query stringclasses 2
values | image dict | annot stringlengths 75 192 | reasoning stringclasses 0
values | cate stringclasses 1
value | task stringclasses 1
value | metadata stringlengths 439 563 |
|---|---|---|---|---|---|---|
"This is a cross-sectional micrograph of a Ti10Mo6Cu fused track made by laser powder bed fusion. Wh(...TRUNCATED) | {"bytes":"/9j/4AAQSkZJRgABAQAAAQABAAD/2wBDAAMCAgICAgMCAgIDAwMDBAYEBAQEBAgGBgUGCQgKCgkICQkKDA8MCgsOCw(...TRUNCATED) | "Laser power: 100 W; scanning speed: 0.40 m/s. Average width: 136.09 µm; height: 57.33 µm; penetra(...TRUNCATED) | null | materials_science | lpbf_track_characterization | "{\"dataset\": \"Ti10Mo6Cu LPBF fused tracks and layers\", \"depth_to_width_ratio\": 0.217992, \"dep(...TRUNCATED) |
"This is a cross-sectional micrograph of a Ti10Mo6Cu fused track made by laser powder bed fusion. Wh(...TRUNCATED) | {"bytes":"/9j/4AAQSkZJRgABAQAAAQABAAD/2wBDAAMCAgICAgMCAgIDAwMDBAYEBAQEBAgGBgUGCQgKCgkICQkKDA8MCgsOCw(...TRUNCATED) | "Laser power: 100 W; scanning speed: 0.40 m/s. Average width: 136.09 µm; height: 57.33 µm; penetra(...TRUNCATED) | null | materials_science | lpbf_track_characterization | "{\"dataset\": \"Ti10Mo6Cu LPBF fused tracks and layers\", \"depth_to_width_ratio\": 0.217992, \"dep(...TRUNCATED) |
"This is a cross-sectional micrograph of a Ti10Mo6Cu fused track made by laser powder bed fusion. Wh(...TRUNCATED) | {"bytes":"/9j/4AAQSkZJRgABAQAAAQABAAD/2wBDAAMCAgICAgMCAgIDAwMDBAYEBAQEBAgGBgUGCQgKCgkICQkKDA8MCgsOCw(...TRUNCATED) | "Laser power: 100 W; scanning speed: 0.40 m/s. Average width: 136.09 µm; height: 57.33 µm; penetra(...TRUNCATED) | null | materials_science | lpbf_track_characterization | "{\"dataset\": \"Ti10Mo6Cu LPBF fused tracks and layers\", \"depth_to_width_ratio\": 0.217992, \"dep(...TRUNCATED) |
"This is a cross-sectional micrograph of a Ti10Mo6Cu fused track made by laser powder bed fusion. Wh(...TRUNCATED) | {"bytes":"/9j/4AAQSkZJRgABAQAAAQABAAD/2wBDAAMCAgICAgMCAgIDAwMDBAYEBAQEBAgGBgUGCQgKCgkICQkKDA8MCgsOCw(...TRUNCATED) | "Laser power: 100 W; scanning speed: 0.50 m/s. Average width: 120.85 µm; height: 46.67 µm; penetra(...TRUNCATED) | null | materials_science | lpbf_track_characterization | "{\"dataset\": \"Ti10Mo6Cu LPBF fused tracks and layers\", \"depth_to_width_ratio\": 0.231695, \"dep(...TRUNCATED) |
"This is a cross-sectional micrograph of a Ti10Mo6Cu fused track made by laser powder bed fusion. Wh(...TRUNCATED) | {"bytes":"/9j/4AAQSkZJRgABAQAAAQABAAD/2wBDAAMCAgICAgMCAgIDAwMDBAYEBAQEBAgGBgUGCQgKCgkICQkKDA8MCgsOCw(...TRUNCATED) | "Laser power: 100 W; scanning speed: 0.50 m/s. Average width: 120.85 µm; height: 46.67 µm; penetra(...TRUNCATED) | null | materials_science | lpbf_track_characterization | "{\"dataset\": \"Ti10Mo6Cu LPBF fused tracks and layers\", \"depth_to_width_ratio\": 0.231695, \"dep(...TRUNCATED) |
"This is a cross-sectional micrograph of a Ti10Mo6Cu fused track made by laser powder bed fusion. Wh(...TRUNCATED) | {"bytes":"/9j/4AAQSkZJRgABAQAAAQABAAD/2wBDAAMCAgICAgMCAgIDAwMDBAYEBAQEBAgGBgUGCQgKCgkICQkKDA8MCgsOCw(...TRUNCATED) | "Laser power: 100 W; scanning speed: 0.50 m/s. Average width: 120.85 µm; height: 46.67 µm; penetra(...TRUNCATED) | null | materials_science | lpbf_track_characterization | "{\"dataset\": \"Ti10Mo6Cu LPBF fused tracks and layers\", \"depth_to_width_ratio\": 0.231695, \"dep(...TRUNCATED) |
"This is a cross-sectional micrograph of a Ti10Mo6Cu fused track made by laser powder bed fusion. Wh(...TRUNCATED) | {"bytes":"/9j/4AAQSkZJRgABAQAAAQABAAD/2wBDAAMCAgICAgMCAgIDAwMDBAYEBAQEBAgGBgUGCQgKCgkICQkKDA8MCgsOCw(...TRUNCATED) | "Laser power: 100 W; scanning speed: 0.60 m/s. Average width: 101.52 µm; height: 64.00 µm; penetra(...TRUNCATED) | null | materials_science | lpbf_track_characterization | "{\"dataset\": \"Ti10Mo6Cu LPBF fused tracks and layers\", \"depth_to_width_ratio\": 0.075522, \"dep(...TRUNCATED) |
"This is a cross-sectional micrograph of a Ti10Mo6Cu fused track made by laser powder bed fusion. Wh(...TRUNCATED) | {"bytes":"/9j/4AAQSkZJRgABAQAAAQABAAD/2wBDAAMCAgICAgMCAgIDAwMDBAYEBAQEBAgGBgUGCQgKCgkICQkKDA8MCgsOCw(...TRUNCATED) | "Laser power: 100 W; scanning speed: 0.60 m/s. Average width: 101.52 µm; height: 64.00 µm; penetra(...TRUNCATED) | null | materials_science | lpbf_track_characterization | "{\"dataset\": \"Ti10Mo6Cu LPBF fused tracks and layers\", \"depth_to_width_ratio\": 0.075522, \"dep(...TRUNCATED) |
"This is a cross-sectional micrograph of a Ti10Mo6Cu fused track made by laser powder bed fusion. Wh(...TRUNCATED) | {"bytes":"/9j/4AAQSkZJRgABAQAAAQABAAD/2wBDAAMCAgICAgMCAgIDAwMDBAYEBAQEBAgGBgUGCQgKCgkICQkKDA8MCgsOCw(...TRUNCATED) | "Laser power: 100 W; scanning speed: 0.60 m/s. Average width: 101.52 µm; height: 64.00 µm; penetra(...TRUNCATED) | null | materials_science | lpbf_track_characterization | "{\"dataset\": \"Ti10Mo6Cu LPBF fused tracks and layers\", \"depth_to_width_ratio\": 0.075522, \"dep(...TRUNCATED) |
"This is a cross-sectional micrograph of a Ti10Mo6Cu fused track made by laser powder bed fusion. Wh(...TRUNCATED) | {"bytes":"/9j/4AAQSkZJRgABAQAAAQABAAD/2wBDAAMCAgICAgMCAgIDAwMDBAYEBAQEBAgGBgUGCQgKCgkICQkKDA8MCgsOCw(...TRUNCATED) | "Laser power: 100 W; scanning speed: 0.80 m/s. Average width: 91.88 µm; height: 44.00 µm; penetrat(...TRUNCATED) | null | materials_science | lpbf_track_characterization | "{\"dataset\": \"Ti10Mo6Cu LPBF fused tracks and layers\", \"depth_to_width_ratio\": 0.206794, \"dep(...TRUNCATED) |
End of preview. Expand in Data Studio
YAML Metadata Warning:empty or missing yaml metadata in repo card
Check out the documentation for more information.
Ti10Mo6Cu LPBF VQA dataset
Each Parquet row has the seven fields query, image, annot, reasoning, cate, task, and metadata. image is a Hugging Face-compatible {bytes, path} image struct containing an RGB JPEG. The source spreadsheet supplies measured condition-level averages; all images for a power/speed condition are in the same split.
- Downloads last month
- -