text
stringlengths
0
43
stamped O
silicone S-MATE
specimens O
. O
The O
additive B-MANP
manufactured E-MANP
specimens O
with O
±45° O
and O
90° O
infill S-PARA
direction O
and O
either O
the O
minimal O
or O
small O
void S-CONPRI
extrusion S-MANP
configuration S-CONPRI
had O
the O
strongest O
ultimate B-PRO
tensile I-PRO
strength E-PRO
( O
average S-CONPRI
ranged O
from O
1.44 O
to O
1.51 O
MPa S-CONPRI
) O
. O
This O
strength S-PRO
is O
close O
to O
that O
of O
the O
sheet S-MATE
stamped O
specimens O
which O
have O
an O
average S-CONPRI
ultimate O
tensile B-PRO
strength E-PRO
of O
1.63 O
MPa S-CONPRI
. O
As S-MATE
the O
void S-CONPRI
size O
became O
larger O
and O
more O
elongated O
in O
shape O
, O
the O
average S-CONPRI
ultimate O
tensile B-PRO
strength E-PRO
significantly O
reduced O
to O
1.15 O
and O
0.90 O
MPa S-CONPRI
for O
specimens O
with O
±45° O
and O
90° O
infill S-PARA
direction O
, O