# Welding Defects Detector |
|
|
|
|
|
#### Supported Labels |
|
|
['Defect', 'Welding Line', 'Workpiece', 'porosity'] |
|
|
|
|
|
#### How to use |
|
|
``` |
|
|
from ultralytics import YOLO |
|
|
|
|
|
# Load a pretrained YOLO model |
|
|
model = YOLO(r'weights\welding_defects_yolo11x.pt') |
|
|
|
|
|
# Run inference on 'image.png' with arguments |
|
|
model.predict( |
|
|
'image.png', |
|
|
save=True, |
|
|
device=0 |
|
|
) |
|
|
``` |
|
|
#### Confusion matrix normalized |
|
|
 |
|
|
#### Labels |
|
|
 |
|
|
 |
|
|
#### Results |
|
|
 |
|
|
#### Predict |
|
|
 |
|
|
 |
|
|
``` |
|
|
YOLO11x summary (fused): 464 layers, 56,831,644 parameters, 0 gradients, 194.4 GFLOPs |
|
|
Class Images Instances Box(P R mAP50 mAP50-95): 100%|ββββββββββ| 7/7 [00:06<00:00, 1.11it/s] |
|
|
all 116 773 0.826 0.827 0.842 0.632 |
|
|
Defect 56 131 0.552 0.427 0.445 0.202 |
|
|
Welding Line 116 294 0.873 0.966 0.966 0.679 |
|
|
Workpiece 110 307 0.941 0.987 0.992 0.938 |
|
|
porosity 35 41 0.939 0.927 0.965 0.71 |
|
|
Speed: 0.5ms preprocess, 26.3ms inference, 0.0ms loss, 2.9ms postprocess per image |
|
|
``` |
|
|
|
|
|