title: Material sintering-window comparison (PA12 / PA11 / TPU)
summary: >-
  Relative processing-window widths and handling differences across our powder
  family.

DRAFT — PENDING HUMAN REVIEW. Not served to agents until promoted into source/ (top level). Numbers below are extracted from the cited papers by the 2026-07-16 deep-research pass and domain-checked, but adversarial verification is still in progress. Review before promotion.

Material Windows Comparison

Material Sintering window Notes for agents
PA12 / PA12 GF ~20–25 °C (PA12/CF measured 21 °C) The forgiving baseline; GF adds stiffness, narrows practical window slightly
PA11 ~11 °C — HALF of PA12's Far less bed-temp margin; nitrogen strongly recommended (air degrades faster per Formlabs); expect tighter tolerance to drift
TPU 90A Wide, elastomer behavior Different failure modes (elastic recovery vs curl); Formlabs runs it at ~50 % refresh
PP ~16 °C measured Reference only (not in our powder set)

Sources: Materials 14:1169 survey; SSR-optimization study; Formlabs TDS/support.