.6d84bab6b4e97783a6e9834004745ef4.txt b/valid/labels/good_weld_vid148_jpeg.rf.6d84bab6b4e97783a6e9834004745ef4.txt new file mode 100644 index 0000000000000000000000000000000000000000..d099c288e14a4d8bed01074866b386acb04dfca7 --- /dev/null +++ b/valid/labels/good_weld_vid148_jpeg.rf.6d84bab6b4e97783a6e9834004745ef4.txt @@ -0,0 +1 @@ +1 0.4375 0.47890625 0.6703125 0.21640625 diff --git a/valid/labels/good_weld_vid1520_jpeg_jpg.rf.069454b1311a4c9bb61c83c7e8c13101.txt b/valid/labels/good_weld_vid1520_jpeg_jpg.rf.069454b1311a4c9bb61c83c7e8c13101.txt new file mode 100644 index 0000000000000000000000000000000000000000..38671f5fe0b803939b8206c1a34543fc77fed1d9 --- /dev/null +++ b/valid/labels/good_weld_vid1520_jpeg_jpg.rf.069454b1311a4c9bb61c83c7e8c13101.txt @@ -0,0 +1 @@ +1 0.51015625 0.5078125 0.1828125 0.4328125 diff --git a/valid/labels/good_weld_vid1523_jpeg_jpg.rf.33293031b5a78828dc02481cb9afe063.txt b/valid/labels/good_weld_vid1523_jpeg_jpg.rf.33293031b5a78828dc02481cb9afe063.txt new file mode 100644 index 0000000000000000000000000000000000000000..218bd7756ec80e8e0b34419fe702d46504d826c9 --- /dev/null +++ b/valid/labels/good_weld_vid1523_jpeg_jpg.rf.33293031b5a78828dc02481cb9afe063.txt @@ -0,0 +1 @@ +1 0.5015625 0.5171875 0.16875 0.4125 diff --git a/valid/labels/good_weld_vid1527_jpeg.rf.8e23dad01703aec000043e81c88b8877.txt b/valid/labels/good_weld_vid1527_jpeg.rf.8e23dad01703aec000043e81c88b8877.txt new file mode 100644 index 0000000000000000000000000000000000000000..28ab22cb061a16fcb44d09d2a01054edb07cb8e8 --- /dev/null +++ b/valid/labels/good_weld_vid1527_jpeg.rf.8e23dad01703aec000043e81c88b8877.txt @@ -0,0 +1 @@ +1 0.5484375 0.4703125 0.11796875 0.21875 diff --git a/valid/labels/good_weld_vid1569_jpeg_jpg.rf.c7ecf8b67c461959a861afaf1a17b16c.txt b/valid/labels/good_weld_vid1569_jpeg_jpg.rf.c7ecf8b67c461959a861afaf1a17b16c.txt new file mode 100644 index 0000000000000000000000000000000000000000..24621ac1b050daab01591ebf18059a2b91a9ae7c --- /dev/null +++ b/valid/labels/good_weld_vid1569_jpeg_jpg.rf.c7ecf8b67c461959a861afaf1a17b16c.txt @@ -0,0 +1 @@ +1 0.515625 0.42421875 0.203125 0.0859375 diff --git a/valid/labels/good_weld_vid1600_jpeg_jpg.rf.e258db55de2a6988c92866a10db01064.txt b/valid/labels/good_weld_vid1600_jpeg_jpg.rf.e258db55de2a6988c92866a10db01064.txt new file mode 100644 index 0000000000000000000000000000000000000000..9d497d96e811763fa47bfc4c3eb3d0fcd5f40afd --- /dev/null +++ b/valid/labels/good_weld_vid1600_jpeg_jpg.rf.e258db55de2a6988c92866a10db01064.txt @@ -0,0 +1,4 @@ +1 0.41015625 0.4984375 0.4640625 0.0703125 +1 0.82109375 0.55859375 0.3484375 0.2234375 +1 0.39296875 0.3265625 0.325 0.2375 +1 0.79375 0.22578125 0.35625 0.1765625 diff --git a/valid/labels/good_weld_vid1604_jpeg_jpg.rf.940dd5f241fdcfffc6454c3bbf470937.txt b/valid/labels/good_weld_vid1604_jpeg_jpg.rf.940dd5f241fdcfffc6454c3bbf470937.txt new file mode 100644 index 0000000000000000000000000000000000000000..68210ce7f32c1fcb2fd3877f00ef5951825a0f9d --- /dev/null +++ b/valid/labels/good_weld_vid1604_jpeg_jpg.rf.940dd5f241fdcfffc6454c3bbf470937.txt @@ -0,0 +1,7 @@ +1 0.09453125 0.53671875 0.1890625 0.0703125 +1 0.171875 0.65859375 0.328125 0.159375 +1 0.56953125 0.68046875 0.2390625 0.35625 +1 0.84140625 0.52265625 0.23125 0.4109375 +1 0.7734375 0.215625 0.4328125 0.1734375 +1 0.1578125 0.2703125 0.3 0.2640625 +1 0.390625 0.1875 0.09375 0.1765625 diff --git a/valid/labels/good_weld_vid1680_jpeg.rf.e87dd04a5d63b3f51a22c0a7c0273485.txt b/valid/labels/good_weld_vid1680_jpeg.rf.e87dd04a5d63b3f51a22c0a7c0273485.txt new file mode 100644 index 0000000000000000000000000000000000000000..7eeedc3eabc27cc8e1e7a14e0c5605bfc585dabc --- /dev/null +++ b/valid/labels/good_weld_vid1680_jpeg.rf.e87dd04a5d63b3f51a22c0a7c0273485.txt @@ -0,0 +1 @@ +1 0.69140625 0.49375 0.565625 0.15078125 diff --git a/valid/labels/good_weld_vid1682_jpeg_jpg.rf.10257117cffe5eadf40ec722c68a44ec.txt b/valid/labels/good_weld_vid1682_jpeg_jpg.rf.10257117cffe5eadf40ec722c68a44ec.txt new file mode 100644 index 0000000000000000000000000000000000000000..d285823250a31bd20108f5d32623aedcec1b9d4f --- /dev/null +++ b/valid/labels/good_weld_vid1682_jpeg_jpg.rf.10257117cffe5eadf40ec722c68a44ec.txt @@ -0,0 +1 @@ +1 0.61484375 0.41796875 0.753125 0.2296875 diff --git a/valid/labels/good_weld_vid1684_jpeg.rf.5a7dce32f42570add99076f5721f129d.txt b/valid/labels/good_weld_vid1684_jpeg.rf.5a7dce32f42570add99076f5721f129d.txt new file mode 100644 index 0000000000000000000000000000000000000000..619e87413605f59cc05408ea47a2bae5fea7a7d3 --- /dev/null +++ b/valid/labels/good_weld_vid1684_jpeg.rf.5a7dce32f42570add99076f5721f129d.txt @@ -0,0 +1 @@ +1 0.57734375 0.38828125 0.84375 0.30078125 diff --git a/valid/labels/good_weld_vid1738_jpeg.rf.276fcdc411baa162469c26c8a0c60a2f.txt b/valid/labels/good_weld_vid1738_jpeg.rf.276fcdc411baa162469c26c8a0c60a2f.txt new file mode 100644 index 0000000000000000000000000000000000000000..33e3a0e357f26b2798cdc0db5ba76020e6215607 --- /dev/null +++ b/valid/labels/good_weld_vid1738_jpeg.rf.276fcdc411baa162469c26c8a0c60a2f.txt @@ -0,0 +1,3 @@ +1 0.49609375 0.5359375 0.246875 0.034375 +1 0.234375 0.68046875 0.0359375 0.15625 +1 0.75546875 0.6828125 0.02890625 0.16015625 diff --git a/valid/labels/good_weld_vid1738_jpeg_jpg.rf.56e11c16e8efd8dbc814badff75dd505.txt b/valid/labels/good_weld_vid1738_jpeg_jpg.rf.56e11c16e8efd8dbc814badff75dd505.txt new file mode 100644 index 0000000000000000000000000000000000000000..5c86b2fc8a4d90fedf9f1cb3db7f1c788796dde8 --- /dev/null +++ b/valid/labels/good_weld_vid1738_jpeg_jpg.rf.56e11c16e8efd8dbc814badff75dd505.txt @@ -0,0 +1,3 @@ +1 0.49609375 0.5359375 0.246875 0.034375 +1 0.234375 0.68046875 0.0359375 0.15625 +1 0.75546875 0.6828125 0.028125 0.1609375 diff --git a/valid/labels/good_weld_vid1770_jpeg.rf.5ede94d7661002ef99197a6a3eddebb0.txt b/valid/labels/good_weld_vid1770_jpeg.rf.5ede94d7661002ef99197a6a3eddebb0.txt new file mode 100644 index 0000000000000000000000000000000000000000..d03235b8d73ef98d56dce3a41f1fc1e5beb58418 --- /dev/null +++ b/valid/labels/good_weld_vid1770_jpeg.rf.5ede94d7661002ef99197a6a3eddebb0.txt @@ -0,0 +1 @@ +1 0.4859375 0.4390625 0.84296875 0.0703125 diff --git a/valid/labels/good_weld_vid1770_jpeg_jpg.rf.3d6ac3ab48c3f9f8a78b613b1675f730.txt b/valid/labels/good_weld_vid1770_jpeg_jpg.rf.3d6ac3ab48c3f9f8a78b613b1675f730.txt new file mode 100644 index 0000000000000000000000000000000000000000..27cb8da2c4851e0154fe78b6242c30be741c7b08 --- /dev/null +++ b/valid/labels/good_weld_vid1770_jpeg_jpg.rf.3d6ac3ab48c3f9f8a78b613b1675f730.txt @@ -0,0 +1 @@ +1 0.4859375 0.4390625 0.84375 0.0703125 diff --git a/valid/labels/good_weld_vid1780_jpeg_jpg.rf.b4c96e5853360d3bbc6cfaeea9477bf6.txt b/valid/labels/good_weld_vid1780_jpeg_jpg.rf.b4c96e5853360d3bbc6cfaeea9477bf6.txt new file mode 100644 index 0000000000000000000000000000000000000000..1b63c708d723aa41e1605b82a0a66dc8e2963e70 --- /dev/null +++ b/valid/labels/good_weld_vid1780_jpeg_jpg.rf.b4c96e5853360d3bbc6cfaeea9477bf6.txt @@ -0,0 +1,2 @@ +1 0.21875 0.59765625 0.4359375 0.1828125 +1 0.72265625 0.4015625 0.4765625 0.3203125 diff --git a/valid/labels/good_weld_vid1783_jpeg_jpg.rf.ef6a5c0a7e855c352349e3280e259c99.txt b/valid/labels/good_weld_vid1783_jpeg_jpg.rf.ef6a5c0a7e855c352349e3280e259c99.txt new file mode 100644 index 0000000000000000000000000000000000000000..591a5159c6bcb9d0a479aa77b62b1e36ce6f9d03 --- /dev/null +++ b/valid/labels/good_weld_vid1783_jpeg_jpg.rf.ef6a5c0a7e855c352349e3280e259c99.txt @@ -0,0 +1,3 @@ +1 0.46953125 0.50703125 0.4359375 0.0453125 +1 0.7265625 0.446875 0.0859375 0.0765625 +1 0.1890625 0.46953125 0.078125 0.04375 diff --git a/valid/labels/good_weld_vid1788_jpeg.rf.f2c2a7aa4fa7b5603c45af044b166685.txt b/valid/labels/good_weld_vid1788_jpeg.rf.f2c2a7aa4fa7b5603c45af044b166685.txt new file mode 100644 index 0000000000000000000000000000000000000000..cccad1202918bf0a2de7de89c50153c0da95d2dc --- /dev/null +++ b/valid/labels/good_weld_vid1788_jpeg.rf.f2c2a7aa4fa7b5603c45af044b166685.txt @@ -0,0 +1 @@ +1 0.68125 0.67734375 0.3578125 0.37109375 diff --git a/valid/labels/good_weld_vid187_jpeg_jpg.rf.5bfdaa71186008f89ba60f228fa99da5.txt b/valid/labels/good_weld_vid187_jpeg_jpg.rf.5bfdaa71186008f89ba60f228fa99da5.txt new file mode 100644 index 0000000000000000000000000000000000000000..4b3faab77e2c10002efb6e5275aa31547448ef16 --- /dev/null +++ b/valid/labels/good_weld_vid187_jpeg_jpg.rf.5bfdaa71186008f89ba60f228fa99da5.txt @@ -0,0 +1 @@ +1 0.3578125 0.359375 0.509375 0.234375 diff --git a/valid/labels/good_weld_vid1929_jpeg.rf.6bb57f69405ec3f3682f9540b0ff183e.txt b/valid/labels/good_weld_vid1929_jpeg.rf.6bb57f69405ec3f3682f9540b0ff183e.txt new file mode 100644 index 0000000000000000000000000000000000000000..f38fb8312c080a69ec17964e14cc13823022be7c --- /dev/null +++ b/valid/labels/good_weld_vid1929_jpeg.rf.6bb57f69405ec3f3682f9540b0ff183e.txt @@ -0,0 +1 @@ +1 0.54375 0.50390625 0.87421875 0.22421875 diff --git a/valid/labels/good_weld_vid1933_jpeg.rf.19902af76debc606df4fc2f2f8ef5396.txt b/valid/labels/good_weld_vid1933_jpeg.rf.19902af76debc606df4fc2f2f8ef5396.txt new file mode 100644 index 0000000000000000000000000000000000000000..75c3c2e535b1514f75602f0d031ff8bf51f934a3 --- /dev/null +++ b/valid/labels/good_weld_vid1933_jpeg.rf.19902af76debc606df4fc2f2f8ef5396.txt @@ -0,0 +1 @@ +1 0.51484375 0.5203125 0.93671875 0.55703125 diff --git a/valid/labels/good_weld_vid1933_jpeg_jpg.rf.8b6a6ebb96490e82e6da0202e37ae0a4.txt b/valid/labels/good_weld_vid1933_jpeg_jpg.rf.8b6a6ebb96490e82e6da0202e37ae0a4.txt new file mode 100644 index 0000000000000000000000000000000000000000..593f556cf9573711a4b3800481842b01ec68c084 --- /dev/null +++ b/valid/labels/good_weld_vid1933_jpeg_jpg.rf.8b6a6ebb96490e82e6da0202e37ae0a4.txt @@ -0,0 +1 @@ +1 0.51484375 0.5203125 0.9375 0.5578125 diff --git a/valid/labels/good_weld_vid1975_jpeg_jpg.rf.b4e52a3f47008ca065356ebc2b462bbc.txt b/valid/labels/good_weld_vid1975_jpeg_jpg.rf.b4e52a3f47008ca065356ebc2b462bbc.txt new file mode 100644 index 0000000000000000000000000000000000000000..dc4ea101efd72f178096c150c946f41d008ebfa4 --- /dev/null +++ b/valid/labels/good_weld_vid1975_jpeg_jpg.rf.b4e52a3f47008ca065356ebc2b462bbc.txt @@ -0,0 +1,4 @@ +1 0.396875 0.7890625 0.5484375 0.1296875 +1 0.45 0.3515625 0.4859375 0.084375 +1 0.7390625 0.56171875 0.1640625 0.321875 +1 0.10859375 0.5640625 0.1296875 0.2921875 diff --git a/valid/labels/good_weld_vid2007_jpeg_jpg.rf.c0ce2bdcd026b431991acfbe28ca05b6.txt b/valid/labels/good_weld_vid2007_jpeg_jpg.rf.c0ce2bdcd026b431991acfbe28ca05b6.txt new file mode 100644 index 0000000000000000000000000000000000000000..98800079682d89e403846a617ab69a31deda7039 --- /dev/null +++ b/valid/labels/good_weld_vid2007_jpeg_jpg.rf.c0ce2bdcd026b431991acfbe28ca05b6.txt @@ -0,0 +1 @@ +1 0.5296875 0.5109375 0.88125 0.740625 diff --git a/valid/labels/good_weld_vid2030_jpeg.rf.a6b04126e9c1e5ca28b08733a8e11c4e.txt b/valid/labels/good_weld_vid2030_jpeg.rf.a6b04126e9c1e5ca28b08733a8e11c4e.txt new file mode 100644 index 0000000000000000000000000000000000000000..51f50f1e253a9373c1351a3923c8809e2ed6c601 --- /dev/null +++ b/valid/labels/good_weld_vid2030_jpeg.rf.a6b04126e9c1e5ca28b08733a8e11c4e.txt @@ -0,0 +1 @@ +1 0.56171875 0.553125 0.34296875 0.44921875 diff --git a/valid/labels/good_weld_vid273_jpeg_jpg.rf.f4ba448c45acb0afd49bc4ae2a2b8428.txt b/valid/labels/good_weld_vid273_jpeg_jpg.rf.f4ba448c45acb0afd49bc4ae2a2b8428.txt new file mode 100644 index 0000000000000000000000000000000000000000..b9955de2ff4d6bae7af82a08206e6ea57e2df65d --- /dev/null +++ b/valid/labels/good_weld_vid273_jpeg_jpg.rf.f4ba448c45acb0afd49bc4ae2a2b8428.txt @@ -0,0 +1 @@ +1 0.64609375 0.4171875 0.2171875 0.834375 diff --git a/valid/labels/good_weld_vid275_jpeg_jpg.rf.b82ae5625c6da2b43a53cd057e49165d.txt b/valid/labels/good_weld_vid275_jpeg_jpg.rf.b82ae5625c6da2b43a53cd057e49165d.txt new file mode 100644 index 0000000000000000000000000000000000000000..a542427394bed50fd5e804a596b6df1be03f7f0b --- /dev/null +++ b/valid/labels/good_weld_vid275_jpeg_jpg.rf.b82ae5625c6da2b43a53cd057e49165d.txt @@ -0,0 +1 @@ +1 0.6203125 0.46875 0.2390625 0.9375 diff --git a/valid/labels/good_weld_vid332_jpeg.rf.27283c9e6c56ffd45375c220c32cd2a8.txt b/valid/labels/good_weld_vid332_jpeg.rf.27283c9e6c56ffd45375c220c32cd2a8.txt new file mode 100644 index 0000000000000000000000000000000000000000..b0d0f0507d5d8d60f272f35b1a5e7ec758c0d970 --- /dev/null +++ b/valid/labels/good_weld_vid332_jpeg.rf.27283c9e6c56ffd45375c220c32cd2a8.txt @@ -0,0 +1 @@ +1 0.7 0.559375 0.15859375 0.2125 diff --git a/valid/labels/good_weld_vid467_jpeg_jpg.rf.fb3a42f9145ece41a08fa662d976d30d.txt b/valid/labels/good_weld_vid467_jpeg_jpg.rf.fb3a42f9145ece41a08fa662d976d30d.txt new file mode 100644 index 0000000000000000000000000000000000000000..5e7721a5a6ba30875eb2a51a1ffda13d53c7cc11 --- /dev/null +++ b/valid/labels/good_weld_vid467_jpeg_jpg.rf.fb3a42f9145ece41a08fa662d976d30d.txt @@ -0,0 +1 @@ +1 0.640625 0.78046875 0.1859375 0.4359375 diff --git a/valid/labels/good_weld_vid468_jpeg.rf.9c534a5a48dda4edfff77e57bef9944b.txt b/valid/labels/good_weld_vid468_jpeg.rf.9c534a5a48dda4edfff77e57bef9944b.txt new file mode 100644 index 0000000000000000000000000000000000000000..bea0b850317ba859c6c74e0c92090754f4283c25 --- /dev/null +++ b/valid/labels/good_weld_vid468_jpeg.rf.9c534a5a48dda4edfff77e57bef9944b.txt @@ -0,0 +1 @@ +1 0.6375 0.54453125 0.18515625 0.4359375 diff --git a/valid/labels/good_weld_vid481_jpeg_jpg.rf.1af79b409340dde5afc20610357ac570.txt b/valid/labels/good_weld_vid481_jpeg_jpg.rf.1af79b409340dde5afc20610357ac570.txt new file mode 100644 index 0000000000000000000000000000000000000000..4d4cc5fa30df568db7d8920a81990fd74bfdc7f6 --- /dev/null +++ b/valid/labels/good_weld_vid481_jpeg_jpg.rf.1af79b409340dde5afc20610357ac570.txt @@ -0,0 +1 @@ +1 0.46640625 0.5578125 0.4453125 0.2234375 diff --git a/valid/labels/good_weld_vid506_jpeg.rf.640a0f3404338397380a5c420189c3b0.txt b/valid/labels/good_weld_vid506_jpeg.rf.640a0f3404338397380a5c420189c3b0.txt new file mode 100644 index 0000000000000000000000000000000000000000..2e7b7da798af97c176ea721a305bdb68a126f28b --- /dev/null +++ b/valid/labels/good_weld_vid506_jpeg.rf.640a0f3404338397380a5c420189c3b0.txt @@ -0,0 +1 @@ +1 0.5171875 0.62578125 0.05703125 0.10390625 diff --git a/valid/labels/good_weld_vid567_jpeg.rf.bd51fda54e1eb420596dc22b9ebed738.txt b/valid/labels/good_weld_vid567_jpeg.rf.bd51fda54e1eb420596dc22b9ebed738.txt new file mode 100644 index 0000000000000000000000000000000000000000..f0ed06d80bbfd918c5c3f8dc70ab7e1d2bf0ec31 --- /dev/null +++ b/valid/labels/good_weld_vid567_jpeg.rf.bd51fda54e1eb420596dc22b9ebed738.txt @@ -0,0 +1 @@ +1 0.4921875 0.66875 0.16640625 0.4265625 diff --git a/valid/labels/good_weld_vid583_jpeg.rf.f1d0ad3980cbf6e1c2c8bb81614ba486.txt b/valid/labels/good_weld_vid583_jpeg.rf.f1d0ad3980cbf6e1c2c8bb81614ba486.txt new file mode 100644 index 0000000000000000000000000000000000000000..605da7235f2d0354de3cf42e8fd5de9ed60ae2be --- /dev/null +++ b/valid/labels/good_weld_vid583_jpeg.rf.f1d0ad3980cbf6e1c2c8bb81614ba486.txt @@ -0,0 +1,2 @@ +1 0.390625 0.6609375 0.1734375 0.3359375 +1 0.5578125 0.540625 0.15546875 0.18203125 diff --git a/valid/labels/good_weld_vid584_jpeg.rf.54c326cbe938a698313b248457a890f8.txt b/valid/labels/good_weld_vid584_jpeg.rf.54c326cbe938a698313b248457a890f8.txt new file mode 100644 index 0000000000000000000000000000000000000000..605da7235f2d0354de3cf42e8fd5de9ed60ae2be --- /dev/null +++ b/valid/labels/good_weld_vid584_jpeg.rf.54c326cbe938a698313b248457a890f8.txt @@ -0,0 +1,2 @@ +1 0.390625 0.6609375 0.1734375 0.3359375 +1 0.5578125 0.540625 0.15546875 0.18203125 diff --git a/valid/labels/good_weld_vid628_jpeg_jpg.rf.11522af8f907da1a1c37b49b9b582846.txt b/valid/labels/good_weld_vid628_jpeg_jpg.rf.11522af8f907da1a1c37b49b9b582846.txt new file mode 100644 index 0000000000000000000000000000000000000000..02b778e5f6c16069e8742b8825e53b0f0a924003 --- /dev/null +++ b/valid/labels/good_weld_vid628_jpeg_jpg.rf.11522af8f907da1a1c37b49b9b582846.txt @@ -0,0 +1 @@ +1 0.76015625 0.621875 0.4765625 0.2609375 diff --git a/valid/labels/good_weld_vid631_jpeg_jpg.rf.2aaf532b39e4fc78fe0d91f14318f982.txt b/valid/labels/good_weld_vid631_jpeg_jpg.rf.2aaf532b39e4fc78fe0d91f14318f982.txt new file mode 100644 index 0000000000000000000000000000000000000000..333c42ea91fea26fa97d65b8f23be30e11675649 --- /dev/null +++ b/valid/labels/good_weld_vid631_jpeg_jpg.rf.2aaf532b39e4fc78fe0d91f14318f982.txt @@ -0,0 +1 @@ +1 0.7359375 0.5546875 0.5265625 0.3265625 diff --git a/valid/labels/good_weld_vid686_jpeg_jpg.rf.6a58a23440ba50cef78c98e9bee3ad34.txt b/valid/labels/good_weld_vid686_jpeg_jpg.rf.6a58a23440ba50cef78c98e9bee3ad34.txt new file mode 100644 index 0000000000000000000000000000000000000000..c0265e5d0657fead2d8122303f9d2ea44a0613c7 --- /dev/null +++ b/valid/labels/good_weld_vid686_jpeg_jpg.rf.6a58a23440ba50cef78c98e9bee3ad34.txt @@ -0,0 +1 @@ +1 0.4171875 0.646875 0.2 0.0625 diff --git a/valid/labels/good_weld_vid689_jpeg_jpg.rf.5231a0ce31b90674c7a49a6aa0691963.txt b/valid/labels/good_weld_vid689_jpeg_jpg.rf.5231a0ce31b90674c7a49a6aa0691963.txt new file mode 100644 index 0000000000000000000000000000000000000000..a63d45b9e78a89e56eeeb49d37f3f85c83d725b7 --- /dev/null +++ b/valid/labels/good_weld_vid689_jpeg_jpg.rf.5231a0ce31b90674c7a49a6aa0691963.txt @@ -0,0 +1 @@ +1 0.3640625 0.6078125 0.271875 0.0796875 diff --git a/valid/labels/good_weld_vid692_jpeg.rf.604d791ce43cc6c9bbd97a386cec3451.txt b/valid/labels/good_weld_vid692_jpeg.rf.604d791ce43cc6c9bbd97a386cec3451.txt new file mode 100644 index 0000000000000000000000000000000000000000..76b026d0d03a682f3a73efdfb2f69a94431914f3 --- /dev/null +++ b/valid/labels/good_weld_vid692_jpeg.rf.604d791ce43cc6c9bbd97a386cec3451.txt @@ -0,0 +1 @@ +1 0.2921875 0.55859375 0.309375 0.06640625 diff --git a/valid/labels/good_weld_vid704_jpeg.rf.41ca0a33942e0bcb936968f70be15d73.txt b/valid/labels/good_weld_vid704_jpeg.rf.41ca0a33942e0bcb936968f70be15d73.txt new file mode 100644 index 0000000000000000000000000000000000000000..ae1e6da6c6715ce6282562fe2713821941365ddd --- /dev/null +++ b/valid/labels/good_weld_vid704_jpeg.rf.41ca0a33942e0bcb936968f70be15d73.txt @@ -0,0 +1 @@ +1 0.578125 0.4359375 0.54375 0.1140625 diff --git a/valid/labels/good_weld_vid706_jpeg_jpg.rf.69f9004c760b047d124d0f1084118e80.txt b/valid/labels/good_weld_vid706_jpeg_jpg.rf.69f9004c760b047d124d0f1084118e80.txt new file mode 100644 index 0000000000000000000000000000000000000000..11dfc1f117e82ab7d9ec1a1838b406ab5b42a9fa --- /dev/null +++ b/valid/labels/good_weld_vid706_jpeg_jpg.rf.69f9004c760b047d124d0f1084118e80.txt @@ -0,0 +1 @@ +1 0.525 0.46328125 0.621875 0.096875 diff --git a/valid/labels/good_weld_vid708_jpeg_jpg.rf.dcc9a0bd5a16f6568adc86044f214671.txt b/valid/labels/good_weld_vid708_jpeg_jpg.rf.dcc9a0bd5a16f6568adc86044f214671.txt new file mode 100644 index 0000000000000000000000000000000000000000..39b82bd7c73aeec262fdf2a2c706e1b4149b0355 --- /dev/null +++ b/valid/labels/good_weld_vid708_jpeg_jpg.rf.dcc9a0bd5a16f6568adc86044f214671.txt @@ -0,0 +1 @@ +1 0.51484375 0.428125 0.621875 0.096875 diff --git a/valid/labels/good_weld_vid928_jpeg.rf.60d4886ddce4b044f0520f56825b491f.txt b/valid/labels/good_weld_vid928_jpeg.rf.60d4886ddce4b044f0520f56825b491f.txt new file mode 100644 index 0000000000000000000000000000000000000000..1045e44968dc8058183f39d82cb6472659e8517e --- /dev/null +++ b/valid/labels/good_weld_vid928_jpeg.rf.60d4886ddce4b044f0520f56825b491f.txt @@ -0,0 +1 @@ +1 0.396875 0.35390625 0.07890625 0.096875 diff --git a/valid/labels/good_weld_vid93_jpeg.rf.6798773d3f0a779f7191917ef52dc154.txt b/valid/labels/good_weld_vid93_jpeg.rf.6798773d3f0a779f7191917ef52dc154.txt new file mode 100644 index 0000000000000000000000000000000000000000..1c4667c7e478e5f88b35ec73f5aa31b02a6b50e2 --- /dev/null +++ b/valid/labels/good_weld_vid93_jpeg.rf.6798773d3f0a779f7191917ef52dc154.txt @@ -0,0 +1 @@ +1 0.5375 0.51953125 0.33828125 0.275 diff --git a/valid/labels/good_weld_vid98_jpeg.rf.36c1d83d40cfe0217688ab63b7873f23.txt b/valid/labels/good_weld_vid98_jpeg.rf.36c1d83d40cfe0217688ab63b7873f23.txt new file mode 100644 index 0000000000000000000000000000000000000000..70c1f950bc18f8a7cd7aa91215b8fe97fca4ed5e --- /dev/null +++ b/valid/labels/good_weld_vid98_jpeg.rf.36c1d83d40cfe0217688ab63b7873f23.txt @@ -0,0 +1 @@ +1 0.5 0.38125 0.16640625 0.75703125 diff --git a/valid/labels/good_weld_vid993_jpeg.rf.2f4706121723a28cdc38335a344af889.txt b/valid/labels/good_weld_vid993_jpeg.rf.2f4706121723a28cdc38335a344af889.txt new file mode 100644 index 0000000000000000000000000000000000000000..8192d11eb1b53f27228a05ecb0b3e770b60a1827 --- /dev/null +++ b/valid/labels/good_weld_vid993_jpeg.rf.2f4706121723a28cdc38335a344af889.txt @@ -0,0 +1,2 @@ +1 0.58828125 0.58203125 0.01875 0.36953125 +1 0.65703125 0.58984375 0.025 0.34296875 diff --git a/valid/labels/good_weld_vid995_jpeg.rf.3b97a81ea684a57bb12326f57752fbda.txt b/valid/labels/good_weld_vid995_jpeg.rf.3b97a81ea684a57bb12326f57752fbda.txt new file mode 100644 index 0000000000000000000000000000000000000000..319cd061d67151ee591251b158824bebea5f9fd7 --- /dev/null +++ b/valid/labels/good_weld_vid995_jpeg.rf.3b97a81ea684a57bb12326f57752fbda.txt @@ -0,0 +1,2 @@ +1 0.2015625 0.5171875 0.103125 0.4515625 +1 0.40546875 0.54140625 0.103125 0.4 diff --git a/valid/labels/imagSCes_jpeg_jpg.rf.edcce0b7cff3c48fd39c7803fee67900.txt b/valid/labels/imagSCes_jpeg_jpg.rf.edcce0b7cff3c48fd39c7803fee67900.txt new file mode 100644 index 0000000000000000000000000000000000000000..70790bb3a8e1aff00539786c683f5824708fa8fa --- /dev/null +++ b/valid/labels/imagSCes_jpeg_jpg.rf.edcce0b7cff3c48fd39c7803fee67900.txt @@ -0,0 +1,6 @@ +0 0.4984375 0.49375 0.996875 0.2703125 +2 0.0953125 0.509375 0.1421875 0.096875 +2 0.41015625 0.496875 0.1234375 0.0703125 +2 0.57265625 0.48046875 0.1015625 0.0515625 +2 0.71484375 0.47734375 0.1203125 0.084375 +2 0.9046875 0.490625 0.1859375 0.1484375 diff --git a/valid/labels/imagertrty4s_jpeg_jpg.rf.74107847fc0b3075d7e59d40593d32df.txt b/valid/labels/imagertrty4s_jpeg_jpg.rf.74107847fc0b3075d7e59d40593d32df.txt new file mode 100644 index 0000000000000000000000000000000000000000..24d87746dda58b6f698c2bdc6f6c5a17fd2a5fe4 --- /dev/null +++ b/valid/labels/imagertrty4s_jpeg_jpg.rf.74107847fc0b3075d7e59d40593d32df.txt @@ -0,0 +1 @@ +2 0.4890625 0.49609375 0.3734375 0.9921875 diff --git a/valid/labels/images_jpeg.rf.0ba3e75ca3821bc1ff657ab5b548aeb9.txt b/valid/labels/images_jpeg.rf.0ba3e75ca3821bc1ff657ab5b548aeb9.txt new file mode 100644 index 0000000000000000000000000000000000000000..92380aeeb8de53a4ecb9945b0b9a1fd3216e4b87 --- /dev/null +++ b/valid/labels/images_jpeg.rf.0ba3e75ca3821bc1ff657ab5b548aeb9.txt @@ -0,0 +1,6 @@ +0 0.1859375 0.48203125 0.221875 0.58515625 +0 0.67265625 0.3625 0.17890625 0.4328125 +2 0.1859375 0.5671875 0.078125 0.09765625 +2 0.1609375 0.47265625 0.08125 0.10390625 +2 0.1984375 0.28359375 0.0453125 0.04296875 +2 0.17734375 0.34453125 0.05546875 0.0546875 diff --git a/valid/labels/imagesdf_jpeg_jpg.rf.ba91add9d246d3cef499db334e8a4954.txt b/valid/labels/imagesdf_jpeg_jpg.rf.ba91add9d246d3cef499db334e8a4954.txt new file mode 100644 index 0000000000000000000000000000000000000000..38f0ba4b3f2fef678bf4c310b2a4d9ec36b1258d --- /dev/null +++ b/valid/labels/imagesdf_jpeg_jpg.rf.ba91add9d246d3cef499db334e8a4954.txt @@ -0,0 +1 @@ +1 0.49765625 0.4125 0.9953125 0.15 diff --git a/valid/labels/imagesrttytr_jpeg_jpg.rf.114d5014cd586dee989bb0a9858f7ff1.txt b/valid/labels/imagesrttytr_jpeg_jpg.rf.114d5014cd586dee989bb0a9858f7ff1.txt new file mode 100644 index 0000000000000000000000000000000000000000..0bfdb7989cb350ab6d48b7015d2b069a9913599c --- /dev/null +++ b/valid/labels/imagesrttytr_jpeg_jpg.rf.114d5014cd586dee989bb0a9858f7ff1.txt @@ -0,0 +1,3 @@ +0 0.521875 0.83515625 0.6796875 0.2203125 +1 0.49375 0.43515625 0.8140625 0.1796875 +1 0.62890625 0.1296875 0.646875 0.2109375 diff --git a/valid/labels/imagesry4y_jpeg_jpg.rf.a0d2397191b66ddf88ec1010ad73a781.txt b/valid/labels/imagesry4y_jpeg_jpg.rf.a0d2397191b66ddf88ec1010ad73a781.txt new file mode 100644 index 0000000000000000000000000000000000000000..194b61359014b6a368612bfef4ecb4cdb9bae483 --- /dev/null +++ b/valid/labels/imagesry4y_jpeg_jpg.rf.a0d2397191b66ddf88ec1010ad73a781.txt @@ -0,0 +1,3 @@ +0 0.159375 0.496875 0.196875 0.56875 +1 0.52421875 0.42265625 0.190625 0.7171875 +1 0.79765625 0.48671875 0.2390625 0.5359375 diff --git a/valid/labels/imagkvyfes_jpeg.rf.9a3675037a196097f81fbf8d3ee10c72.txt b/valid/labels/imagkvyfes_jpeg.rf.9a3675037a196097f81fbf8d3ee10c72.txt new file mode 100644 index 0000000000000000000000000000000000000000..3a0d392e2757c1ed7dffcbaf4e08360d21e133f0 --- /dev/null +++ b/valid/labels/imagkvyfes_jpeg.rf.9a3675037a196097f81fbf8d3ee10c72.txt @@ -0,0 +1,3 @@ +2 0.140625 0.4890625 0.084375 0.14140625 +2 0.28515625 0.49140625 0.0703125 0.1578125 +2 0.77265625 0.46015625 0.165625 0.084375 diff --git a/valid/labels/imagkvyfes_jpeg_jpg.rf.662acf5b9d03af6a8d54231561e9b285.txt b/valid/labels/imagkvyfes_jpeg_jpg.rf.662acf5b9d03af6a8d54231561e9b285.txt new file mode 100644 index 0000000000000000000000000000000000000000..135b030ef42528adf4649ce542047cb6f89a690c --- /dev/null +++ b/valid/labels/imagkvyfes_jpeg_jpg.rf.662acf5b9d03af6a8d54231561e9b285.txt @@ -0,0 +1,3 @@ +2 0.140625 0.4890625 0.084375 0.1421875 +2 0.28515625 0.49140625 0.0703125 0.1578125 +2 0.77265625 0.46015625 0.165625 0.084375 diff --git a/valid/labels/istockphoto-1006281428-612x612_jpeg_jpg.rf.097a9032fb3decdd9fec0d929cb29754.txt b/valid/labels/istockphoto-1006281428-612x612_jpeg_jpg.rf.097a9032fb3decdd9fec0d929cb29754.txt new file mode 100644 index 0000000000000000000000000000000000000000..feb791e406faeb350e11f55c9ebf5e09e1be3cc1 --- /dev/null +++ b/valid/labels/istockphoto-1006281428-612x612_jpeg_jpg.rf.097a9032fb3decdd9fec0d929cb29754.txt @@ -0,0 +1 @@ +2 0.5359375 0.59765625 0.565625 0.26875 diff --git a/valid/labels/istockphoto-1006281470-612x612_jpeg.rf.c340a57a2fa3f33cf21bd28b6e96e28a.txt b/valid/labels/istockphoto-1006281470-612x612_jpeg.rf.c340a57a2fa3f33cf21bd28b6e96e28a.txt new file mode 100644 index 0000000000000000000000000000000000000000..4283a2af23c9bfa989c77cdbab790620f062b20b --- /dev/null +++ b/valid/labels/istockphoto-1006281470-612x612_jpeg.rf.c340a57a2fa3f33cf21bd28b6e96e28a.txt @@ -0,0 +1,2 @@ +2 0.671875 0.33125 0.0328125 0.03046875 +2 0.6015625 0.5390625 0.01953125 0.028125 diff --git a/valid/labels/istockphoto-1006281470-612x612_jpeg_jpg.rf.c7d8b3cfa109ff2f895494227f0f3355.txt b/valid/labels/istockphoto-1006281470-612x612_jpeg_jpg.rf.c7d8b3cfa109ff2f895494227f0f3355.txt new file mode 100644 index 0000000000000000000000000000000000000000..d8d929a42e929949162fa3d850ae5bd971089237 --- /dev/null +++ b/valid/labels/istockphoto-1006281470-612x612_jpeg_jpg.rf.c7d8b3cfa109ff2f895494227f0f3355.txt @@ -0,0 +1,2 @@ +2 0.671875 0.33125 0.0328125 0.03125 +2 0.6015625 0.5390625 0.0203125 0.028125 diff --git a/valid/labels/istockphoto-1006281518-612x612_jpeg.rf.1de08bb6edf46aa7cf6b31e420d73ce6.txt b/valid/labels/istockphoto-1006281518-612x612_jpeg.rf.1de08bb6edf46aa7cf6b31e420d73ce6.txt new file mode 100644 index 0000000000000000000000000000000000000000..4aff8fcf46b45a7f7d22368daa8a2c6943f5f314 --- /dev/null +++ b/valid/labels/istockphoto-1006281518-612x612_jpeg.rf.1de08bb6edf46aa7cf6b31e420d73ce6.txt @@ -0,0 +1,3 @@ +0 0.5328125 0.4109375 0.93125 0.19375 +2 0.16171875 0.35546875 0.12734375 0.04765625 +2 0.8140625 0.4125 0.09453125 0.05859375 diff --git a/valid/labels/istockphoto-1008822794-612x612_jpeg.rf.1ba2cbaa48f5a7824fa2f7d098a4e274.txt b/valid/labels/istockphoto-1008822794-612x612_jpeg.rf.1ba2cbaa48f5a7824fa2f7d098a4e274.txt new file mode 100644 index 0000000000000000000000000000000000000000..494f48beb4efe55e93e04a3b4ffc881f6211216d --- /dev/null +++ b/valid/labels/istockphoto-1008822794-612x612_jpeg.rf.1ba2cbaa48f5a7824fa2f7d098a4e274.txt @@ -0,0 +1 @@ +0 0.5 0.515625 0.9671875 0.159375 diff --git a/valid/labels/istockphoto-1008822794-612x612_jpeg_jpg.rf.e367824ca13919c36524749a3eaf2890.txt b/valid/labels/istockphoto-1008822794-612x612_jpeg_jpg.rf.e367824ca13919c36524749a3eaf2890.txt new file mode 100644 index 0000000000000000000000000000000000000000..494f48beb4efe55e93e04a3b4ffc881f6211216d --- /dev/null +++ b/valid/labels/istockphoto-1008822794-612x612_jpeg_jpg.rf.e367824ca13919c36524749a3eaf2890.txt @@ -0,0 +1 @@ +0 0.5 0.515625 0.9671875 0.159375 diff --git a/valid/labels/istockphoto-1329411389-612x612_jpeg.rf.d8805916b1db1bf82de3c0b248ac0840.txt b/valid/labels/istockphoto-1329411389-612x612_jpeg.rf.d8805916b1db1bf82de3c0b248ac0840.txt new file mode 100644 index 0000000000000000000000000000000000000000..3c74b17758c82fc0d2dfcccf0fc1f84cd64d2e3d --- /dev/null +++ b/valid/labels/istockphoto-1329411389-612x612_jpeg.rf.d8805916b1db1bf82de3c0b248ac0840.txt @@ -0,0 +1 @@ +0 0.4921875 0.5390625 0.425 0.37265625 diff --git a/valid/labels/istockphoto-1341142829-612x612_jpeg.rf.8662723e5b33d0168fcac1f214c2bf5f.txt b/valid/labels/istockphoto-1341142829-612x612_jpeg.rf.8662723e5b33d0168fcac1f214c2bf5f.txt new file mode 100644 index 0000000000000000000000000000000000000000..9442ffccedbcbb232a57596183b54dd435de372e --- /dev/null +++ b/valid/labels/istockphoto-1341142829-612x612_jpeg.rf.8662723e5b33d0168fcac1f214c2bf5f.txt @@ -0,0 +1 @@ +2 0.51796875 0.625 0.06875 0.41640625 diff --git a/valid/labels/istockphoto-1341142829-612x612_jpeg_jpg.rf.35fd75d819410e802938795158ed5bf6.txt b/valid/labels/istockphoto-1341142829-612x612_jpeg_jpg.rf.35fd75d819410e802938795158ed5bf6.txt new file mode 100644 index 0000000000000000000000000000000000000000..f13cea022091f4eb192d5b2b68bbe679033c3db6 --- /dev/null +++ b/valid/labels/istockphoto-1341142829-612x612_jpeg_jpg.rf.35fd75d819410e802938795158ed5bf6.txt @@ -0,0 +1 @@ +2 0.51796875 0.625 0.06875 0.4171875 diff --git a/valid/labels/mig-good-welds_10_jpeg_jpg.rf.b35c10d98c3d3b194b87a6a11e8d5204.txt b/valid/labels/mig-good-welds_10_jpeg_jpg.rf.b35c10d98c3d3b194b87a6a11e8d5204.txt new file mode 100644 index 0000000000000000000000000000000000000000..5896c4da6922586c6e0b1bf6ac8d945fcc9c84fc --- /dev/null +++ b/valid/labels/mig-good-welds_10_jpeg_jpg.rf.b35c10d98c3d3b194b87a6a11e8d5204.txt @@ -0,0 +1,2 @@ +1 0.21640625 0.64765625 0.3140625 0.1765625 +1 0.6046875 0.45703125 0.484375 0.215625 diff --git a/valid/labels/mig-good-welds_11_jpeg.rf.f7d53cdf1deeee8d1ebb918d2788f3ee.txt b/valid/labels/mig-good-welds_11_jpeg.rf.f7d53cdf1deeee8d1ebb918d2788f3ee.txt new file mode 100644 index 0000000000000000000000000000000000000000..8617dc7aa85212e299c4c2cf22d0c4015900279a --- /dev/null +++ b/valid/labels/mig-good-welds_11_jpeg.rf.f7d53cdf1deeee8d1ebb918d2788f3ee.txt @@ -0,0 +1,3 @@ +1 0.51953125 0.1453125 0.85703125 0.1703125 +0 0.48828125 0.5 0.86484375 0.1703125 +0 0.54921875 0.7953125 0.63125 0.2203125 diff --git a/valid/labels/mig-good-welds_18_jpeg.rf.a6229f75ebdfb3e8f60f32c424023b57.txt b/valid/labels/mig-good-welds_18_jpeg.rf.a6229f75ebdfb3e8f60f32c424023b57.txt new file mode 100644 index 0000000000000000000000000000000000000000..4cbed2fd5053b6272d3a8daa3793f0c369a4c643 --- /dev/null +++ b/valid/labels/mig-good-welds_18_jpeg.rf.a6229f75ebdfb3e8f60f32c424023b57.txt @@ -0,0 +1 @@ +1 0.55625 0.459375 0.828125 0.79453125 diff --git a/valid/labels/mig-good-welds_25_jpeg_jpg.rf.67ba7b27a9740a2cee33de0b2aa07b38.txt b/valid/labels/mig-good-welds_25_jpeg_jpg.rf.67ba7b27a9740a2cee33de0b2aa07b38.txt new file mode 100644 index 0000000000000000000000000000000000000000..7cb6eeb866d646f498b821bd1671945a556f89ab --- /dev/null +++ b/valid/labels/mig-good-welds_25_jpeg_jpg.rf.67ba7b27a9740a2cee33de0b2aa07b38.txt @@ -0,0 +1,2 @@ +1 0.1609375 0.44375 0.321875 0.14375 +1 0.76796875 0.4375 0.3390625 0.13125 diff --git a/valid/labels/mig-good-welds_26_jpeg_jpg.rf.d2df980ab9ff653d757151b3f09c7b60.txt b/valid/labels/mig-good-welds_26_jpeg_jpg.rf.d2df980ab9ff653d757151b3f09c7b60.txt new file mode 100644 index 0000000000000000000000000000000000000000..19c3db39026b0d70b02c175f4ca8884e8839b336 --- /dev/null +++ b/valid/labels/mig-good-welds_26_jpeg_jpg.rf.d2df980ab9ff653d757151b3f09c7b60.txt @@ -0,0 +1 @@ +1 0.56796875 0.50703125 0.390625 0.328125 diff --git a/valid/labels/mig-good-welds_27_jpeg_jpg.rf.a62ab80b5453ebdff52f4318f95a2128.txt b/valid/labels/mig-good-welds_27_jpeg_jpg.rf.a62ab80b5453ebdff52f4318f95a2128.txt new file mode 100644 index 0000000000000000000000000000000000000000..e552980b6e1b970d088e19ed1a81d4649de45cc4 --- /dev/null +++ b/valid/labels/mig-good-welds_27_jpeg_jpg.rf.a62ab80b5453ebdff52f4318f95a2128.txt @@ -0,0 +1 @@ +1 0.54375 0.5015625 0.134375 0.7859375 diff --git a/valid/labels/mig-good-welds_31_jpeg_jpg.rf.15788d80fb006bac20b18c5e25a8ab38.txt b/valid/labels/mig-good-welds_31_jpeg_jpg.rf.15788d80fb006bac20b18c5e25a8ab38.txt new file mode 100644 index 0000000000000000000000000000000000000000..44276546387a71d1013cc635c42cb2e12985ee37 --- /dev/null +++ b/valid/labels/mig-good-welds_31_jpeg_jpg.rf.15788d80fb006bac20b18c5e25a8ab38.txt @@ -0,0 +1 @@ +1 0.56015625 0.64921875 0.203125 0.696875 diff --git a/valid/labels/mig-good-welds_35_jpeg_jpg.rf.cd003ef912040fb387bc238928885861.txt b/valid/labels/mig-good-welds_35_jpeg_jpg.rf.cd003ef912040fb387bc238928885861.txt new file mode 100644 index 0000000000000000000000000000000000000000..1387695636a41b4539a27287592240575784529a --- /dev/null +++ b/valid/labels/mig-good-welds_35_jpeg_jpg.rf.cd003ef912040fb387bc238928885861.txt @@ -0,0 +1 @@ +1 0.56171875 0.39921875 0.5515625 0.065625 diff --git a/valid/labels/overlap-welding-images_26_jpeg.rf.2ab860d40487f0e21dbd74cd2571a64b.txt b/valid/labels/overlap-welding-images_26_jpeg.rf.2ab860d40487f0e21dbd74cd2571a64b.txt new file mode 100644 index 0000000000000000000000000000000000000000..4a6b665a104e5eacd84f540c8163e4972cbe6e4c --- /dev/null +++ b/valid/labels/overlap-welding-images_26_jpeg.rf.2ab860d40487f0e21dbd74cd2571a64b.txt @@ -0,0 +1,8 @@ +0 0.5015625 0.46640625 0.9953125 0.0578125 +2 0.246875 0.4671875 0.03203125 0.02734375 +2 0.2984375 0.4640625 0.03828125 0.02265625 +2 0.33671875 0.465625 0.01875 0.01640625 +2 0.38046875 0.46484375 0.03125 0.0234375 +2 0.4359375 0.46484375 0.03125 0.01328125 +2 0.51015625 0.4640625 0.0234375 0.0171875 +2 0.2 0.4578125 0.01015625 0.0171875 diff --git a/valid/labels/overlap-welding-images_26_jpeg_jpg.rf.52dce3834bd8eae983c31c2141a20d3c.txt b/valid/labels/overlap-welding-images_26_jpeg_jpg.rf.52dce3834bd8eae983c31c2141a20d3c.txt new file mode 100644 index 0000000000000000000000000000000000000000..e60cc61be8259b311da4ec208dc505bd512ca3fb --- /dev/null +++ b/valid/labels/overlap-welding-images_26_jpeg_jpg.rf.52dce3834bd8eae983c31c2141a20d3c.txt @@ -0,0 +1,8 @@ +0 0.5015625 0.46640625 0.9953125 0.0578125 +2 0.246875 0.4671875 0.0328125 0.028125 +2 0.2984375 0.4640625 0.0390625 0.0234375 +2 0.33671875 0.465625 0.01875 0.0171875 +2 0.38046875 0.46484375 0.03125 0.0234375 +2 0.4359375 0.46484375 0.03125 0.0140625 +2 0.51015625 0.4640625 0.0234375 0.0171875 +2 0.2 0.4578125 0.009375 0.0171875 diff --git a/valid/labels/overlap-welding-images_8_jpeg.rf.496a0365bbdbeb1062d1127867afa159.txt b/valid/labels/overlap-welding-images_8_jpeg.rf.496a0365bbdbeb1062d1127867afa159.txt new file mode 100644 index 0000000000000000000000000000000000000000..67b87e8e655ec44c72768879a22684154320eace --- /dev/null +++ b/valid/labels/overlap-welding-images_8_jpeg.rf.496a0365bbdbeb1062d1127867afa159.txt @@ -0,0 +1 @@ +0 0.50078125 0.465625 0.996875 0.44375 diff --git a/valid/labels/poor-Welding-Images_10_jpeg.rf.76882ad1939df69e3059e065f8e8c377.txt b/valid/labels/poor-Welding-Images_10_jpeg.rf.76882ad1939df69e3059e065f8e8c377.txt new file mode 100644 index 0000000000000000000000000000000000000000..f04c980b31eb264179e166f797c18bde513d9b5c --- /dev/null +++ b/valid/labels/poor-Welding-Images_10_jpeg.rf.76882ad1939df69e3059e065f8e8c377.txt @@ -0,0 +1,3 @@ +0 0.55546875 0.54765625 0.875 0.7515625 +2 0.603125 0.45703125 0.0546875 0.05390625 +2 0.46640625 0.5609375 0.034375 0.05078125 diff --git a/valid/labels/poor-Welding-Images_20_jpeg_jpg.rf.9de9f53203c40abe734f99f1daf735d3.txt b/valid/labels/poor-Welding-Images_20_jpeg_jpg.rf.9de9f53203c40abe734f99f1daf735d3.txt new file mode 100644 index 0000000000000000000000000000000000000000..abc69efc37adfd55fe2a3d9b6d4c4e2dbbb4bf75 --- /dev/null +++ b/valid/labels/poor-Welding-Images_20_jpeg_jpg.rf.9de9f53203c40abe734f99f1daf735d3.txt @@ -0,0 +1 @@ +1 0.42578125 0.49609375 0.775 0.175 diff --git a/valid/labels/poor-Welding-Images_30_jpeg.rf.182688e8dbcf6740de764394e86eaf7b.txt b/valid/labels/poor-Welding-Images_30_jpeg.rf.182688e8dbcf6740de764394e86eaf7b.txt new file mode 100644 index 0000000000000000000000000000000000000000..e199eeae53e5c3b62b310dfea2b890148beb19fb --- /dev/null +++ b/valid/labels/poor-Welding-Images_30_jpeg.rf.182688e8dbcf6740de764394e86eaf7b.txt @@ -0,0 +1 @@ +2 0.44375 0.440625 0.1078125 0.10234375 diff --git a/valid/labels/poor-Welding-Images_30_jpeg_jpg.rf.9c41acc876f697dfbe12a27cd68536c9.txt b/valid/labels/poor-Welding-Images_30_jpeg_jpg.rf.9c41acc876f697dfbe12a27cd68536c9.txt new file mode 100644 index 0000000000000000000000000000000000000000..e7f9d304af5c20d46bc5315891eeb92e9f6d72cc --- /dev/null +++ b/valid/labels/poor-Welding-Images_30_jpeg_jpg.rf.9c41acc876f697dfbe12a27cd68536c9.txt @@ -0,0 +1 @@ +2 0.44375 0.440625 0.1078125 0.103125 diff --git a/valid/labels/poor-Welding-Images_43_jpeg.rf.30d7319782a1a3adb6083bf57a22c151.txt b/valid/labels/poor-Welding-Images_43_jpeg.rf.30d7319782a1a3adb6083bf57a22c151.txt new file mode 100644 index 0000000000000000000000000000000000000000..e03b87623aa580cbc2bc08ef2d9db75691242cf7 --- /dev/null +++ b/valid/labels/poor-Welding-Images_43_jpeg.rf.30d7319782a1a3adb6083bf57a22c151.txt @@ -0,0 +1,3 @@ +0 0.49921875 0.3921875 0.9984375 0.2796875 +2 0.42265625 0.46015625 0.121875 0.08984375 +2 0.8640625 0.46015625 0.0765625 0.075 diff --git a/valid/labels/poor-Welding-Images_52_jpeg_jpg.rf.a2c054b968740496a6930c40a9f8c947.txt b/valid/labels/poor-Welding-Images_52_jpeg_jpg.rf.a2c054b968740496a6930c40a9f8c947.txt new file mode 100644 index 0000000000000000000000000000000000000000..81b5e1a8377a078b744871737585b44794143e95 --- /dev/null +++ b/valid/labels/poor-Welding-Images_52_jpeg_jpg.rf.a2c054b968740496a6930c40a9f8c947.txt @@ -0,0 +1,3 @@ +0 0.440625 0.43515625 0.79375 0.8078125 +2 0.48671875 0.45859375 0.09375 0.078125 +2 0.38671875 0.49765625 0.0796875 0.078125 diff --git a/valid/labels/poor-Welding-Images_9_jpeg_jpg.rf.f950f91df976733e2291ff30bea45aa0.txt b/valid/labels/poor-Welding-Images_9_jpeg_jpg.rf.f950f91df976733e2291ff30bea45aa0.txt new file mode 100644 index 0000000000000000000000000000000000000000..26cbd5545a23703de1ede55b7e8a80159089011e --- /dev/null +++ b/valid/labels/poor-Welding-Images_9_jpeg_jpg.rf.f950f91df976733e2291ff30bea45aa0.txt @@ -0,0 +1,3 @@ +0 0.51640625 0.4171875 0.5671875 0.5609375 +2 0.328125 0.56796875 0.0515625 0.075 +2 0.43046875 0.5484375 0.13125 0.1609375 diff --git a/valid/labels/weld-defect-work-was-carried-out-using-semi-automatic-arc-welding-mig-welding-weld-defect-work-was-carried-out-using-semi-242006161_jpeg.rf.abf277a0e2de19ced505d1f57f0e6011.txt b/valid/labels/weld-defect-work-was-carried-out-using-semi-automatic-arc-welding-mig-welding-weld-defect-work-was-carried-out-using-semi-242006161_jpeg.rf.abf277a0e2de19ced505d1f57f0e6011.txt new file mode 100644 index 0000000000000000000000000000000000000000..7893504ff52bff1e15321aff80f013f49199ba87 --- /dev/null +++ b/valid/labels/weld-defect-work-was-carried-out-using-semi-automatic-arc-welding-mig-welding-weld-defect-work-was-carried-out-using-semi-242006161_jpeg.rf.abf277a0e2de19ced505d1f57f0e6011.txt @@ -0,0 +1,7 @@ +0 0.50234375 0.50390625 0.98515625 0.43359375 +2 0.62578125 0.4875 0.1140625 0.284375 +2 0.80390625 0.478125 0.125 0.23046875 +2 0.16484375 0.4671875 0.07265625 0.1296875 +2 0.55234375 0.54296875 0.06015625 0.090625 +2 0.93125 0.47578125 0.075 0.0734375 +2 0.7125 0.56484375 0.04765625 0.0609375 diff --git a/valid/labels/weld-defect-work-was-carried-out-using-semi-automatic-arc-welding-mig-welding-weld-defect-work-was-carried-out-using-semi-242007435_jpeg.rf.68bf8b6a1c26ca1a0cd2d06ee11d8eff.txt b/valid/labels/weld-defect-work-was-carried-out-using-semi-automatic-arc-welding-mig-welding-weld-defect-work-was-carried-out-using-semi-242007435_jpeg.rf.68bf8b6a1c26ca1a0cd2d06ee11d8eff.txt new file mode 100644 index 0000000000000000000000000000000000000000..ad3c2f9f825813325bc8d7be4af3cc7bdc40d1de --- /dev/null +++ b/valid/labels/weld-defect-work-was-carried-out-using-semi-automatic-arc-welding-mig-welding-weld-defect-work-was-carried-out-using-semi-242007435_jpeg.rf.68bf8b6a1c26ca1a0cd2d06ee11d8eff.txt @@ -0,0 +1,7 @@ +0 0.5 0.5078125 0.9984375 0.259375 +2 0.0953125 0.5078125 0.1390625 0.08828125 +2 0.40703125 0.49609375 0.13046875 0.04921875 +2 0.571875 0.4828125 0.11953125 0.06484375 +2 0.7171875 0.48671875 0.12421875 0.09453125 +2 0.84296875 0.4984375 0.04765625 0.08671875 +2 0.9421875 0.4859375 0.1140625 0.17109375