record_id int64 332 22.6k | paper_id stringclasses 66
values | material_name stringlengths 1 60 | material_class stringclasses 21
values | irradiation_state stringclasses 2
values | dose_dpa float64 0 400 ⌀ | irradiation_temp_C float64 -273.15 3.1k ⌀ | reactor stringclasses 333
values | particle stringclasses 6
values | helium_appm float64 0.01 400k ⌀ | test_temp_C float64 -273.15 2k ⌀ | experiment_type stringclasses 16
values | yield_strength_mpa_irradiated float64 5 2.65k ⌀ | uts_mpa_irradiated float64 -1 24k ⌀ | elongation_pct_irradiated float64 -7.3 105 ⌀ | hardness_value float64 -45 588k ⌀ | fracture_toughness_mpa_sqrt_m float64 1 1.1k ⌀ | dbtt_k_irradiated float64 -50 1.27k ⌀ | yield_strength_mpa_unirradiated float64 -29 420k ⌀ | uts_mpa_unirradiated float64 -3 13.5k ⌀ | elongation_pct_unirradiated float64 -5 822 ⌀ | volumetric_swelling_pct float64 -60 140 ⌀ | void_diameter_nm float64 0 6.27k ⌀ | void_density_per_m3 float64 0 61,300,000,000,000,010B ⌀ | charpy_energy_j float64 0.1 1.1k ⌀ | confidence_score float64 0.5 1 | reviewed_by_human bool 2
classes | source stringclasses 2
values | grain_size_um float64 0 400 ⌀ | yield_strength_mpa_std float64 0 500 ⌀ | dislocation_loop_diameter_nm float64 1 500 ⌀ | electrical_resistivity_uohm_cm_irradiated float64 -0 42,000B ⌀ |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
1,577 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 100 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,578 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 150 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,580 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 250 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,581 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 300 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,583 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 400 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,584 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 450 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,585 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 500 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,586 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 20 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,587 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 50 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,588 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 100 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,589 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 150 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,590 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 200 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,591 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 250 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,592 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 300 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,594 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 400 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,595 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 20 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,597 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 100 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,599 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 200 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,600 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 250 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,601 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 300 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,602 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 350 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,603 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 400 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,604 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 450 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,605 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 500 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,607 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 50 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,608 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 100 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,611 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 250 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,612 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 300 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,613 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 20 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,614 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 50 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,615 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 100 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,616 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 150 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,617 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 200 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,619 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 300 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,620 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 350 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,622 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 450 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,623 | sdc_ic_iter | Copper-Chromium-Zirconium Alloy | copper_alloy | unirradiated | null | null | null | null | null | 500 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,624 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 20 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,625 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 50 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,627 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 150 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,631 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 350 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,633 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 450 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,634 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 20 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,635 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 50 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,637 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 150 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,638 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 200 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,639 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 250 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,640 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 300 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,641 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 350 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,643 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 450 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,644 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 500 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,645 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 20 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,646 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 50 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,647 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 100 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,648 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 150 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,649 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 200 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,650 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 250 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,651 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 300 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,652 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 350 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,653 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 400 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,654 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 450 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,655 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 20 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,656 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 20 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,657 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 50 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,658 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 100 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,659 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 150 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,661 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 250 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,662 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 300 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,663 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 350 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,664 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 400 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,665 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 450 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,666 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 500 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,667 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 20 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,669 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 100 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,671 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 200 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,674 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 350 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,675 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 400 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,676 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 450 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,677 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 500 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,678 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 20 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,679 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 50 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,680 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 100 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,681 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 150 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,682 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 200 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,683 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 250 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,684 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 300 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,687 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 450 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,688 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 500 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,689 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 20 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,690 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 50 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,691 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 100 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,692 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 150 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,693 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 200 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,694 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 250 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,696 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 350 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,698 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 450 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,699 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | unirradiated | null | null | null | null | null | 500 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,701 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | irradiated | null | null | null | null | null | 100 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,702 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | irradiated | null | null | null | null | null | 150 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
1,703 | sdc_ic_iter | Dispersion-Strengthened Copper | copper_alloy | irradiated | null | null | null | null | null | 200 | null | null | null | null | null | null | null | null | null | null | null | null | null | null | 1 | true | sdc_ic_iter | null | null | null | null |
Subsets and Splits
No community queries yet
The top public SQL queries from the community will appear here once available.