rikkarth commited on
Commit
9d14eb8
·
verified ·
1 Parent(s): 3316158

Add welding defect dataset: YOLO labels + COCO conversions

Browse files
This view is limited to 50 files because it contains too many changes.   See raw diff
Files changed (50) hide show
  1. .DS_Store +0 -0
  2. coco/test.json +1 -0
  3. coco/train.json +0 -0
  4. coco/valid.json +0 -0
  5. data.yaml +6 -0
  6. test/.DS_Store +0 -0
  7. test/images/02fd0af7-51ab46bb-c13_jpg.rf.7de08cd3b264d9098d09f5fe6d21c959.jpg +3 -0
  8. test/images/1aa4b44c-d01b8a11-Hot-crack_jpg.rf.57393ca7936f061ca5991481b2b5c485.jpg +3 -0
  9. test/images/295992d6-f617b725-c1_png_jpg.rf.5f645e13f1695df588b0644ca9702c43.jpg +3 -0
  10. test/images/4a05306b-ca866e1f-c12_jpg.rf.c5c926823394e6056b533bedd6e64c99.jpg +3 -0
  11. test/images/Good-Welding-images_11_jpeg.rf.4807e1282a383cba87b1e2e3c77ca9ce.jpg +3 -0
  12. test/images/Good-Welding-images_12_jpeg.rf.126bee697b91a6562ffb0e9701b2fe8c.jpg +3 -0
  13. test/images/Good-Welding-images_12_jpeg_jpg.rf.9fa5a26596733b74baf1f974b8210c28.jpg +3 -0
  14. test/images/Good-Welding-images_17_jpeg_jpg.rf.be58c70a9f7f542fc89cb48847776741.jpg +3 -0
  15. test/images/Good-Welding-images_23_jpeg_jpg.rf.fdf50352e3c124ff6edab3e96257a040.jpg +3 -0
  16. test/images/Good-Welding-images_28_png.rf.503eeed161b61cf8ec218b1c17440787.jpg +3 -0
  17. test/images/Good-Welding-images_30_jpeg.rf.4af312f6d3af2b9ec3a3c7814019f387.jpg +3 -0
  18. test/images/Good-Welding-images_33_jpeg.rf.0e3a517af5a8cc2a5ea0a02f5ed2fbab.jpg +3 -0
  19. test/images/Good-Welding-images_33_jpeg_jpg.rf.782ccc0dfca926b946a6b664dd4cacd1.jpg +3 -0
  20. test/images/SampleV1_1_mp4-1_jpg.rf.3f50c974a91c4e6348dd49491f06def8.jpg +3 -0
  21. test/images/SampleV1_1_mp4-42_jpg.rf.6e68d9186e630ffb996233ad2a593f51.jpg +3 -0
  22. test/images/SampleV1_2_mp4-14_jpg.rf.4dba7e8bd84314a155dd85df33b5f4d9.jpg +3 -0
  23. test/images/SampleV2_1_mp4-0_jpg.rf.32dc225d9b5d11d01260f75c918a9961.jpg +3 -0
  24. test/images/SampleV2_1_mp4-59_jpg.rf.b500f4a89177615c16be765f9f15b910.jpg +3 -0
  25. test/images/SampleV2_1_mp4-60_jpg.rf.40f4a4094130e65b1a801b49fefc5d01.jpg +3 -0
  26. test/images/SampleV2_1_mp4-90_jpg.rf.19ad4979865d6aba1cfaaa23f1dfb1f9.jpg +3 -0
  27. test/images/SampleV2_1_mp4-97_jpg.rf.1cbd06413c3d08495ffce915e0d8bd94.jpg +3 -0
  28. test/images/SampleV2_2_mp4-100_jpg.rf.95c9ff940b64d347919b6d49dfb8b0b3.jpg +3 -0
  29. test/images/SampleV2_2_mp4-24_jpg.rf.0909700c29763d6bbe0f3e7df949475b.jpg +3 -0
  30. test/images/SampleV2_2_mp4-39_jpg.rf.e18c2b9f47afa039f3f2fee002312552.jpg +3 -0
  31. test/images/SampleV2_2_mp4-57_jpg.rf.95a7afd6a5fef7ea6a6161a433182ce3.jpg +3 -0
  32. test/images/SampleV2_2_mp4-59_jpg.rf.5e6543b79b7abac05cf8005d24f61eb5.jpg +3 -0
  33. test/images/SampleV2_2_mp4-71_jpg.rf.de0eaa495c44a7817fab26c6c6277796.jpg +3 -0
  34. test/images/SampleV2_2_mp4-76_jpg.rf.492360f34b458a190c41d157fff3dbba.jpg +3 -0
  35. test/images/SampleV2_2_mp4-98_jpg.rf.83b6e5f3fa68582da8fe9db065a00a98.jpg +3 -0
  36. test/images/SampleV3_1_mp4-24_jpg.rf.017f90fdc7b6c9677febabbd168597fb.jpg +3 -0
  37. test/images/SampleV3_1_mp4-45_jpg.rf.a4085868c8ba207b4e9941d0af06c894.jpg +3 -0
  38. test/images/SampleV3_1_mp4-50_jpg.rf.5a367e6d492cd43c4a8627799b654370.jpg +3 -0
  39. test/images/SampleV3_1_mp4-8_jpg.rf.15adb36ac87bf5e5533ced60df5f5635.jpg +3 -0
  40. test/images/SampleV3_2_mp4-2_jpg.rf.f673f3917f7d15f03110e853f63696dc.jpg +3 -0
  41. test/images/Screenshot-2022-12-05-223424_jpeg.rf.3de790d465fbb0428d1066ab0ec33daf.jpg +3 -0
  42. test/images/Screenshot-2022-12-05-223445_jpeg.rf.a835025488cff5c8564c4d16df1b7ad6.jpg +3 -0
  43. test/images/Screenshot-2022-12-05-223445_jpeg_jpg.rf.e35a047d0ee08846662cb19b302fb1a7.jpg +3 -0
  44. test/images/Screenshot-2022-12-05-223504_jpeg.rf.f6c1d1d819ba7212516d5da2471bdb04.jpg +3 -0
  45. test/images/Screenshot-2022-12-05-223616_jpeg_jpg.rf.ed5db415112db98336eb0a6eabfe3fd0.jpg +3 -0
  46. test/images/Screenshot-2022-12-05-224056_jpeg.rf.0198544ad2d024d446a77d8f8c04ff12.jpg +3 -0
  47. test/images/Screenshot-2022-12-05-224335_jpeg_jpg.rf.bcfe0035e76676a1f9056aea47c18999.jpg +3 -0
  48. test/images/Screenshot-2022-12-05-230149_jpeg.rf.9a609cc50aed07d1532d574bdfddd081.jpg +3 -0
  49. test/images/Screenshot-2022-12-05-230257_jpeg_jpg.rf.b7d7eb8e010e48641638d6a878f9af61.jpg +3 -0
  50. test/images/Slag-inclusion-welding-images_11_jpeg.rf.06f53c90b96f942c575dad2d8ba10992.jpg +3 -0
.DS_Store ADDED
Binary file (8.2 kB). View file
 
coco/test.json ADDED
@@ -0,0 +1 @@
 
 
1
+ {"images": [{"id": 1, "file_name": "02fd0af7-51ab46bb-c13_jpg.rf.7de08cd3b264d9098d09f5fe6d21c959.jpg", "width": 640, "height": 640}, {"id": 2, "file_name": "1aa4b44c-d01b8a11-Hot-crack_jpg.rf.57393ca7936f061ca5991481b2b5c485.jpg", "width": 640, "height": 640}, {"id": 3, "file_name": "295992d6-f617b725-c1_png_jpg.rf.5f645e13f1695df588b0644ca9702c43.jpg", "width": 640, "height": 640}, {"id": 4, "file_name": "4a05306b-ca866e1f-c12_jpg.rf.c5c926823394e6056b533bedd6e64c99.jpg", "width": 640, "height": 640}, {"id": 5, "file_name": "Good-Welding-images_11_jpeg.rf.4807e1282a383cba87b1e2e3c77ca9ce.jpg", "width": 640, "height": 640}, {"id": 6, "file_name": "Good-Welding-images_12_jpeg.rf.126bee697b91a6562ffb0e9701b2fe8c.jpg", "width": 640, "height": 640}, {"id": 7, "file_name": "Good-Welding-images_12_jpeg_jpg.rf.9fa5a26596733b74baf1f974b8210c28.jpg", "width": 640, "height": 640}, {"id": 8, "file_name": "Good-Welding-images_17_jpeg_jpg.rf.be58c70a9f7f542fc89cb48847776741.jpg", "width": 640, "height": 640}, {"id": 9, "file_name": "Good-Welding-images_23_jpeg_jpg.rf.fdf50352e3c124ff6edab3e96257a040.jpg", "width": 640, "height": 640}, {"id": 10, "file_name": "Good-Welding-images_28_png.rf.503eeed161b61cf8ec218b1c17440787.jpg", "width": 640, "height": 640}, {"id": 11, "file_name": "Good-Welding-images_30_jpeg.rf.4af312f6d3af2b9ec3a3c7814019f387.jpg", "width": 640, "height": 640}, {"id": 12, "file_name": "Good-Welding-images_33_jpeg.rf.0e3a517af5a8cc2a5ea0a02f5ed2fbab.jpg", "width": 640, "height": 640}, {"id": 13, "file_name": "Good-Welding-images_33_jpeg_jpg.rf.782ccc0dfca926b946a6b664dd4cacd1.jpg", "width": 640, "height": 640}, {"id": 14, "file_name": "SampleV1_1_mp4-1_jpg.rf.3f50c974a91c4e6348dd49491f06def8.jpg", "width": 640, "height": 640}, {"id": 15, "file_name": "SampleV1_1_mp4-42_jpg.rf.6e68d9186e630ffb996233ad2a593f51.jpg", "width": 640, "height": 640}, {"id": 16, "file_name": "SampleV1_2_mp4-14_jpg.rf.4dba7e8bd84314a155dd85df33b5f4d9.jpg", "width": 640, "height": 640}, {"id": 17, "file_name": "SampleV2_1_mp4-0_jpg.rf.32dc225d9b5d11d01260f75c918a9961.jpg", "width": 640, "height": 640}, {"id": 18, "file_name": "SampleV2_1_mp4-59_jpg.rf.b500f4a89177615c16be765f9f15b910.jpg", "width": 640, "height": 640}, {"id": 19, "file_name": "SampleV2_1_mp4-60_jpg.rf.40f4a4094130e65b1a801b49fefc5d01.jpg", "width": 640, "height": 640}, {"id": 20, "file_name": "SampleV2_1_mp4-90_jpg.rf.19ad4979865d6aba1cfaaa23f1dfb1f9.jpg", "width": 640, "height": 640}, {"id": 21, "file_name": "SampleV2_1_mp4-97_jpg.rf.1cbd06413c3d08495ffce915e0d8bd94.jpg", "width": 640, "height": 640}, {"id": 22, "file_name": "SampleV2_2_mp4-100_jpg.rf.95c9ff940b64d347919b6d49dfb8b0b3.jpg", "width": 640, "height": 640}, {"id": 23, "file_name": "SampleV2_2_mp4-24_jpg.rf.0909700c29763d6bbe0f3e7df949475b.jpg", "width": 640, "height": 640}, {"id": 24, "file_name": "SampleV2_2_mp4-39_jpg.rf.e18c2b9f47afa039f3f2fee002312552.jpg", "width": 640, "height": 640}, {"id": 25, "file_name": "SampleV2_2_mp4-57_jpg.rf.95a7afd6a5fef7ea6a6161a433182ce3.jpg", "width": 640, "height": 640}, {"id": 26, "file_name": "SampleV2_2_mp4-59_jpg.rf.5e6543b79b7abac05cf8005d24f61eb5.jpg", "width": 640, "height": 640}, {"id": 27, "file_name": "SampleV2_2_mp4-71_jpg.rf.de0eaa495c44a7817fab26c6c6277796.jpg", "width": 640, "height": 640}, {"id": 28, "file_name": "SampleV2_2_mp4-76_jpg.rf.492360f34b458a190c41d157fff3dbba.jpg", "width": 640, "height": 640}, {"id": 29, "file_name": "SampleV2_2_mp4-98_jpg.rf.83b6e5f3fa68582da8fe9db065a00a98.jpg", "width": 640, "height": 640}, {"id": 30, "file_name": "SampleV3_1_mp4-24_jpg.rf.017f90fdc7b6c9677febabbd168597fb.jpg", "width": 640, "height": 640}, {"id": 31, "file_name": "SampleV3_1_mp4-45_jpg.rf.a4085868c8ba207b4e9941d0af06c894.jpg", "width": 640, "height": 640}, {"id": 32, "file_name": "SampleV3_1_mp4-50_jpg.rf.5a367e6d492cd43c4a8627799b654370.jpg", "width": 640, "height": 640}, {"id": 33, "file_name": "SampleV3_1_mp4-8_jpg.rf.15adb36ac87bf5e5533ced60df5f5635.jpg", "width": 640, "height": 640}, {"id": 34, "file_name": "SampleV3_2_mp4-2_jpg.rf.f673f3917f7d15f03110e853f63696dc.jpg", "width": 640, "height": 640}, {"id": 35, "file_name": "Screenshot-2022-12-05-223424_jpeg.rf.3de790d465fbb0428d1066ab0ec33daf.jpg", "width": 640, "height": 640}, {"id": 36, "file_name": "Screenshot-2022-12-05-223445_jpeg.rf.a835025488cff5c8564c4d16df1b7ad6.jpg", "width": 640, "height": 640}, {"id": 37, "file_name": "Screenshot-2022-12-05-223445_jpeg_jpg.rf.e35a047d0ee08846662cb19b302fb1a7.jpg", "width": 640, "height": 640}, {"id": 38, "file_name": "Screenshot-2022-12-05-223504_jpeg.rf.f6c1d1d819ba7212516d5da2471bdb04.jpg", "width": 640, "height": 640}, {"id": 39, "file_name": "Screenshot-2022-12-05-223616_jpeg_jpg.rf.ed5db415112db98336eb0a6eabfe3fd0.jpg", "width": 640, "height": 640}, {"id": 40, "file_name": "Screenshot-2022-12-05-224056_jpeg.rf.0198544ad2d024d446a77d8f8c04ff12.jpg", "width": 640, "height": 640}, {"id": 41, "file_name": "Screenshot-2022-12-05-224335_jpeg_jpg.rf.bcfe0035e76676a1f9056aea47c18999.jpg", "width": 640, "height": 640}, {"id": 42, "file_name": "Screenshot-2022-12-05-230149_jpeg.rf.9a609cc50aed07d1532d574bdfddd081.jpg", "width": 640, "height": 640}, {"id": 43, "file_name": "Screenshot-2022-12-05-230257_jpeg_jpg.rf.b7d7eb8e010e48641638d6a878f9af61.jpg", "width": 640, "height": 640}, {"id": 44, "file_name": "Slag-inclusion-welding-images_11_jpeg.rf.06f53c90b96f942c575dad2d8ba10992.jpg", "width": 640, "height": 640}, {"id": 45, "file_name": "Slag-inclusion-welding-images_5_jpeg_jpg.rf.0e134d6e310d401ae657279a12daa898.jpg", "width": 640, "height": 640}, {"id": 46, "file_name": "Spatters-welding-images_20_jpeg.rf.a22cf567f9f4a000618175f38dc1b1ee.jpg", "width": 640, "height": 640}, {"id": 47, "file_name": "Spatters-welding-images_30_jpeg_jpg.rf.ac1f61755f14395f6e5da156c7fd043f.jpg", "width": 640, "height": 640}, {"id": 48, "file_name": "Spatters-welding-images_6_jpeg.rf.867f4257d076b9301eb62946e06c60d7.jpg", "width": 640, "height": 640}, {"id": 49, "file_name": "Spatters-welding-images_9_jpeg_jpg.rf.a43f10bbaf404937f530d9c278654acb.jpg", "width": 640, "height": 640}, {"id": 50, "file_name": "bad_weld_vid166_jpeg_jpg.rf.525052424b574a43de777660f6cb2d10.jpg", "width": 640, "height": 640}, {"id": 51, "file_name": "bad_weld_vid177_jpeg.rf.5bf77a9a97b327dc04a8575ba9375aea.jpg", "width": 640, "height": 640}, {"id": 52, "file_name": "bad_weld_vid181_jpeg.rf.e76607a4dd9ac855668e049bdc68515d.jpg", "width": 640, "height": 640}, {"id": 53, "file_name": "bad_weld_vid199_jpeg.rf.2b6c1dc8c0858d47d0cf1eaf41d55663.jpg", "width": 640, "height": 640}, {"id": 54, "file_name": "bad_weld_vid205_jpeg.rf.4732128c8ac74427330c636ff0e63949.jpg", "width": 640, "height": 640}, {"id": 55, "file_name": "bad_weld_vid233_jpeg.rf.3306ed2878bce5f9d840c8701faced72.jpg", "width": 640, "height": 640}, {"id": 56, "file_name": "bad_weld_vid233_jpeg_jpg.rf.17d61563d86c4d1fc157c29f5a109d98.jpg", "width": 640, "height": 640}, {"id": 57, "file_name": "bad_weld_vid261_jpeg_jpg.rf.5ae3866fd5de7b144659fa7f7b92c5ba.jpg", "width": 640, "height": 640}, {"id": 58, "file_name": "bad_weld_vid277_jpeg_jpg.rf.0e6aafa2605c842edfaedaba06ded02c.jpg", "width": 640, "height": 640}, {"id": 59, "file_name": "bad_weld_vid278_jpeg_jpg.rf.d7b37caf0f75a2942cae27dedf5c4c64.jpg", "width": 640, "height": 640}, {"id": 60, "file_name": "bad_weld_vid280_jpeg.rf.84ae852be0cfdf652d6c54a8ea04b4f9.jpg", "width": 640, "height": 640}, {"id": 61, "file_name": "bad_weld_vid368_jpeg.rf.513a43066292f2b16b8428284df2b472.jpg", "width": 640, "height": 640}, {"id": 62, "file_name": "bad_weld_vid374_jpeg.rf.b0028e044a8253fcd89bc91e0ebfbd88.jpg", "width": 640, "height": 640}, {"id": 63, "file_name": "bad_weld_vid374_jpeg_jpg.rf.d1c904ca6a097b2c51665238ba9e1147.jpg", "width": 640, "height": 640}, {"id": 64, "file_name": "bad_weld_vid397_jpeg_jpg.rf.6aacbe170c5956e56b1024f24d60c60c.jpg", "width": 640, "height": 640}, {"id": 65, "file_name": "bad_weld_vid446_jpeg.rf.a6dec617f873aa1a4f95bf3aa26dff05.jpg", "width": 640, "height": 640}, {"id": 66, "file_name": "bad_weld_vid643_jpeg_jpg.rf.4198326c850625e57e8851f1da196032.jpg", "width": 640, "height": 640}, {"id": 67, "file_name": "bad_weld_vid686_jpeg.rf.aa5cd8e60bd0b308a51315cfd9d08c87.jpg", "width": 640, "height": 640}, {"id": 68, "file_name": "bad_weld_vid690_jpeg.rf.7deeeeb79064c7ad5761a04e2dbb40ae.jpg", "width": 640, "height": 640}, {"id": 69, "file_name": "bad_weld_vid691_jpeg.rf.bd03731534b9f7f5ae4eb395426f44c7.jpg", "width": 640, "height": 640}, {"id": 70, "file_name": "bad_weld_vid84_jpeg_jpg.rf.f148c4898a835b73a3eb087d905ed8f3.jpg", "width": 640, "height": 640}, {"id": 71, "file_name": "bad_weld_vid88_jpeg.rf.dbf17e5df452b1a7910a87f6442f0341.jpg", "width": 640, "height": 640}, {"id": 72, "file_name": "bad_weld_vid89_jpeg_jpg.rf.cdeeae57ff588da1b969bfd75c2a7747.jpg", "width": 640, "height": 640}, {"id": 73, "file_name": "bad_weld_vid92_jpeg.rf.a3a1a6b5570c15b43fe91e402bb3e4d4.jpg", "width": 640, "height": 640}, {"id": 74, "file_name": "carbon-steel-good-welds_28_png_jpg.rf.0d13b8fd981d7a68d163528d61a2e534.jpg", "width": 640, "height": 640}, {"id": 75, "file_name": "carbon-steel-good-welds_4_jpeg.rf.b6f85c08c46fa9d199f916958e5b957f.jpg", "width": 640, "height": 640}, {"id": 76, "file_name": "crack-welding-images_11_jpeg_jpg.rf.5174724ff08d893dc926840b5d3a3e22.jpg", "width": 640, "height": 640}, {"id": 77, "file_name": "crack-welding-images_17_jpeg_jpg.rf.ff570716da313da84983bc629ae7e331.jpg", "width": 640, "height": 640}, {"id": 78, "file_name": "crack-welding-images_25_jpeg.rf.af2b8cc0f3616d045ea7e539504dca28.jpg", "width": 640, "height": 640}, {"id": 79, "file_name": "good-stick-welds_19_png_jpg.rf.dc807e5b52e58b41c2c3c1dd6b833ec8.jpg", "width": 640, "height": 640}, {"id": 80, "file_name": "good-stick-welds_21_jpeg.rf.efbb03ebea526cb3b14ebf8607957933.jpg", "width": 640, "height": 640}, {"id": 81, "file_name": "good-stick-welds_36_jpeg.rf.f82337b4f1f0b3b21e15819eb6298549.jpg", "width": 640, "height": 640}, {"id": 82, "file_name": "good-stick-welds_38_jpeg_jpg.rf.a798a6f14879da205dac297a653d167f.jpg", "width": 640, "height": 640}, {"id": 83, "file_name": "good-tig-welds_17_jpeg.rf.f09940f732257aefe3d81fe09ce55cb2.jpg", "width": 640, "height": 640}, {"id": 84, "file_name": "good-tig-welds_23_jpeg_jpg.rf.1513147f7df61d6a13bedd62c03c846e.jpg", "width": 640, "height": 640}, {"id": 85, "file_name": "good-tig-welds_29_jpeg.rf.c55465f1ddf62560e7d04de0dc4df63e.jpg", "width": 640, "height": 640}, {"id": 86, "file_name": "good-tig-welds_32_png_jpg.rf.31e47557dc8768f6a9dd99627ca3a6e7.jpg", "width": 640, "height": 640}, {"id": 87, "file_name": "good-tig-welds_35_jpeg.rf.7b1a37d7c715bf0f82d25b51bc90afa9.jpg", "width": 640, "height": 640}, {"id": 88, "file_name": "good-tig-welds_3_jpeg.rf.c6afd4c75c9f0f8866e1d58bb2a2ae0d.jpg", "width": 640, "height": 640}, {"id": 89, "file_name": "good-tig-welds_49_jpeg.rf.0a42f6bb041a139dc54f82c007c91b66.jpg", "width": 640, "height": 640}, {"id": 90, "file_name": "good-tig-welds_4_jpeg_jpg.rf.3e3a5bbd002257f6e3845eaecef98355.jpg", "width": 640, "height": 640}, {"id": 91, "file_name": "good_weld_vid100_jpeg.rf.8119452a868f43e546f35a5c98975194.jpg", "width": 640, "height": 640}, {"id": 92, "file_name": "good_weld_vid104_jpeg_jpg.rf.892dcfa6c4ff7737002a45507ebace2b.jpg", "width": 640, "height": 640}, {"id": 93, "file_name": "good_weld_vid1090_jpeg_jpg.rf.7699ffefea4a937a0b9620b4ad77b6d2.jpg", "width": 640, "height": 640}, {"id": 94, "file_name": "good_weld_vid1098_jpeg.rf.fa02bd1ec37898d82bf990525548da93.jpg", "width": 640, "height": 640}, {"id": 95, "file_name": "good_weld_vid1098_jpeg_jpg.rf.9237cce5d77a8a1c3a6dda6c976ca7d5.jpg", "width": 640, "height": 640}, {"id": 96, "file_name": "good_weld_vid1134_jpeg_jpg.rf.5531f5eb2fc03e6b2b992469c012caa4.jpg", "width": 640, "height": 640}, {"id": 97, "file_name": "good_weld_vid1199_jpeg.rf.9d57a01453bae20900fa6b90909f299b.jpg", "width": 640, "height": 640}, {"id": 98, "file_name": "good_weld_vid1266_jpeg.rf.cb9d92f6b9be101524092b92229f3df9.jpg", "width": 640, "height": 640}, {"id": 99, "file_name": "good_weld_vid1524_jpeg_jpg.rf.923ca28d540ddd883e105a445dfff8a3.jpg", "width": 640, "height": 640}, {"id": 100, "file_name": "good_weld_vid1762_jpeg.rf.92508865967a0204f5b78457d8131ac6.jpg", "width": 640, "height": 640}, {"id": 101, "file_name": "good_weld_vid1778_jpeg_jpg.rf.d35cb0ff2061fb1318822c88996de9e0.jpg", "width": 640, "height": 640}, {"id": 102, "file_name": "good_weld_vid189_jpeg_jpg.rf.33380af68fa3c4f459a81f26d1bdbcb9.jpg", "width": 640, "height": 640}, {"id": 103, "file_name": "good_weld_vid2024_jpeg.rf.a402255ca379799ef7f83f76286bb761.jpg", "width": 640, "height": 640}, {"id": 104, "file_name": "good_weld_vid2265_jpeg_jpg.rf.8a70ab5ca12dc7c63f19d1dadeaddaa5.jpg", "width": 640, "height": 640}, {"id": 105, "file_name": "good_weld_vid2273_jpeg.rf.6be078d0df7495799a432b5fb6674e2f.jpg", "width": 640, "height": 640}, {"id": 106, "file_name": "good_weld_vid274_jpeg.rf.b6f11d0f012275ef3823e747c05bb460.jpg", "width": 640, "height": 640}, {"id": 107, "file_name": "good_weld_vid414_jpeg_jpg.rf.39639646ba20dd336dd4f880cafd2f7a.jpg", "width": 640, "height": 640}, {"id": 108, "file_name": "good_weld_vid469_jpeg.rf.bb8d4104e49f8bd79aef34b7ed48b49f.jpg", "width": 640, "height": 640}, {"id": 109, "file_name": "good_weld_vid505_jpeg_jpg.rf.45b33c7999793e28cfd56029c6f5d0fd.jpg", "width": 640, "height": 640}, {"id": 110, "file_name": "good_weld_vid529_jpeg_jpg.rf.4dc697dcd18f7c7de001311bb1f845e6.jpg", "width": 640, "height": 640}, {"id": 111, "file_name": "good_weld_vid570_jpeg_jpg.rf.15e7a658b6f4bf340960ea1a205a1cdc.jpg", "width": 640, "height": 640}, {"id": 112, "file_name": "good_weld_vid571_jpeg.rf.538c3e8d94cd30d4bfa03e6af6be320c.jpg", "width": 640, "height": 640}, {"id": 113, "file_name": "good_weld_vid634_jpeg_jpg.rf.9b7bc6b6e69b54eb707c9bab8857b7a1.jpg", "width": 640, "height": 640}, {"id": 114, "file_name": "good_weld_vid780_jpeg.rf.f7e0a7a13d7a9d95291d104a36e20c4c.jpg", "width": 640, "height": 640}, {"id": 115, "file_name": "good_weld_vid863_jpeg_jpg.rf.9e85aba7b2a24a1cd973afa34c9278c0.jpg", "width": 640, "height": 640}, {"id": 116, "file_name": "good_weld_vid864_jpeg.rf.4d2653d4914fd46123c732cd0bf3cfb5.jpg", "width": 640, "height": 640}, {"id": 117, "file_name": "good_weld_vid95_jpeg_jpg.rf.fb5e83f9ec7edfd902f8d1e715fcb83a.jpg", "width": 640, "height": 640}, {"id": 118, "file_name": "imagerty4ys_jpeg_jpg.rf.63bb94db9a6bb65e4f87abe7f1eae488.jpg", "width": 640, "height": 640}, {"id": 119, "file_name": "istockphoto-1141599875-612x612_jpeg.rf.4e91c0a0fd5238a855a277f1d3bf0c0f.jpg", "width": 640, "height": 640}, {"id": 120, "file_name": "mig-good-welds_11_jpeg_jpg.rf.c488ebd180387fc1f20114bed459fbb5.jpg", "width": 640, "height": 640}, {"id": 121, "file_name": "mig-good-welds_5_jpeg.rf.34d691732b9aaf7d94f3fcdaa144fdba.jpg", "width": 640, "height": 640}, {"id": 122, "file_name": "poor-Welding-Images_22_jpeg_jpg.rf.3706f7e9a367ae053abfee4902a78288.jpg", "width": 640, "height": 640}, {"id": 123, "file_name": "poor-Welding-Images_52_jpeg.rf.c581b9cc8ce08cae3120e82b201d0efb.jpg", "width": 640, "height": 640}, {"id": 124, "file_name": "poor-Welding-Images_8_jpeg_jpg.rf.b9316d294ddc2466e9565069260103d0.jpg", "width": 640, "height": 640}, {"id": 125, "file_name": "porosity-worm-hole-weld-defect-welding-process-flux-cored-arc-fcaw-204492534_jpeg_jpg.rf.c5201d1c888e3ffa1fded39930503d32.jpg", "width": 640, "height": 640}, {"id": 126, "file_name": "process-welding-work-slag-industry-steel-old-rusty-metal-texture-background-252108058_jpeg.rf.42f552e558e17b6d79a8777af04dbae6.jpg", "width": 640, "height": 640}], "annotations": [{"id": 1, "image_id": 1, "category_id": 3, "bbox": [115.5, 118.25, 80.0, 158.5], "area": 12680.0, "iscrowd": 0}, {"id": 2, "image_id": 1, "category_id": 3, "bbox": [201.25, 239.50000000000003, 112.5, 42.99999999999997], "area": 4837.499999999996, "iscrowd": 0}, {"id": 3, "image_id": 2, "category_id": 3, "bbox": [92.25000000000001, 391.5, 547.5, 102.99999999999994], "area": 56392.49999999997, "iscrowd": 0}, {"id": 4, "image_id": 3, "category_id": 3, "bbox": [154.5, 294.0, 171.0, 54.00000000000006], "area": 9234.00000000001, "iscrowd": 0}, {"id": 5, "image_id": 4, "category_id": 3, "bbox": [2.250000000000014, 255.5, 635.5, 31.0], "area": 19700.5, "iscrowd": 0}, {"id": 6, "image_id": 5, "category_id": 2, "bbox": [39.49999999999999, 294.25, 363.99999999999994, 172.5], "area": 62789.99999999999, "iscrowd": 0}, {"id": 7, "image_id": 5, "category_id": 2, "bbox": [408.75, 206.75, 230.5, 112.5], "area": 25931.25, "iscrowd": 0}, {"id": 8, "image_id": 6, "category_id": 2, "bbox": [143.5, 225.49999999999997, 482.0, 255.00000000000003], "area": 122910.00000000001, "iscrowd": 0}, {"id": 9, "image_id": 7, "category_id": 2, "bbox": [143.5, 225.49999999999997, 482.0, 255.00000000000003], "area": 122910.00000000001, "iscrowd": 0}, {"id": 10, "image_id": 8, "category_id": 1, "bbox": [41.99999999999999, 151.50000000000003, 233.0, 359.0], "area": 83647.0, "iscrowd": 0}, {"id": 11, "image_id": 8, "category_id": 2, "bbox": [384.5, 185.99999999999997, 210.0, 301.0], "area": 63210.0, "iscrowd": 0}, {"id": 12, "image_id": 9, "category_id": 2, "bbox": [306.5, 378.5, 216.0, 137.0], "area": 29592.0, "iscrowd": 0}, {"id": 13, "image_id": 10, "category_id": 2, "bbox": [119.74999999999997, 346.50000000000006, 143.50000000000003, 85.99999999999994], "area": 12340.999999999995, "iscrowd": 0}, {"id": 14, "image_id": 10, "category_id": 2, "bbox": [408.75, 354.25, 115.5, 81.5], "area": 9413.25, "iscrowd": 0}, {"id": 15, "image_id": 11, "category_id": 2, "bbox": [410.50000000000006, 423.5, 122.99999999999994, 47.00000000000006], "area": 5781.000000000005, "iscrowd": 0}, {"id": 16, "image_id": 12, "category_id": 2, "bbox": [2.0000000000000284, 251.25, 628.0, 101.5], "area": 63742.0, "iscrowd": 0}, {"id": 17, "image_id": 13, "category_id": 2, "bbox": [2.0000000000000284, 251.0, 628.0, 102.0], "area": 64056.0, "iscrowd": 0}, {"id": 18, "image_id": 14, "category_id": 3, "bbox": [58.75, 64.25, 42.5, 16.5], "area": 701.25, "iscrowd": 0}, {"id": 19, "image_id": 14, "category_id": 3, "bbox": [58.75, 151.0, 42.5, 24.0], "area": 1020.0, "iscrowd": 0}, {"id": 20, "image_id": 14, "category_id": 3, "bbox": [251.50000000000003, 66.75, 23.99999999999997, 126.5], "area": 3035.9999999999964, "iscrowd": 0}, {"id": 21, "image_id": 14, "category_id": 3, "bbox": [589.5, 72.75, 39.0, 72.5], "area": 2827.5, "iscrowd": 0}, {"id": 22, "image_id": 14, "category_id": 3, "bbox": [574.0, 383.0, 56.0, 117.0], "area": 6552.0, "iscrowd": 0}, {"id": 23, "image_id": 14, "category_id": 3, "bbox": [430.0, 425.75, 49.00000000000006, 27.5], "area": 1347.5000000000016, "iscrowd": 0}, {"id": 24, "image_id": 14, "category_id": 3, "bbox": [263.5, 425.74999999999994, 57.0, 19.500000000000057], "area": 1111.5000000000032, "iscrowd": 0}, {"id": 25, "image_id": 14, "category_id": 1, "bbox": [62.75, 60.0, 33.5, 128.0], "area": 4288.0, "iscrowd": 0}, {"id": 26, "image_id": 14, "category_id": 1, "bbox": [256.0, 67.25, 18.0, 123.5], "area": 2223.0, "iscrowd": 0}, {"id": 27, "image_id": 14, "category_id": 2, "bbox": [436.50000000000006, 71.5, 20.999999999999943, 124.0], "area": 2603.9999999999927, "iscrowd": 0}, {"id": 28, "image_id": 14, "category_id": 1, "bbox": [595.0, 74.25, 28.0, 122.5], "area": 3430.0, "iscrowd": 0}, {"id": 29, "image_id": 14, "category_id": 2, "bbox": [49.25, 227.5, 32.5, 120.0], "area": 3900.0, "iscrowd": 0}, {"id": 30, "image_id": 14, "category_id": 2, "bbox": [256.75, 230.5, 21.5, 120.0], "area": 2580.0, "iscrowd": 0}, {"id": 31, "image_id": 14, "category_id": 2, "bbox": [442.5, 232.24999999999997, 24.000000000000057, 118.49999999999997], "area": 2844.000000000006, "iscrowd": 0}, {"id": 32, "image_id": 14, "category_id": 2, "bbox": [597.75, 231.5, 21.5, 117.0], "area": 2515.5, "iscrowd": 0}, {"id": 33, "image_id": 14, "category_id": 2, "bbox": [67.50000000000001, 385.5, 46.0, 115.0], "area": 5290.0, "iscrowd": 0}, {"id": 34, "image_id": 14, "category_id": 1, "bbox": [271.5, 382.5, 20.0, 115.0], "area": 2300.0, "iscrowd": 0}, {"id": 35, "image_id": 14, "category_id": 1, "bbox": [437.0, 380.75, 23.0, 113.5], "area": 2610.5, "iscrowd": 0}, {"id": 36, "image_id": 14, "category_id": 1, "bbox": [578.25, 384.25000000000006, 45.5, 113.49999999999994], "area": 5164.249999999997, "iscrowd": 0}, {"id": 37, "image_id": 15, "category_id": 3, "bbox": [304.25, 133.25, 116.5, 22.5], "area": 2621.25, "iscrowd": 0}, {"id": 38, "image_id": 15, "category_id": 3, "bbox": [405.0, 189.74999999999997, 59.00000000000006, 23.50000000000003], "area": 1386.500000000003, "iscrowd": 0}, {"id": 39, "image_id": 15, "category_id": 3, "bbox": [300.0, 356.99999999999994, 278.0, 24.000000000000057], "area": 6672.0000000000155, "iscrowd": 0}, {"id": 40, "image_id": 15, "category_id": 1, "bbox": [283.25, 152.75, 356.5, 32.5], "area": 11586.25, "iscrowd": 0}, {"id": 41, "image_id": 15, "category_id": 2, "bbox": [0.25000000000000355, 171.75, 117.5, 26.5], "area": 3113.75, "iscrowd": 0}, {"id": 42, "image_id": 15, "category_id": 1, "bbox": [294.0, 375.25, 346.0, 41.50000000000006], "area": 14359.00000000002, "iscrowd": 0}, {"id": 43, "image_id": 15, "category_id": 2, "bbox": [0.0, 407.0, 126.0, 30.0], "area": 3780.0, "iscrowd": 0}, {"id": 44, "image_id": 16, "category_id": 3, "bbox": [333.00000000000006, 0.0, 65.99999999999994, 53.0], "area": 3497.999999999997, "iscrowd": 0}, {"id": 45, "image_id": 16, "category_id": 3, "bbox": [266.0, 405.50000000000006, 80.99999999999994, 40.99999999999994], "area": 3320.999999999993, "iscrowd": 0}, {"id": 46, "image_id": 16, "category_id": 1, "bbox": [276.0, 0.0, 87.0, 232.0], "area": 20184.0, "iscrowd": 0}, {"id": 47, "image_id": 16, "category_id": 1, "bbox": [323.5, 338.25, 78.0, 301.5], "area": 23517.0, "iscrowd": 0}, {"id": 48, "image_id": 17, "category_id": 3, "bbox": [215.75, 43.0, 28.5, 39.0], "area": 1111.5, "iscrowd": 0}, {"id": 49, "image_id": 17, "category_id": 3, "bbox": [97.5, 303.25, 26.000000000000014, 35.5], "area": 923.0000000000005, "iscrowd": 0}, {"id": 50, "image_id": 17, "category_id": 3, "bbox": [329.75, 164.24999999999997, 27.5, 29.50000000000003], "area": 811.2500000000008, "iscrowd": 0}, {"id": 51, "image_id": 17, "category_id": 3, "bbox": [440.75, 296.75, 100.5, 28.5], "area": 2864.25, "iscrowd": 0}, {"id": 52, "image_id": 17, "category_id": 3, "bbox": [536.0, 496.5, 33.0, 78.0], "area": 2574.0, "iscrowd": 0}, {"id": 53, "image_id": 17, "category_id": 1, "bbox": [166.5, 45.5, 77.0, 19.0], "area": 1463.0, "iscrowd": 0}, {"id": 54, "image_id": 17, "category_id": 2, "bbox": [142.0, 168.0, 83.0, 15.0], "area": 1245.0, "iscrowd": 0}, {"id": 55, "image_id": 17, "category_id": 1, "bbox": [121.0, 311.25, 68.0, 20.5], "area": 1394.0, "iscrowd": 0}, {"id": 56, "image_id": 17, "category_id": 2, "bbox": [54.75, 499.0, 110.5, 32.0], "area": 3536.0, "iscrowd": 0}, {"id": 57, "image_id": 17, "category_id": 2, "bbox": [241.5, 513.0, 112.0, 28.0], "area": 3136.0, "iscrowd": 0}, {"id": 58, "image_id": 17, "category_id": 2, "bbox": [277.5, 308.5, 80.0, 24.0], "area": 1920.0, "iscrowd": 0}, {"id": 59, "image_id": 17, "category_id": 1, "bbox": [278.5, 170.75000000000003, 85.0, 15.499999999999972], "area": 1317.4999999999975, "iscrowd": 0}, {"id": 60, "image_id": 17, "category_id": 2, "bbox": [285.75, 58.50000000000001, 77.5, 16.999999999999993], "area": 1317.4999999999995, "iscrowd": 0}, {"id": 61, "image_id": 17, "category_id": 2, "bbox": [429.25, 50.0, 82.5, 23.0], "area": 1897.5, "iscrowd": 0}, {"id": 62, "image_id": 17, "category_id": 2, "bbox": [428.75, 168.0, 94.5, 20.0], "area": 1890.0, "iscrowd": 0}, {"id": 63, "image_id": 17, "category_id": 2, "bbox": [444.25000000000006, 518.5, 83.49999999999994, 18.0], "area": 1502.999999999999, "iscrowd": 0}, {"id": 64, "image_id": 18, "category_id": 3, "bbox": [263.25, 98.99999999999999, 72.5, 161.0], "area": 11672.5, "iscrowd": 0}, {"id": 65, "image_id": 18, "category_id": 1, "bbox": [272.0, 40.50000000000001, 25.0, 495.0], "area": 12375.0, "iscrowd": 0}, {"id": 66, "image_id": 18, "category_id": 2, "bbox": [83.0, 117.5, 24.0, 333.0], "area": 7992.0, "iscrowd": 0}, {"id": 67, "image_id": 18, "category_id": 2, "bbox": [473.00000000000006, 10.999999999999979, 15.999999999999943, 621.0], "area": 9935.999999999965, "iscrowd": 0}, {"id": 68, "image_id": 19, "category_id": 3, "bbox": [193.75, 115.5, 70.5, 156.0], "area": 10998.0, "iscrowd": 0}, {"id": 69, "image_id": 19, "category_id": 3, "bbox": [457.24999999999994, 0.0, 56.50000000000006, 174.0], "area": 9831.00000000001, "iscrowd": 0}, {"id": 70, "image_id": 19, "category_id": 1, "bbox": [464.5, 2.0000000000000284, 40.0, 638.0], "area": 25520.0, "iscrowd": 0}, {"id": 71, "image_id": 19, "category_id": 1, "bbox": [201.74999999999997, 85.25000000000003, 24.50000000000003, 425.5], "area": 10424.750000000013, "iscrowd": 0}, {"id": 72, "image_id": 19, "category_id": 2, "bbox": [52.5, 145.25, 24.0, 290.5], "area": 6972.0, "iscrowd": 0}, {"id": 73, "image_id": 20, "category_id": 3, "bbox": [176.75, 195.5, 56.5, 141.0], "area": 7966.5, "iscrowd": 0}, {"id": 74, "image_id": 20, "category_id": 3, "bbox": [46.25, 334.0, 29.5, 69.00000000000006], "area": 2035.5000000000016, "iscrowd": 0}, {"id": 75, "image_id": 20, "category_id": 3, "bbox": [45.50000000000001, 113.74999999999999, 41.99999999999999, 100.49999999999999], "area": 4220.999999999999, "iscrowd": 0}, {"id": 76, "image_id": 20, "category_id": 2, "bbox": [468.00000000000006, 21.74999999999997, 32.99999999999994, 614.5], "area": 20278.499999999964, "iscrowd": 0}, {"id": 77, "image_id": 20, "category_id": 1, "bbox": [192.24999999999997, 27.749999999999986, 28.50000000000003, 449.5], "area": 12810.750000000013, "iscrowd": 0}, {"id": 78, "image_id": 20, "category_id": 1, "bbox": [50.75, 110.75, 27.5, 344.50000000000006], "area": 9473.750000000002, "iscrowd": 0}, {"id": 79, "image_id": 21, "category_id": 3, "bbox": [268.5, 27.749999999999986, 70.0, 437.5], "area": 30625.0, "iscrowd": 0}, {"id": 80, "image_id": 21, "category_id": 3, "bbox": [101.74999999999999, 51.25, 30.500000000000014, 369.5], "area": 11269.750000000005, "iscrowd": 0}, {"id": 81, "image_id": 21, "category_id": 3, "bbox": [3.75, 75.25, 20.5, 289.5], "area": 5934.75, "iscrowd": 0}, {"id": 82, "image_id": 21, "category_id": 1, "bbox": [274.0, 13.999999999999986, 58.0, 462.0], "area": 26796.0, "iscrowd": 0}, {"id": 83, "image_id": 21, "category_id": 1, "bbox": [103.99999999999999, 34.49999999999999, 31.000000000000014, 392.00000000000006], "area": 12152.000000000007, "iscrowd": 0}, {"id": 84, "image_id": 21, "category_id": 1, "bbox": [0.0, 65.5, 33.0, 305.0], "area": 10065.0, "iscrowd": 0}, {"id": 85, "image_id": 22, "category_id": 3, "bbox": [490.0, 45.249999999999986, 32.0, 538.5], "area": 17232.0, "iscrowd": 0}, {"id": 86, "image_id": 22, "category_id": 3, "bbox": [141.75, 183.75000000000003, 18.5, 276.5], "area": 5115.25, "iscrowd": 0}, {"id": 87, "image_id": 22, "category_id": 1, "bbox": [491.25, 26.50000000000002, 40.5, 559.0], "area": 22639.5, "iscrowd": 0}, {"id": 88, "image_id": 22, "category_id": 2, "bbox": [276.5, 112.5, 36.0, 393.0], "area": 14148.0, "iscrowd": 0}, {"id": 89, "image_id": 22, "category_id": 1, "bbox": [135.75, 166.99999999999994, 24.50000000000003, 307.00000000000006], "area": 7521.50000000001, "iscrowd": 0}, {"id": 90, "image_id": 23, "category_id": 3, "bbox": [374.5, 290.50000000000006, 50.0, 77.99999999999994], "area": 3899.9999999999973, "iscrowd": 0}, {"id": 91, "image_id": 23, "category_id": 3, "bbox": [304.99999999999994, 296.5, 46.0, 64.00000000000006], "area": 2944.0000000000027, "iscrowd": 0}, {"id": 92, "image_id": 23, "category_id": 3, "bbox": [0.0, 341.99999999999994, 56.0, 57.00000000000006], "area": 3192.000000000003, "iscrowd": 0}, {"id": 93, "image_id": 23, "category_id": 3, "bbox": [262.0, 78.75000000000001, 163.0, 43.5], "area": 7090.5, "iscrowd": 0}, {"id": 94, "image_id": 23, "category_id": 1, "bbox": [227.00000000000003, 305.25, 242.99999999999997, 53.5], "area": 13000.499999999998, "iscrowd": 0}, {"id": 95, "image_id": 23, "category_id": 2, "bbox": [0.0, 96.74999999999999, 123.0, 55.500000000000014], "area": 6826.500000000002, "iscrowd": 0}, {"id": 96, "image_id": 23, "category_id": 1, "bbox": [258.5, 74.25, 178.0, 51.5], "area": 9167.0, "iscrowd": 0}, {"id": 97, "image_id": 24, "category_id": 3, "bbox": [420.25, 220.5, 49.5, 69.0], "area": 3415.5, "iscrowd": 0}, {"id": 98, "image_id": 24, "category_id": 1, "bbox": [207.75, 233.25, 260.49999999999994, 51.5], "area": 13415.749999999996, "iscrowd": 0}, {"id": 99, "image_id": 24, "category_id": 2, "bbox": [224.5, 23.75, 185.0, 53.5], "area": 9897.5, "iscrowd": 0}, {"id": 100, "image_id": 24, "category_id": 2, "bbox": [0.0, 31.999999999999996, 82.0, 42.0], "area": 3444.0, "iscrowd": 0}, {"id": 101, "image_id": 25, "category_id": 2, "bbox": [287.0, 131.5, 315.0, 62.0], "area": 19530.0, "iscrowd": 0}, {"id": 102, "image_id": 26, "category_id": 3, "bbox": [170.5, 283.75, 94.0, 104.5], "area": 9823.0, "iscrowd": 0}, {"id": 103, "image_id": 26, "category_id": 3, "bbox": [372.75000000000006, 272.5, 201.49999999999994, 97.0], "area": 19545.499999999993, "iscrowd": 0}, {"id": 104, "image_id": 26, "category_id": 1, "bbox": [171.75, 282.49999999999994, 403.5, 96.0], "area": 38736.0, "iscrowd": 0}, {"id": 105, "image_id": 26, "category_id": 2, "bbox": [278.75000000000006, 2.749999999999999, 236.49999999999994, 35.5], "area": 8395.749999999998, "iscrowd": 0}, {"id": 106, "image_id": 27, "category_id": 3, "bbox": [373.0, 182.99999999999997, 34.0, 457.0], "area": 15538.0, "iscrowd": 0}, {"id": 107, "image_id": 27, "category_id": 2, "bbox": [180.25000000000003, 164.25000000000006, 25.49999999999997, 345.49999999999994], "area": 8810.249999999989, "iscrowd": 0}, {"id": 108, "image_id": 27, "category_id": 1, "bbox": [378.0, 167.00000000000003, 52.0, 473.0], "area": 24596.0, "iscrowd": 0}, {"id": 109, "image_id": 27, "category_id": 2, "bbox": [607.75, 124.25000000000004, 23.5, 515.5], "area": 12114.25, "iscrowd": 0}, {"id": 110, "image_id": 28, "category_id": 2, "bbox": [381.25, 94.75000000000001, 39.5, 455.5], "area": 17992.25, "iscrowd": 0}, {"id": 111, "image_id": 29, "category_id": 3, "bbox": [528.25, 63.00000000000001, 73.5, 177.0], "area": 13009.5, "iscrowd": 0}, {"id": 112, "image_id": 29, "category_id": 3, "bbox": [530.0, 259.75, 46.0, 199.50000000000006], "area": 9177.000000000002, "iscrowd": 0}, {"id": 113, "image_id": 29, "category_id": 3, "bbox": [265.25, 90.0, 34.5, 411.0], "area": 14179.5, "iscrowd": 0}, {"id": 114, "image_id": 29, "category_id": 3, "bbox": [45.0, 176.0, 25.0, 245.0], "area": 6125.0, "iscrowd": 0}, {"id": 115, "image_id": 29, "category_id": 1, "bbox": [536.5, 0.0, 55.0, 623.0], "area": 34265.0, "iscrowd": 0}, {"id": 116, "image_id": 29, "category_id": 1, "bbox": [268.25, 84.25, 34.5, 421.5], "area": 14541.75, "iscrowd": 0}, {"id": 117, "image_id": 29, "category_id": 2, "bbox": [142.0, 132.5, 31.0, 315.0], "area": 9765.0, "iscrowd": 0}, {"id": 118, "image_id": 29, "category_id": 1, "bbox": [46.25, 161.25, 22.5, 260.5], "area": 5861.25, "iscrowd": 0}, {"id": 119, "image_id": 30, "category_id": 3, "bbox": [270.25, 444.25, 72.5, 57.5], "area": 4168.75, "iscrowd": 0}, {"id": 120, "image_id": 30, "category_id": 2, "bbox": [270.5, 0.0, 41.0, 76.0], "area": 3116.0, "iscrowd": 0}, {"id": 121, "image_id": 30, "category_id": 1, "bbox": [279.25, 197.24999999999997, 57.5, 308.5], "area": 17738.75, "iscrowd": 0}, {"id": 122, "image_id": 31, "category_id": 3, "bbox": [335.50000000000006, 396.99999999999994, 70.99999999999994, 54.00000000000006], "area": 3834.000000000001, "iscrowd": 0}, {"id": 123, "image_id": 31, "category_id": 3, "bbox": [416.5, 157.5, 67.99999999999994, 50.0], "area": 3399.9999999999973, "iscrowd": 0}, {"id": 124, "image_id": 31, "category_id": 1, "bbox": [58.24999999999999, 167.24999999999997, 506.5, 33.50000000000003], "area": 16967.750000000015, "iscrowd": 0}, {"id": 125, "image_id": 31, "category_id": 1, "bbox": [41.75000000000001, 405.25, 500.5, 51.50000000000006], "area": 25775.75000000003, "iscrowd": 0}, {"id": 126, "image_id": 32, "category_id": 3, "bbox": [473.25, 100.0, 72.5, 35.0], "area": 2537.5, "iscrowd": 0}, {"id": 127, "image_id": 32, "category_id": 1, "bbox": [98.24999999999996, 102.5, 454.50000000000006, 29.0], "area": 13180.500000000002, "iscrowd": 0}, {"id": 128, "image_id": 32, "category_id": 2, "bbox": [117.24999999999997, 312.49999999999994, 426.5, 36.0], "area": 15354.0, "iscrowd": 0}, {"id": 129, "image_id": 32, "category_id": 2, "bbox": [119.24999999999997, 530.75, 442.5, 37.5], "area": 16593.75, "iscrowd": 0}, {"id": 130, "image_id": 33, "category_id": 2, "bbox": [294.0, 33.999999999999986, 50.0, 335.0], "area": 16750.0, "iscrowd": 0}, {"id": 131, "image_id": 33, "category_id": 2, "bbox": [289.25, 483.24999999999994, 74.5, 156.50000000000006], "area": 11659.250000000004, "iscrowd": 0}, {"id": 132, "image_id": 34, "category_id": 3, "bbox": [160.75, 469.00000000000006, 54.50000000000003, 130.99999999999994], "area": 7139.500000000001, "iscrowd": 0}, {"id": 133, "image_id": 34, "category_id": 3, "bbox": [172.5, 280.75, 50.0, 97.5], "area": 4875.0, "iscrowd": 0}, {"id": 134, "image_id": 34, "category_id": 3, "bbox": [551.75, 134.0, 51.5, 226.0], "area": 11639.0, "iscrowd": 0}, {"id": 135, "image_id": 34, "category_id": 1, "bbox": [177.0, 141.5, 41.0, 231.0], "area": 9471.0, "iscrowd": 0}, {"id": 136, "image_id": 34, "category_id": 1, "bbox": [553.25, 135.5, 42.5, 231.00000000000006], "area": 9817.500000000002, "iscrowd": 0}, {"id": 137, "image_id": 34, "category_id": 1, "bbox": [163.5, 469.00000000000006, 49.0, 170.99999999999994], "area": 8378.999999999996, "iscrowd": 0}, {"id": 138, "image_id": 34, "category_id": 2, "bbox": [555.5, 480.0, 42.0, 160.0], "area": 6720.0, "iscrowd": 0}, {"id": 139, "image_id": 35, "category_id": 3, "bbox": [277.25, 230.0, 171.5, 312.0], "area": 53508.0, "iscrowd": 0}, {"id": 140, "image_id": 35, "category_id": 1, "bbox": [197.99999999999997, 0.0, 310.0, 637.0], "area": 197470.0, "iscrowd": 0}, {"id": 141, "image_id": 36, "category_id": 1, "bbox": [0.0, 110.0, 637.0, 470.0], "area": 299390.0, "iscrowd": 0}, {"id": 142, "image_id": 36, "category_id": 3, "bbox": [76.0, 184.0, 88.0, 221.0], "area": 19448.0, "iscrowd": 0}, {"id": 143, "image_id": 36, "category_id": 3, "bbox": [252.00000000000003, 133.5, 300.0, 410.0], "area": 123000.0, "iscrowd": 0}, {"id": 144, "image_id": 36, "category_id": 3, "bbox": [575.75, 276.5, 37.5, 92.0], "area": 3450.0, "iscrowd": 0}, {"id": 145, "image_id": 37, "category_id": 1, "bbox": [0.0, 110.0, 637.0, 470.0], "area": 299390.0, "iscrowd": 0}, {"id": 146, "image_id": 37, "category_id": 3, "bbox": [76.0, 184.0, 88.0, 221.0], "area": 19448.0, "iscrowd": 0}, {"id": 147, "image_id": 37, "category_id": 3, "bbox": [252.00000000000003, 133.5, 300.0, 410.0], "area": 123000.0, "iscrowd": 0}, {"id": 148, "image_id": 37, "category_id": 3, "bbox": [575.5, 276.5, 38.0, 92.0], "area": 3496.0, "iscrowd": 0}, {"id": 149, "image_id": 38, "category_id": 1, "bbox": [57.749999999999986, 14.499999999999993, 277.5, 559.0], "area": 155122.5, "iscrowd": 0}, {"id": 150, "image_id": 39, "category_id": 3, "bbox": [0.0, 162.99999999999997, 638.0, 98.00000000000003], "area": 62524.000000000015, "iscrowd": 0}, {"id": 151, "image_id": 40, "category_id": 1, "bbox": [249.25, 105.75, 108.5, 463.5], "area": 50289.75, "iscrowd": 0}, {"id": 152, "image_id": 41, "category_id": 1, "bbox": [123.99999999999999, 188.5, 296.0, 105.0], "area": 31080.0, "iscrowd": 0}, {"id": 153, "image_id": 41, "category_id": 1, "bbox": [371.5, 183.49999999999997, 202.0, 321.0], "area": 64842.0, "iscrowd": 0}, {"id": 154, "image_id": 42, "category_id": 2, "bbox": [401.99999999999994, 0.0, 154.00000000000006, 637.0], "area": 98098.00000000003, "iscrowd": 0}, {"id": 155, "image_id": 43, "category_id": 1, "bbox": [17.99999999999997, 131.5, 620.0, 210.0], "area": 130200.0, "iscrowd": 0}, {"id": 156, "image_id": 43, "category_id": 3, "bbox": [496.5, 225.0, 20.0, 35.0], "area": 700.0, "iscrowd": 0}, {"id": 157, "image_id": 43, "category_id": 3, "bbox": [541.0, 232.5, 18.0, 24.0], "area": 432.0, "iscrowd": 0}, {"id": 158, "image_id": 44, "category_id": 1, "bbox": [183.25, 70.24999999999999, 228.5, 472.5], "area": 107966.25, "iscrowd": 0}, {"id": 159, "image_id": 45, "category_id": 3, "bbox": [326.5, 255.49999999999997, 129.00000000000006, 207.00000000000003], "area": 26703.000000000015, "iscrowd": 0}, {"id": 160, "image_id": 45, "category_id": 1, "bbox": [163.5, 5.999999999999979, 313.0, 492.0], "area": 153996.0, "iscrowd": 0}, {"id": 161, "image_id": 46, "category_id": 2, "bbox": [206.5, 368.75, 190.0, 44.5], "area": 8455.0, "iscrowd": 0}, {"id": 162, "image_id": 46, "category_id": 1, "bbox": [414.5, 365.0, 35.0, 62.0], "area": 2170.0, "iscrowd": 0}, {"id": 163, "image_id": 46, "category_id": 1, "bbox": [445.25000000000006, 433.75, 23.499999999999943, 62.5], "area": 1468.7499999999964, "iscrowd": 0}, {"id": 164, "image_id": 47, "category_id": 1, "bbox": [0.0, 211.0, 638.0, 183.0], "area": 116754.0, "iscrowd": 0}, {"id": 165, "image_id": 48, "category_id": 1, "bbox": [177.75, 0.2499999999999858, 225.5, 589.5], "area": 132932.25, "iscrowd": 0}, {"id": 166, "image_id": 48, "category_id": 3, "bbox": [236.75, 203.75, 81.5, 45.49999999999997], "area": 3708.2499999999977, "iscrowd": 0}, {"id": 167, "image_id": 48, "category_id": 3, "bbox": [55.5, 224.25, 96.0, 77.5], "area": 7440.0, "iscrowd": 0}, {"id": 168, "image_id": 48, "category_id": 3, "bbox": [7.5, 18.25, 126.0, 107.5], "area": 13545.0, "iscrowd": 0}, {"id": 169, "image_id": 48, "category_id": 3, "bbox": [62.999999999999986, 471.0, 48.000000000000014, 32.00000000000006], "area": 1536.0000000000032, "iscrowd": 0}, {"id": 170, "image_id": 48, "category_id": 3, "bbox": [133.25, 500.75, 55.5, 52.5], "area": 2913.75, "iscrowd": 0}, {"id": 171, "image_id": 49, "category_id": 2, "bbox": [58.00000000000001, 195.0, 564.0, 154.0], "area": 86856.0, "iscrowd": 0}, {"id": 172, "image_id": 50, "category_id": 1, "bbox": [175.49999999999997, 236.0, 198.00000000000003, 100.0], "area": 19800.000000000004, "iscrowd": 0}, {"id": 173, "image_id": 51, "category_id": 1, "bbox": [274.0, 225.0, 176.0, 160.0], "area": 28160.0, "iscrowd": 0}, {"id": 174, "image_id": 51, "category_id": 3, "bbox": [283.75, 329.75, 46.5, 44.50000000000006], "area": 2069.2500000000027, "iscrowd": 0}, {"id": 175, "image_id": 51, "category_id": 3, "bbox": [333.24999999999994, 286.0, 49.50000000000006, 49.0], "area": 2425.5000000000027, "iscrowd": 0}, {"id": 176, "image_id": 52, "category_id": 1, "bbox": [290.0, 250.49999999999997, 122.0, 112.00000000000003], "area": 13664.000000000004, "iscrowd": 0}, {"id": 177, "image_id": 52, "category_id": 3, "bbox": [295.5, 320.75, 31.0, 35.5], "area": 1100.5, "iscrowd": 0}, {"id": 178, "image_id": 52, "category_id": 3, "bbox": [329.25000000000006, 290.5, 33.49999999999994, 34.0], "area": 1138.9999999999982, "iscrowd": 0}, {"id": 179, "image_id": 53, "category_id": 1, "bbox": [241.75, 354.0, 158.5, 127.99999999999994], "area": 20287.999999999993, "iscrowd": 0}, {"id": 180, "image_id": 54, "category_id": 1, "bbox": [259.75, 309.0, 118.49999999999994, 66.0], "area": 7820.999999999996, "iscrowd": 0}, {"id": 181, "image_id": 55, "category_id": 1, "bbox": [234.50000000000003, 263.00000000000006, 199.99999999999997, 137.99999999999994], "area": 27599.999999999985, "iscrowd": 0}, {"id": 182, "image_id": 56, "category_id": 1, "bbox": [234.50000000000003, 263.00000000000006, 199.99999999999997, 137.99999999999994], "area": 27599.999999999985, "iscrowd": 0}, {"id": 183, "image_id": 57, "category_id": 1, "bbox": [281.99999999999994, 239.0, 82.00000000000006, 62.0], "area": 5084.000000000004, "iscrowd": 0}, {"id": 184, "image_id": 57, "category_id": 2, "bbox": [403.5, 282.0, 97.00000000000006, 70.0], "area": 6790.000000000004, "iscrowd": 0}, {"id": 185, "image_id": 57, "category_id": 2, "bbox": [176.50000000000003, 218.0, 72.99999999999997, 51.0], "area": 3722.9999999999986, "iscrowd": 0}, {"id": 186, "image_id": 57, "category_id": 3, "bbox": [313.5, 275.0, 7.0, 14.0], "area": 98.0, "iscrowd": 0}, {"id": 187, "image_id": 57, "category_id": 3, "bbox": [338.00000000000006, 280.0, 20.999999999999943, 17.0], "area": 356.99999999999903, "iscrowd": 0}, {"id": 188, "image_id": 58, "category_id": 1, "bbox": [299.49999999999994, 152.5, 157.00000000000006, 84.0], "area": 13188.000000000005, "iscrowd": 0}, {"id": 189, "image_id": 58, "category_id": 2, "bbox": [0.0, 189.00000000000003, 268.0, 108.99999999999997], "area": 29211.999999999993, "iscrowd": 0}, {"id": 190, "image_id": 59, "category_id": 1, "bbox": [345.5, 155.5, 147.0, 86.00000000000003], "area": 12642.000000000004, "iscrowd": 0}, {"id": 191, "image_id": 59, "category_id": 2, "bbox": [29.999999999999982, 182.0, 268.0, 109.0], "area": 29212.0, "iscrowd": 0}, {"id": 192, "image_id": 60, "category_id": 2, "bbox": [113.75, 174.24999999999997, 268.5, 85.50000000000003], "area": 22956.750000000007, "iscrowd": 0}, {"id": 193, "image_id": 60, "category_id": 1, "bbox": [420.75, 146.75, 172.5, 92.5], "area": 15956.25, "iscrowd": 0}, {"id": 194, "image_id": 61, "category_id": 1, "bbox": [175.25, 11.499999999999986, 359.5, 362.0], "area": 130139.0, "iscrowd": 0}, {"id": 195, "image_id": 61, "category_id": 3, "bbox": [301.5, 119.25, 18.0, 76.5], "area": 1377.0, "iscrowd": 0}, {"id": 196, "image_id": 61, "category_id": 3, "bbox": [365.99999999999994, 182.99999999999997, 24.000000000000057, 42.00000000000003], "area": 1008.0000000000031, "iscrowd": 0}, {"id": 197, "image_id": 62, "category_id": 1, "bbox": [3.75, 200.75, 554.5, 157.5], "area": 87333.75, "iscrowd": 0}, {"id": 198, "image_id": 62, "category_id": 3, "bbox": [2.749999999999986, 249.75, 534.5, 75.5], "area": 40354.75, "iscrowd": 0}, {"id": 199, "image_id": 63, "category_id": 1, "bbox": [3.500000000000014, 200.49999999999997, 555.0, 158.00000000000003], "area": 87690.00000000001, "iscrowd": 0}, {"id": 200, "image_id": 63, "category_id": 3, "bbox": [2.5, 249.5, 535.0, 76.0], "area": 40660.0, "iscrowd": 0}, {"id": 201, "image_id": 64, "category_id": 2, "bbox": [0.0, 127.99999999999999, 376.0, 118.00000000000001], "area": 44368.00000000001, "iscrowd": 0}, {"id": 202, "image_id": 64, "category_id": 1, "bbox": [432.0, 137.5, 208.0, 131.0], "area": 27248.0, "iscrowd": 0}, {"id": 203, "image_id": 65, "category_id": 1, "bbox": [275.5, 230.49999999999997, 181.00000000000006, 158.00000000000003], "area": 28598.000000000015, "iscrowd": 0}, {"id": 204, "image_id": 66, "category_id": 1, "bbox": [295.0, 57.500000000000036, 92.0, 579.0], "area": 53268.0, "iscrowd": 0}, {"id": 205, "image_id": 67, "category_id": 1, "bbox": [271.25, 2.7500000000000213, 129.5, 626.5], "area": 81131.75, "iscrowd": 0}, {"id": 206, "image_id": 67, "category_id": 3, "bbox": [278.0, 154.74999999999997, 79.0, 451.5], "area": 35668.5, "iscrowd": 0}, {"id": 207, "image_id": 67, "category_id": 1, "bbox": [372.0, 30.25000000000002, 50.0, 490.5], "area": 24525.0, "iscrowd": 0}, {"id": 208, "image_id": 68, "category_id": 1, "bbox": [244.24999999999997, 2.5, 109.50000000000003, 512.0], "area": 56064.000000000015, "iscrowd": 0}, {"id": 209, "image_id": 68, "category_id": 1, "bbox": [360.5, 3.000000000000007, 72.0, 437.99999999999994], "area": 31535.999999999996, "iscrowd": 0}, {"id": 210, "image_id": 68, "category_id": 3, "bbox": [258.5, 160.75, 42.0, 348.5], "area": 14637.0, "iscrowd": 0}, {"id": 211, "image_id": 68, "category_id": 3, "bbox": [401.75, 401.75000000000006, 22.5, 50.49999999999994], "area": 1136.2499999999986, "iscrowd": 0}, {"id": 212, "image_id": 69, "category_id": 1, "bbox": [139.0, 0.2500000000000213, 110.0, 595.5], "area": 65505.0, "iscrowd": 0}, {"id": 213, "image_id": 69, "category_id": 3, "bbox": [192.5, 110.25000000000003, 59.0, 436.5], "area": 25753.5, "iscrowd": 0}, {"id": 214, "image_id": 69, "category_id": 1, "bbox": [272.25, 0.0, 97.5, 530.0], "area": 51675.0, "iscrowd": 0}, {"id": 215, "image_id": 70, "category_id": 2, "bbox": [112.5, 242.0, 349.0, 120.0], "area": 41880.0, "iscrowd": 0}, {"id": 216, "image_id": 71, "category_id": 1, "bbox": [86.74999999999999, 154.75, 220.5, 149.5], "area": 32964.75, "iscrowd": 0}, {"id": 217, "image_id": 72, "category_id": 1, "bbox": [87.0, 156.5, 225.0, 153.0], "area": 34425.0, "iscrowd": 0}, {"id": 218, "image_id": 73, "category_id": 1, "bbox": [81.74999999999999, 157.50000000000003, 224.5, 151.99999999999997], "area": 34123.99999999999, "iscrowd": 0}, {"id": 219, "image_id": 74, "category_id": 2, "bbox": [1.5000000000000213, 195.0, 599.0, 231.0], "area": 138369.0, "iscrowd": 0}, {"id": 220, "image_id": 75, "category_id": 2, "bbox": [123.25, 284.25, 339.50000000000006, 244.5], "area": 83007.75000000001, "iscrowd": 0}, {"id": 221, "image_id": 76, "category_id": 3, "bbox": [0.0, 324.0, 576.0, 65.0], "area": 37440.0, "iscrowd": 0}, {"id": 222, "image_id": 77, "category_id": 1, "bbox": [215.49999999999997, 182.99999999999997, 198.00000000000003, 208.00000000000003], "area": 41184.000000000015, "iscrowd": 0}, {"id": 223, "image_id": 77, "category_id": 3, "bbox": [228.49999999999997, 201.0, 161.00000000000003, 179.0], "area": 28819.000000000004, "iscrowd": 0}, {"id": 224, "image_id": 78, "category_id": 3, "bbox": [326.0, 83.75, 75.99999999999994, 415.5], "area": 31577.999999999978, "iscrowd": 0}, {"id": 225, "image_id": 79, "category_id": 2, "bbox": [0.9999999999999787, 60.0, 631.0, 37.0], "area": 23347.0, "iscrowd": 0}, {"id": 226, "image_id": 79, "category_id": 1, "bbox": [0.5000000000000071, 152.0, 638.0, 27.00000000000003], "area": 17226.00000000002, "iscrowd": 0}, {"id": 227, "image_id": 79, "category_id": 1, "bbox": [3.500000000000014, 229.5, 635.0, 36.0], "area": 22860.0, "iscrowd": 0}, {"id": 228, "image_id": 79, "category_id": 1, "bbox": [1.0000000000000142, 322.5, 638.0, 35.99999999999994], "area": 22967.999999999964, "iscrowd": 0}, {"id": 229, "image_id": 79, "category_id": 1, "bbox": [0.0, 407.5, 638.0, 59.00000000000006], "area": 37642.00000000004, "iscrowd": 0}, {"id": 230, "image_id": 79, "category_id": 1, "bbox": [4.500000000000028, 497.5, 635.0, 46.0], "area": 29210.0, "iscrowd": 0}, {"id": 231, "image_id": 79, "category_id": 1, "bbox": [1.0000000000000142, 602.0, 634.0, 33.0], "area": 20922.0, "iscrowd": 0}, {"id": 232, "image_id": 80, "category_id": 2, "bbox": [1.0000000000000142, 113.0, 219.0, 176.0], "area": 38544.0, "iscrowd": 0}, {"id": 233, "image_id": 80, "category_id": 2, "bbox": [234.00000000000003, 250.75, 266.0, 221.49999999999994], "area": 58918.999999999985, "iscrowd": 0}, {"id": 234, "image_id": 81, "category_id": 2, "bbox": [1.4999999999999858, 18.999999999999986, 638.0, 596.0], "area": 380248.0, "iscrowd": 0}, {"id": 235, "image_id": 82, "category_id": 2, "bbox": [180.0, 410.50000000000006, 270.0, 60.99999999999994], "area": 16469.999999999985, "iscrowd": 0}, {"id": 236, "image_id": 83, "category_id": 2, "bbox": [5.749999999999993, 440.75, 313.5, 182.5], "area": 57213.75, "iscrowd": 0}, {"id": 237, "image_id": 83, "category_id": 2, "bbox": [327.0, 156.75000000000006, 278.0, 345.49999999999994], "area": 96048.99999999999, "iscrowd": 0}, {"id": 238, "image_id": 84, "category_id": 2, "bbox": [35.99999999999998, 263.00000000000006, 332.0, 182.99999999999994], "area": 60755.99999999998, "iscrowd": 0}, {"id": 239, "image_id": 84, "category_id": 2, "bbox": [381.5, 364.00000000000006, 255.0, 173.99999999999994], "area": 44369.999999999985, "iscrowd": 0}, {"id": 240, "image_id": 85, "category_id": 2, "bbox": [4.499999999999993, 202.25, 456.0, 176.5], "area": 80484.0, "iscrowd": 0}, {"id": 241, "image_id": 85, "category_id": 2, "bbox": [476.5, 12.249999999999996, 142.0, 284.5], "area": 40399.0, "iscrowd": 0}, {"id": 242, "image_id": 86, "category_id": 2, "bbox": [325.0, 233.00000000000006, 314.0, 232.99999999999994], "area": 73161.99999999999, "iscrowd": 0}, {"id": 243, "image_id": 87, "category_id": 2, "bbox": [6.25, 83.0, 349.5, 334.0], "area": 116733.0, "iscrowd": 0}, {"id": 244, "image_id": 87, "category_id": 2, "bbox": [360.0, 93.25, 262.0, 272.5], "area": 71395.0, "iscrowd": 0}, {"id": 245, "image_id": 87, "category_id": 2, "bbox": [94.75000000000001, 492.0, 251.5, 131.0], "area": 32946.5, "iscrowd": 0}, {"id": 246, "image_id": 88, "category_id": 2, "bbox": [192.99999999999997, 165.5, 87.00000000000003, 324.0], "area": 28188.00000000001, "iscrowd": 0}, {"id": 247, "image_id": 88, "category_id": 2, "bbox": [292.75, 171.5, 163.5, 80.0], "area": 13080.0, "iscrowd": 0}, {"id": 248, "image_id": 89, "category_id": 2, "bbox": [327.25, 289.5, 304.5, 61.0], "area": 18574.5, "iscrowd": 0}, {"id": 249, "image_id": 90, "category_id": 2, "bbox": [137.00000000000003, 210.50000000000006, 490.0, 292.99999999999994], "area": 143569.99999999997, "iscrowd": 0}, {"id": 250, "image_id": 91, "category_id": 2, "bbox": [282.0, 199.00000000000003, 118.0, 434.0], "area": 51212.0, "iscrowd": 0}, {"id": 251, "image_id": 92, "category_id": 2, "bbox": [255.0, 242.00000000000003, 235.0, 219.99999999999997], "area": 51699.99999999999, "iscrowd": 0}, {"id": 252, "image_id": 93, "category_id": 2, "bbox": [104.00000000000003, 379.5, 339.0, 21.0], "area": 7119.0, "iscrowd": 0}, {"id": 253, "image_id": 94, "category_id": 2, "bbox": [90.99999999999997, 98.75, 261.0, 340.5], "area": 88870.5, "iscrowd": 0}, {"id": 254, "image_id": 95, "category_id": 2, "bbox": [90.99999999999997, 98.49999999999997, 261.0, 341.0], "area": 89001.0, "iscrowd": 0}, {"id": 255, "image_id": 96, "category_id": 2, "bbox": [262.5, 89.00000000000003, 73.0, 368.0], "area": 26864.0, "iscrowd": 0}, {"id": 256, "image_id": 97, "category_id": 2, "bbox": [72.24999999999997, 419.49999999999994, 399.5, 129.00000000000006], "area": 51535.50000000002, "iscrowd": 0}, {"id": 257, "image_id": 97, "category_id": 2, "bbox": [61.5, 358.24999999999994, 153.00000000000003, 59.50000000000006], "area": 9103.500000000011, "iscrowd": 0}, {"id": 258, "image_id": 98, "category_id": 2, "bbox": [139.75, 461.0, 130.5, 130.0], "area": 16965.0, "iscrowd": 0}, {"id": 259, "image_id": 99, "category_id": 2, "bbox": [292.49999999999994, 248.5, 91.0, 148.0], "area": 13468.0, "iscrowd": 0}, {"id": 260, "image_id": 100, "category_id": 2, "bbox": [161.0, 276.75, 348.0, 22.5], "area": 7830.0, "iscrowd": 0}, {"id": 261, "image_id": 100, "category_id": 2, "bbox": [429.75, 217.5, 207.5, 60.0], "area": 12450.0, "iscrowd": 0}, {"id": 262, "image_id": 101, "category_id": 2, "bbox": [0.0, 352.0, 216.0, 46.0], "area": 9936.0, "iscrowd": 0}, {"id": 263, "image_id": 101, "category_id": 2, "bbox": [308.5, 197.5, 328.0, 169.0], "area": 55432.0, "iscrowd": 0}, {"id": 264, "image_id": 102, "category_id": 2, "bbox": [202.50000000000003, 108.50000000000001, 319.0, 155.0], "area": 49445.0, "iscrowd": 0}, {"id": 265, "image_id": 103, "category_id": 2, "bbox": [166.74999999999997, 138.74999999999997, 224.50000000000003, 388.5], "area": 87218.25000000001, "iscrowd": 0}, {"id": 266, "image_id": 104, "category_id": 2, "bbox": [119.50000000000003, 387.5, 425.0, 135.0], "area": 57375.0, "iscrowd": 0}, {"id": 267, "image_id": 105, "category_id": 2, "bbox": [143.00000000000006, 385.5, 467.99999999999994, 137.0], "area": 64115.99999999999, "iscrowd": 0}, {"id": 268, "image_id": 106, "category_id": 2, "bbox": [320.75, 0.0, 152.5, 600.0], "area": 91500.0, "iscrowd": 0}, {"id": 269, "image_id": 107, "category_id": 2, "bbox": [283.0, 244.00000000000003, 38.0, 27.99999999999997], "area": 1063.9999999999989, "iscrowd": 0}, {"id": 270, "image_id": 108, "category_id": 2, "bbox": [318.74999999999994, 310.5, 118.5, 279.0], "area": 33061.5, "iscrowd": 0}, {"id": 271, "image_id": 109, "category_id": 2, "bbox": [313.5, 366.99999999999994, 37.00000000000006, 67.00000000000006], "area": 2479.000000000006, "iscrowd": 0}, {"id": 272, "image_id": 110, "category_id": 2, "bbox": [389.5, 234.0, 21.0, 87.0], "area": 1827.0, "iscrowd": 0}, {"id": 273, "image_id": 111, "category_id": 2, "bbox": [252.99999999999997, 115.5, 62.00000000000003, 439.0], "area": 27218.00000000001, "iscrowd": 0}, {"id": 274, "image_id": 111, "category_id": 2, "bbox": [318.5, 83.5, 67.00000000000006, 123.0], "area": 8241.000000000007, "iscrowd": 0}, {"id": 275, "image_id": 112, "category_id": 2, "bbox": [253.25, 115.5, 61.5, 439.0], "area": 26998.5, "iscrowd": 0}, {"id": 276, "image_id": 112, "category_id": 2, "bbox": [318.75000000000006, 83.75, 66.5, 122.5], "area": 8146.25, "iscrowd": 0}, {"id": 277, "image_id": 113, "category_id": 2, "bbox": [270.5, 326.0, 302.0, 98.0], "area": 29596.0, "iscrowd": 0}, {"id": 278, "image_id": 114, "category_id": 2, "bbox": [279.99999999999994, 11.500000000000021, 126.0, 369.0], "area": 46494.0, "iscrowd": 0}, {"id": 279, "image_id": 115, "category_id": 2, "bbox": [189.0, 476.99999999999994, 102.0, 94.00000000000006], "area": 9588.000000000005, "iscrowd": 0}, {"id": 280, "image_id": 116, "category_id": 2, "bbox": [183.75, 431.75, 172.5, 124.5], "area": 21476.25, "iscrowd": 0}, {"id": 281, "image_id": 116, "category_id": 2, "bbox": [403.75, 332.5, 72.5, 55.0], "area": 3987.5, "iscrowd": 0}, {"id": 282, "image_id": 117, "category_id": 2, "bbox": [159.00000000000003, 3.4999999999999964, 78.99999999999997, 278.0], "area": 21961.999999999993, "iscrowd": 0}, {"id": 283, "image_id": 117, "category_id": 2, "bbox": [188.5, 162.5, 99.0, 191.0], "area": 18909.0, "iscrowd": 0}, {"id": 284, "image_id": 118, "category_id": 1, "bbox": [35.50000000000001, 11.999999999999993, 533.0, 575.0], "area": 306475.0, "iscrowd": 0}, {"id": 285, "image_id": 119, "category_id": 1, "bbox": [194.25, 257.0, 167.5, 203.99999999999994], "area": 34169.99999999999, "iscrowd": 0}, {"id": 286, "image_id": 120, "category_id": 2, "bbox": [58.00000000000001, 38.50000000000001, 549.0, 109.0], "area": 59841.0, "iscrowd": 0}, {"id": 287, "image_id": 120, "category_id": 1, "bbox": [35.50000000000001, 265.5, 554.0, 109.0], "area": 60386.0, "iscrowd": 0}, {"id": 288, "image_id": 120, "category_id": 1, "bbox": [149.5, 438.5, 404.0, 141.0], "area": 56964.0, "iscrowd": 0}, {"id": 289, "image_id": 121, "category_id": 2, "bbox": [26.50000000000002, 90.5, 589.0, 496.0], "area": 292144.0, "iscrowd": 0}, {"id": 290, "image_id": 122, "category_id": 2, "bbox": [61.000000000000014, 33.0, 558.0, 131.0], "area": 73098.0, "iscrowd": 0}, {"id": 291, "image_id": 122, "category_id": 2, "bbox": [24.499999999999993, 257.0, 555.0, 95.0], "area": 52725.0, "iscrowd": 0}, {"id": 292, "image_id": 122, "category_id": 2, "bbox": [151.5, 434.5, 407.0, 158.0], "area": 64306.0, "iscrowd": 0}, {"id": 293, "image_id": 123, "category_id": 1, "bbox": [28.000000000000007, 20.0, 508.0, 517.0], "area": 262636.0, "iscrowd": 0}, {"id": 294, "image_id": 123, "category_id": 3, "bbox": [281.5, 268.75, 60.0, 49.5], "area": 2970.0, "iscrowd": 0}, {"id": 295, "image_id": 123, "category_id": 3, "bbox": [222.25, 293.75, 50.5, 49.5], "area": 2499.75, "iscrowd": 0}, {"id": 296, "image_id": 124, "category_id": 1, "bbox": [21.999999999999957, 243.0, 612.0, 70.0], "area": 42840.0, "iscrowd": 0}, {"id": 297, "image_id": 124, "category_id": 1, "bbox": [14.0, 153.5, 52.0, 164.0], "area": 8528.0, "iscrowd": 0}, {"id": 298, "image_id": 125, "category_id": 1, "bbox": [43.999999999999986, 229.5, 517.0, 183.99999999999994], "area": 95127.99999999997, "iscrowd": 0}, {"id": 299, "image_id": 125, "category_id": 3, "bbox": [232.00000000000003, 325.50000000000006, 82.99999999999997, 77.99999999999994], "area": 6473.999999999993, "iscrowd": 0}, {"id": 300, "image_id": 125, "category_id": 3, "bbox": [336.0, 309.0, 138.0, 76.0], "area": 10488.0, "iscrowd": 0}, {"id": 301, "image_id": 126, "category_id": 1, "bbox": [169.5, 6.000000000000014, 51.0, 615.0], "area": 31365.0, "iscrowd": 0}], "categories": [{"id": 1, "name": "Bad Weld"}, {"id": 2, "name": "Good Weld"}, {"id": 3, "name": "Defect"}]}
coco/train.json ADDED
The diff for this file is too large to render. See raw diff
 
coco/valid.json ADDED
The diff for this file is too large to render. See raw diff
 
data.yaml ADDED
@@ -0,0 +1,6 @@
 
 
 
 
 
 
 
1
+ train: ../train/images
2
+ val: ../valid/images
3
+ test: ../test/images
4
+
5
+ nc: 3
6
+ names: ['Bad Weld', 'Good Weld', 'Defect']
test/.DS_Store ADDED
Binary file (6.15 kB). View file
 
test/images/02fd0af7-51ab46bb-c13_jpg.rf.7de08cd3b264d9098d09f5fe6d21c959.jpg ADDED

Git LFS Details

  • SHA256: dca734f3287f823ab85fbfb3c85a4a04b4acb43046b4dbc39af53cafc8e85f47
  • Pointer size: 130 Bytes
  • Size of remote file: 34.7 kB
test/images/1aa4b44c-d01b8a11-Hot-crack_jpg.rf.57393ca7936f061ca5991481b2b5c485.jpg ADDED

Git LFS Details

  • SHA256: 4ae59bd790ea6ae4bea66fc6268c512b2510128e638c648890220765a10ecf09
  • Pointer size: 130 Bytes
  • Size of remote file: 53.4 kB
test/images/295992d6-f617b725-c1_png_jpg.rf.5f645e13f1695df588b0644ca9702c43.jpg ADDED

Git LFS Details

  • SHA256: 411e6a606d32b1d2b039e0dff328f18a3f9fe7ae16e8a24df0868ae5238bc539
  • Pointer size: 130 Bytes
  • Size of remote file: 44.6 kB
test/images/4a05306b-ca866e1f-c12_jpg.rf.c5c926823394e6056b533bedd6e64c99.jpg ADDED

Git LFS Details

  • SHA256: 7a4fe8a8e5b456a8ea7695a45d9ed9c7ef95c19cad5a1a422fb2d472cb65c719
  • Pointer size: 130 Bytes
  • Size of remote file: 66.3 kB
test/images/Good-Welding-images_11_jpeg.rf.4807e1282a383cba87b1e2e3c77ca9ce.jpg ADDED

Git LFS Details

  • SHA256: a57d4e8615c3c87e0cd6b522fd84a21e4e39e55265907b8cd49589a7a4160f1b
  • Pointer size: 130 Bytes
  • Size of remote file: 51.1 kB
test/images/Good-Welding-images_12_jpeg.rf.126bee697b91a6562ffb0e9701b2fe8c.jpg ADDED

Git LFS Details

  • SHA256: 15c07240f7b77a32e8d8dc853610f3890258e731b787b129625b0aeb46e4b8ed
  • Pointer size: 130 Bytes
  • Size of remote file: 35.4 kB
test/images/Good-Welding-images_12_jpeg_jpg.rf.9fa5a26596733b74baf1f974b8210c28.jpg ADDED

Git LFS Details

  • SHA256: 1c8db86928c04c3fe0179dacb9d4e406f985db980950f52975acf782f94474c3
  • Pointer size: 130 Bytes
  • Size of remote file: 35.4 kB
test/images/Good-Welding-images_17_jpeg_jpg.rf.be58c70a9f7f542fc89cb48847776741.jpg ADDED

Git LFS Details

  • SHA256: 014a409ce5de31ea5c0a2a15241b148d10482a8213de783efb2eb6a401a767f3
  • Pointer size: 130 Bytes
  • Size of remote file: 61.6 kB
test/images/Good-Welding-images_23_jpeg_jpg.rf.fdf50352e3c124ff6edab3e96257a040.jpg ADDED

Git LFS Details

  • SHA256: 24a338c60fb276729d9927d6f665457bfa73623ab5b39f5100d8a001f87d5978
  • Pointer size: 130 Bytes
  • Size of remote file: 63 kB
test/images/Good-Welding-images_28_png.rf.503eeed161b61cf8ec218b1c17440787.jpg ADDED

Git LFS Details

  • SHA256: 87bceea8ab06738420f5fa957d07577f8cd02c1f64f55c04b59550cc06d4c532
  • Pointer size: 130 Bytes
  • Size of remote file: 36.3 kB
test/images/Good-Welding-images_30_jpeg.rf.4af312f6d3af2b9ec3a3c7814019f387.jpg ADDED

Git LFS Details

  • SHA256: 11eaca71a04c656f34ea34138f6da1036a5769980e49d8a906dca1b9135019de
  • Pointer size: 130 Bytes
  • Size of remote file: 64 kB
test/images/Good-Welding-images_33_jpeg.rf.0e3a517af5a8cc2a5ea0a02f5ed2fbab.jpg ADDED

Git LFS Details

  • SHA256: 2f52c785774bc7c70b4dd94b04c9ca2087f5f0b0bd5fb11e5a10ebfd008599ff
  • Pointer size: 130 Bytes
  • Size of remote file: 76.5 kB
test/images/Good-Welding-images_33_jpeg_jpg.rf.782ccc0dfca926b946a6b664dd4cacd1.jpg ADDED

Git LFS Details

  • SHA256: 2bd7d0fe0b246fb7c0d32935ec1ca1a163566b0e2ef2c8a40b3d66b326d4770d
  • Pointer size: 130 Bytes
  • Size of remote file: 76.3 kB
test/images/SampleV1_1_mp4-1_jpg.rf.3f50c974a91c4e6348dd49491f06def8.jpg ADDED

Git LFS Details

  • SHA256: 675f64530af07e74ab438bd676d66cd6da468dadda6e1e077c0ecf0ea2b1161e
  • Pointer size: 130 Bytes
  • Size of remote file: 43.4 kB
test/images/SampleV1_1_mp4-42_jpg.rf.6e68d9186e630ffb996233ad2a593f51.jpg ADDED

Git LFS Details

  • SHA256: 804549538ace0b2d49b63914395043c4b4ee6677c5b9bf5097003eac408c6026
  • Pointer size: 130 Bytes
  • Size of remote file: 43.4 kB
test/images/SampleV1_2_mp4-14_jpg.rf.4dba7e8bd84314a155dd85df33b5f4d9.jpg ADDED

Git LFS Details

  • SHA256: de3b754ba047d307017f0691c2b56fc8df83860a72ab23bf73f1221f4d175179
  • Pointer size: 130 Bytes
  • Size of remote file: 39.4 kB
test/images/SampleV2_1_mp4-0_jpg.rf.32dc225d9b5d11d01260f75c918a9961.jpg ADDED

Git LFS Details

  • SHA256: 0037544b90d38fad26808f279d835d4ebd137918645fb953f241bac28d66e7bd
  • Pointer size: 130 Bytes
  • Size of remote file: 50.3 kB
test/images/SampleV2_1_mp4-59_jpg.rf.b500f4a89177615c16be765f9f15b910.jpg ADDED

Git LFS Details

  • SHA256: 73114d87a436da5b41e9eff024463afce888dee0b04d37eb67d880508ddc1575
  • Pointer size: 130 Bytes
  • Size of remote file: 56.7 kB
test/images/SampleV2_1_mp4-60_jpg.rf.40f4a4094130e65b1a801b49fefc5d01.jpg ADDED

Git LFS Details

  • SHA256: 0dc7fa8cabcbcb8a4c34a017a8f9f8c6163b0c052619b21041bf088c6023af0a
  • Pointer size: 130 Bytes
  • Size of remote file: 61.8 kB
test/images/SampleV2_1_mp4-90_jpg.rf.19ad4979865d6aba1cfaaa23f1dfb1f9.jpg ADDED

Git LFS Details

  • SHA256: 79a36a6b75675dcc58a1ed5e8a0181b2b16b984771adca07030ae588bbfa62eb
  • Pointer size: 130 Bytes
  • Size of remote file: 61.4 kB
test/images/SampleV2_1_mp4-97_jpg.rf.1cbd06413c3d08495ffce915e0d8bd94.jpg ADDED

Git LFS Details

  • SHA256: c6bc7acb41d000634e9e407bca881d20f73af4e69cb282552d4e88bde3311dcb
  • Pointer size: 130 Bytes
  • Size of remote file: 51.7 kB
test/images/SampleV2_2_mp4-100_jpg.rf.95c9ff940b64d347919b6d49dfb8b0b3.jpg ADDED

Git LFS Details

  • SHA256: 8af8f6440a180be96c164c4849ca7332fa5c855e9ef1fbb37d441347424a52a0
  • Pointer size: 130 Bytes
  • Size of remote file: 60.8 kB
test/images/SampleV2_2_mp4-24_jpg.rf.0909700c29763d6bbe0f3e7df949475b.jpg ADDED

Git LFS Details

  • SHA256: 04a37b3971f5c239fcdd6e7341587321808dcd0e8ef9c14ea96500e607990139
  • Pointer size: 130 Bytes
  • Size of remote file: 45.9 kB
test/images/SampleV2_2_mp4-39_jpg.rf.e18c2b9f47afa039f3f2fee002312552.jpg ADDED

Git LFS Details

  • SHA256: f2a325696637cdeb6d556bdc663ddf7d0474a4d74e73d4f2d5188c599251ad90
  • Pointer size: 130 Bytes
  • Size of remote file: 47.2 kB
test/images/SampleV2_2_mp4-57_jpg.rf.95a7afd6a5fef7ea6a6161a433182ce3.jpg ADDED

Git LFS Details

  • SHA256: a25ee1d7bb1f9f19e876b5ce19731ae3032538066e6271edba9a3159f1eff3e6
  • Pointer size: 130 Bytes
  • Size of remote file: 35.9 kB
test/images/SampleV2_2_mp4-59_jpg.rf.5e6543b79b7abac05cf8005d24f61eb5.jpg ADDED

Git LFS Details

  • SHA256: cab913ac3909ecc52c261e7a073acaf0d6841be74f7b510b3f23d774def8bb78
  • Pointer size: 130 Bytes
  • Size of remote file: 57.9 kB
test/images/SampleV2_2_mp4-71_jpg.rf.de0eaa495c44a7817fab26c6c6277796.jpg ADDED

Git LFS Details

  • SHA256: 50f3823710e59042a480b80631c28d3fa6a3c30e20d19327d55cd029f33f1ea5
  • Pointer size: 130 Bytes
  • Size of remote file: 47.8 kB
test/images/SampleV2_2_mp4-76_jpg.rf.492360f34b458a190c41d157fff3dbba.jpg ADDED

Git LFS Details

  • SHA256: 628d569d97c684bee801818d7110522962cf07e9f3a6dc14a577cd6286b57a17
  • Pointer size: 130 Bytes
  • Size of remote file: 43.8 kB
test/images/SampleV2_2_mp4-98_jpg.rf.83b6e5f3fa68582da8fe9db065a00a98.jpg ADDED

Git LFS Details

  • SHA256: 30908913387585d6ea4b7b5febacef29a572df198c9d11bb57f5ea9f8af7d73c
  • Pointer size: 130 Bytes
  • Size of remote file: 64.5 kB
test/images/SampleV3_1_mp4-24_jpg.rf.017f90fdc7b6c9677febabbd168597fb.jpg ADDED

Git LFS Details

  • SHA256: 8996e362b7f2411afc2af3a0b995bb8fecd7130e3336626c2c490e1d75fb69e8
  • Pointer size: 130 Bytes
  • Size of remote file: 38.9 kB
test/images/SampleV3_1_mp4-45_jpg.rf.a4085868c8ba207b4e9941d0af06c894.jpg ADDED

Git LFS Details

  • SHA256: f133e584643b925da9dcffaf768a7bb2f0fb8d1e95029c5797e72f36b7702aa8
  • Pointer size: 130 Bytes
  • Size of remote file: 48.3 kB
test/images/SampleV3_1_mp4-50_jpg.rf.5a367e6d492cd43c4a8627799b654370.jpg ADDED

Git LFS Details

  • SHA256: f68f1356dcf2b19b511b6a3d314404e195cf2c168667addb3e353a0a0a4d4131
  • Pointer size: 130 Bytes
  • Size of remote file: 47.3 kB
test/images/SampleV3_1_mp4-8_jpg.rf.15adb36ac87bf5e5533ced60df5f5635.jpg ADDED

Git LFS Details

  • SHA256: 74e60234f7eeb70b84bd5d167e35bd090eaa19bbf6f653191be703c5dd26385f
  • Pointer size: 130 Bytes
  • Size of remote file: 43.2 kB
test/images/SampleV3_2_mp4-2_jpg.rf.f673f3917f7d15f03110e853f63696dc.jpg ADDED

Git LFS Details

  • SHA256: 851dd3cd81b0c4874fa8e25ceb0a115d21b3e48e11be5ccf9feae053e4e51dc1
  • Pointer size: 130 Bytes
  • Size of remote file: 32.4 kB
test/images/Screenshot-2022-12-05-223424_jpeg.rf.3de790d465fbb0428d1066ab0ec33daf.jpg ADDED

Git LFS Details

  • SHA256: 7864d8918c50b745aeab87f9cbce38f1e7bd1d16dcc8c504c0ee583cce57a57a
  • Pointer size: 130 Bytes
  • Size of remote file: 44 kB
test/images/Screenshot-2022-12-05-223445_jpeg.rf.a835025488cff5c8564c4d16df1b7ad6.jpg ADDED

Git LFS Details

  • SHA256: 6beaa66d95e3f3abb8c84e4aad6c5dd830977ef3973e03aef68e0a89744519b9
  • Pointer size: 130 Bytes
  • Size of remote file: 57.7 kB
test/images/Screenshot-2022-12-05-223445_jpeg_jpg.rf.e35a047d0ee08846662cb19b302fb1a7.jpg ADDED

Git LFS Details

  • SHA256: 4a28a41e39726b4450251f65e41a03e6188b4d88c948d78bd76c6fc838c8f09a
  • Pointer size: 130 Bytes
  • Size of remote file: 57.7 kB
test/images/Screenshot-2022-12-05-223504_jpeg.rf.f6c1d1d819ba7212516d5da2471bdb04.jpg ADDED

Git LFS Details

  • SHA256: 89c6437b13ca5384f8fb60fe406348ad56ec5652691e93c2758c511a08da40b7
  • Pointer size: 130 Bytes
  • Size of remote file: 45.5 kB
test/images/Screenshot-2022-12-05-223616_jpeg_jpg.rf.ed5db415112db98336eb0a6eabfe3fd0.jpg ADDED

Git LFS Details

  • SHA256: 5f1d56b9259cf51b6437fdf23ef021f83edb3ebe37a55b327d86aa9c148c5480
  • Pointer size: 130 Bytes
  • Size of remote file: 51.4 kB
test/images/Screenshot-2022-12-05-224056_jpeg.rf.0198544ad2d024d446a77d8f8c04ff12.jpg ADDED

Git LFS Details

  • SHA256: af9add31cd2f51d01b019cc78c70f52ff037526e31bba6809a02b9d8140a07c6
  • Pointer size: 130 Bytes
  • Size of remote file: 35.5 kB
test/images/Screenshot-2022-12-05-224335_jpeg_jpg.rf.bcfe0035e76676a1f9056aea47c18999.jpg ADDED

Git LFS Details

  • SHA256: 37f926d1910d1fb1276119b9368e1efebd5fbf2871a91453e15aabc805b83083
  • Pointer size: 130 Bytes
  • Size of remote file: 50.3 kB
test/images/Screenshot-2022-12-05-230149_jpeg.rf.9a609cc50aed07d1532d574bdfddd081.jpg ADDED

Git LFS Details

  • SHA256: e84a7e300aac8202a2c40798e1ef5fdf87f73109deb0fb8b03ab35329d69c1c7
  • Pointer size: 130 Bytes
  • Size of remote file: 37.6 kB
test/images/Screenshot-2022-12-05-230257_jpeg_jpg.rf.b7d7eb8e010e48641638d6a878f9af61.jpg ADDED

Git LFS Details

  • SHA256: 41f809cc6d20e74330918ab1c78bac64601c3be71ee4563418909b0529897abf
  • Pointer size: 130 Bytes
  • Size of remote file: 53.8 kB
test/images/Slag-inclusion-welding-images_11_jpeg.rf.06f53c90b96f942c575dad2d8ba10992.jpg ADDED

Git LFS Details

  • SHA256: fb7b39f447730d473ae47671eff3c578e8cfc3e4d17c15aa0aab5649eb6cd562
  • Pointer size: 130 Bytes
  • Size of remote file: 31.4 kB